INVESTIGATION OF MICROSTRUCTURE AND TEXTURE OF β PHASE IN A FORGED TC18 TITANIUM ALLOY BAR
Received date: 2014-01-02
Revised date: 2014-03-28
Online published: 2014-06-20
To understand the differences in the mechanical properties between the center and surface regions of large size forged TC18 titanium alloy bar, electron backscatter diffraction (EBSD) technique is applied to reveal the differences in textures and strains in β phase in addition to the microstructures observation. The influence of the states of β phase on the deviation to the Burgers orientation relationship (OR) between α/β phases is also analyzed according to the acquired EBSD information. It is found that the β phases in different positions of forged bar are in different states of strain, textures and grain sizes. The β phase in the center shows strong <100> texture and coarse and inhomogeneous grain sizes which all contribute to the difference in properties. The spheroidization of αp phase proceeded mainly within β grains at subgrain boundaries and the OR between two phases changed slightly as the lamella αp phase transforms into block-like αp phase, but changed strongly during transforming to globular morphology. The misorientation in β phase is an effective parameter to evaluate the contribution of work-hardening state for the enhancement of strength, whereas the level of the deviation to Burgers OR is an effective parameter to evaluate the spheroidizing rate and the recovery extent.
Key words: titanium alloy; forging; texture; phase transformation
Kai LI , Ping YANG , Aixue SHA , Mengqi YAN . INVESTIGATION OF MICROSTRUCTURE AND TEXTURE OF β PHASE IN A FORGED TC18 TITANIUM ALLOY BAR[J]. Acta Metall Sin, 2014 , 50(6) : 707 -714 . DOI: 10.3724/SP.J.1037.2014.00003
| [1] | Zhang Y Q, Guo H Z, Sun H L, Yao Z K. Mater Heat Treatment, 2012; 41(6): 147 |
| [1] | (张永强, 郭鸿镇, 孙红兰, 姚泽坤. 热加工工艺, 2012; 41(6): 147) |
| [2] | Huang X, Zhu Z S, Wang H H. Advanced Aeronautical Titanium Alloys and Applications. Beijing: National?Defence?Industry?Press, 2012: 92 |
| [2] | (黄 旭,朱知寿,王红红. 先进航空钛合金材料与应用. 北京: 国防工业出版社, 2012: 92) |
| [3] | Qiao E L, Feng Y Q, Li W Q, Xie R P, Zhang S B, Chen R J. Met World, 2013; (4): 72 |
| [3] | (乔恩利, 冯永琦, 李渭清, 谢仁沛, 张少波, 陈瑞菁. 金属世界, 2013; (4): 72) |
| [4] | Glavicic M G, Goetz R L, Barker D R. Metall Mater Trans, 2008; 49A: 887 |
| [5] | Lonardelli I, Gey N, Wenk H R. Acta Mater, 2007; 55: 5718 |
| [6] | Gurao N P, Ali AA, Suwas S. Mater Sci Eng, 2009; A504: 24 |
| [7] | Cayron C. Scr Mater, 2008; 59: 570 |
| [8] | Salem A A, Glavicic M G, Semiatin S L. Mater Sci Eng, 2008; A494: 350 |
| [9] | Obasi G C, Moat R J, Prakash D G L. Acta Mater, 2012; 60: 7169 |
| [10] | Thomas M J, Wynne B P, Rainforth W M. Mater Charact, 2005; 55: 388 |
| [11] | Markovsky P E, Matviychuk Y V, Bondarchuk V I. Mater Sci Eng,2013; A559: 782 |
| [12] | Semiatin S L, Kinsel K T, Pilchak A L, Sargent G A. Metall Mater Trans, 2013; 44A: 3852 |
| [13] | Sargent G A, Kinsel K T, Pilchak A L. Metall Mater Trans, 2012; 43A: 3570 |
| [14] | Obasi G C, Birosca S, Quinta D F J. Acta Mater, 2012; 60: 1048 |
| [15] | Obasi G C, Quinta D F J, Rugg D. Mater Sci Eng, 2013; A576: 272 |
| [16] | Semiatin S L, Fagin P N, Glavicic M G, Ivasishin O M. Mater Sci Eng, 2001; A299: 225 |
| [17] | Jackson M, Dashwood R, Christodoulou L. Metall Mater Trans, 2005; 36A: 1317 |
| [18] | Karthikeyan T, Dasgupta A, Khatirkar R. Mater Sci Eng, 2010; A528: 549 |
| [19] | He D, Zhu J C, Zaefferer S, Raabe D. Mater Sci Eng, 2012; A549: 20 |
| [20] | Li C, Zhang X, Zhou K. Mater Sci Eng, 2012; A558: 668 |
| [21] | Germain L, Gey N, Humbert M. Acta Mater, 2008; 56: 4298 |
| [22] | Gey N, Bocher P, Uta E. Acta Mater, 2012; 60: 2647 |
| [23] | Leo Prakash D G, Honniball P, Rugg D. Acta Mater, 2013; 61: 3200 |
| [24] | Glavicic M G, Miller G D, Semiatin S L. Scr Mater, 2006; 54: 281 |
| [25] | Gey N, Humbert M. Acta Mater, 2002; 50: 277 |
| [26] | Shao H, Zhao Y Q, Ge P, Zeng W D. Mater Sci Eng, 2013; A586: 215 |
| [27] | Lütjering G. Mater Sci Eng, 1998; A243: 32 |
| [28] | Zhang Z,Wang Q J,Mo W. Titanium Metal Science and Heat Treatment. Beijing: Metallurgical Industry Press, 2009: 86 |
| [28] | (张翥,王群骄,莫畏. 钛的金属学和热处理. 北京: 冶金工业出版社, 2009: 86) |
| [29] | Zhao D H, Wang L, Zhi M S, Xu F. Chin J Stere Image Analy, 2013; 18: 356 |
| [29] | (赵登辉, 王琳, 智茂盛, 徐峰. 中国体视学与图像分析, 2013; 18: 356) |
/
| 〈 |
|
〉 |