EFFECTS OF RE ON THE SOLIDIFICAIION CHARACTERISTICS OF Al-80%Si ALLOY
文 强, 男, 1987年生, 硕士生
Received date: 2013-10-17
Revised date: 2013-10-17
Online published: 2014-05-20
Supported by
Supported by National Basic Research Program of China (No.2011CB610403) and National Natural Science Foundation of China (Nos.51371133, 51071115 and 51171136)
Effects of rare earth (RE) on the morphologies of the recalescence interface, the growing primary Si during the solidification process and the structure after solidification of Al-80%Si alloy were investigated by means of high speed camera and SEM. The critical undercooling ?T1 and ?T2 for the morphology transition of the recalescence interface, the growing primary Si and the structure have been obtained. When the undercooling is lower than ?T1, the morphology of the growing crystal during the solidification process is flake-like; and the structure after the solidification process is composed of large flake grains with pronounced edges and faces. When the undercooling is greater than ?T2, the recalescence interface is a parallel one, and the structure after solidification is composed of homogenous and fine grains, and there exist several smooth spherical bulges on the surface of each grain. In the undercooling region from ?T1 to ?T2 , the recalescence interface and the growing crystal show dendritic features, but some of the dendrites are distributed regularly; after solidification, the structure is composed of refined equiaxed grains and flake grains. For Al-80%Si alloy, ?T1 and ?T2 are equal to 132 and 250 K, respectively. RE can reduce the values of ?T1 and ?T2 . When 1%RE is added into the alloy,?T1 and ?T2 are changed to 60 and 199 K, respectively.
Key words: Al-Si alloy; primary Si; RE; undercooling; structure
Qiang WEN , Zengyun JIAN , Man ZHU , Fang'e CHANG , Bo DANG . EFFECTS OF RE ON THE SOLIDIFICAIION CHARACTERISTICS OF Al-80%Si ALLOY[J]. Acta Metall Sin, 2014 , 50(5) : 610 -618 . DOI: 10.3724/SP.J.1037.2013.00659
| [1] | Zuo M, Jiang K F, Liu X F. J Alloys Compd, 2010; 503: L26 |
| [2] | Faraji M, Todd I, Jones H. J Mater Sci, 2005; 40: 6363 |
| [3] | Jiang Q C, Xu C L, Lu M, Wang H Y. Mater Lett, 2005; 59: 624 |
| [4] | Yi H, Zhang D. Mater Lett, 2003; 57: 2523 |
| [5] | Ohmi T, Matsuura K, Kudoh M. J Jpn Inst Light Met, 1998; 48: 618 |
| [6] | Jian Z Y, Zhu M, Jie W Q. Mater China, 2010; 29: 20 |
| [6] | (坚增运, 朱 满, 介万奇. 中国材料进展, 2010; 29: 20) |
| [7] | Hernandez F C R, Sokolowski J H. J Alloys Compd, 2006; 426: 205 |
| [8] | Jin F W, Ren Z M, Ren W L, Deng K, Zhong Y B, Yu J B. Sci Technol Adv Mater, 2008; 9: 024202 |
| [9] | Xu C L, Wang H Y, Yang F Y, Jiang Q C. Mater Sci Eng, 2007; A452: 341 |
| [10] | Zuo M, Liu X F, Sun Q Q, Jiang K. J Mater Process Technol, 2009; 209: 5504 |
| [11] | Zhang Q, Liu X F, Dai H S. J Alloys Compd, 2009; 480: 376 |
| [12] | Yu L N, Liu X F, Ding H M, Bian X F. J Alloys Compd, 2007; 432: 156 |
| [13] | Zuo M, Zhao D G, Teng X Y, Geng H R, Zhang Z S. Mater Des, 2013; 47: 857 |
| [14] | Wu Y P, Wang S J, Li H, Liu X F. J Alloys Compd, 2009; 477: 139 |
| [15] | Shi W X, Gao B, Tu G F, Li S W, Hao Y, Yu F X. J Rare Earth, 2010; 28: 367 |
| [16] | Chang J Y, Kim G H, Moon I G, Choi C S. Scr Mater, 1998; 39: 307 |
| [17] | Chen C, Liu Z X, Ren B, Wang M X, Weng Y G, Liu Z Y. Trans Nonferrous Met Soc China, 2007; 17: 301 |
| [18] | Li Q L, Xia T D, Lan Y F, Li P F, Fan L. Mater Sci Eng, 2013; A588: 97 |
| [19] | Wei B K, Lin H T, Liu J M, Cai Q Z, Tong X L, Mao Y F. Spec Cast Nonferrous Alloys, 1993; (3): 6 |
| [19] | (魏伯康, 林汉同, 刘俊明, 蔡启舟, 童杏林, 毛玉凤. 特种铸造及有色合金, 1993; (3): 6) |
| [20] | Xu C L, Jiang Q C, Yang Y F, Wang H Y, Wang J G. J Alloys Compd, 2006; 422: L1 |
| [21] | Shi W X, Gao B, Tu G F, Li S W. J Alloys Compd, 2010; 508: 480 |
| [22] | Li Q L, Xia T D, Lan Y F, Zhao W J, Fan L, Li P F. J Alloys Compd, 2013; 562: 25 |
| [23] | Jian Z Y, Nagashio K, Kuribayashi K. Metall Mater Trans, 2002; 33A: 2947 |
| [24] | Jian Z Y, Kuribayashi K, Jie W Q, Chang F E. Acta Mater, 2006; 54: 3227 |
| [25] | Liu R P, Volkmann T, Herlach D M. Acta Mater, 2001; 49: 439 |
| [26] | Wang Q, Liu R P, Qian Y Q, Lou D C, Su Z B, Ma M Z, Wang W K, Panofen C, Herlach D M. Scr Mater, 2006; 54: 37 |
| [27] | Lu S Z, Hellawell A. Metall Mater Trans, 1987; 18A: 1721 |
| [28] | Jian Z Y, Yang X Q, Chang F E, Jie W Q. Metall Mater Trans, 2010; 41A: 1826 |
| [29] | David R L. CRC Handbook of Chemistry and Physics. Tokyo: CRC Press, 1989: B2 |
| [30] | Jian Z Y, Kuribayashi K, Jie W Q. Acta Mater, 2004; 52: 3323 |
/
| 〈 |
|
〉 |