EFFECT OF ULTRA-FAST CONTINIOUS ANNEALING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LOW Si GRADE Nb-Ti MICROALLOYING TRIP STEEL

  • Zongan LUO ,
  • Jiyuan LIU ,
  • Yingying FENG ,
  • Wen PENG
Expand
  • State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
null

Revised date: 2013-09-30

  Online published: 2014-05-20

Supported by

Supported by National High Technology Research and Development Program of China (No.2013AA031302) and Fundamental Research Funds for the Central Universities (No.090307004)

Abstract

Si-containing transformation induced plasticity (TRIP) steel is noted for good balance of excellent formability and high strength as the advanced high strength steel (AHSS). The advantage of this steel can be attributed to the TRIP effect, which is the transformation of the retained austenite. Furthermore, the local increase in specific volume caused by the TRIP effect can help to close propagating cracks. It is favorable for the automotive structural components based on the high work hardening rate and energy absorption behavior. Low Si-containing can optimize the galvanized performance of the cold rolling TRIP steel, and the ferrite stabilization can be compensated by adding Al. Microalloying with Nb and Ti may provide effective means for further strengthening via grain refinement and precipitation strengthening. The ultra-fast continuous annealing comprised of rapid heating and short austempering is a new-style process for grain refinement and precipitation solidifying. However, the influences of the process on the cold rolling low Si TRIP steel, especially the austenite transformation characteristics and their effects on microstructure and mechanical properties, were rarely reported. Therefore, in this work the microstructures of low Si grade Nb-Ti microalloying TRIP steel under different ultra-fast continuous annealing conditions were observed via EBSD and TEM, and the tensile properties were discussed. The results show that the polygonal ferrite is refined by heating rate of 100 ℃/s and short asutempering procedure. The dispersive and fine microalloyed carbonitrides formed during the hot-rolling stage are reserved. Therefore, the strength and ductility are enhanced simultaneously. The slow cooling procedure can effectively contribute to eliminate the yield point, while the strength is slightly decreased. As the annealing temperature increasing, the strength is enhanced. When the annealing temperature is 830 ℃, the morphology of retained austenite consists of alternated film and bainite-ferrite plates, resulting in optimal combination of strength and ductility: tensile strength 748 MPa, yield strength 408 MPa, uniform elongation 21.3%, work hardening exponent 0.27, balance of strength and ductility is 15932.4 MPa·%.

Cite this article

Zongan LUO , Jiyuan LIU , Yingying FENG , Wen PENG . EFFECT OF ULTRA-FAST CONTINIOUS ANNEALING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LOW Si GRADE Nb-Ti MICROALLOYING TRIP STEEL[J]. Acta Metall Sin, 2014 , 50(5) : 515 -523 . DOI: 10.3724/SP.J.1037.2013.00623

References

[1] Jimenez-Melero E, Van Dijk N H, Zhao L, Sietsma J, Offerman S E, Wright J P, Zwaag S. Acta Mater, 2009; 57: 533
[2] Etienne G, Anne M, Pascal J, Yvan H, Bert V, Jan V H. Scr Mater, 2001; 44: 885
[3] Tirumalasetty G K, Van Huis M A, Fang C M, Xu Q, Tichelaar F D, Hanlon D N, Sietsma J, Zandbergen H W. Acta Mater, 2011; 59: 7406
[4] Wang C J, Sun X J, Yong Q L, Li Z D, Zhang X, Jiang L. Acta Metall Sin, 2013; 49: 399
[4] (王长军, 孙新军, 雍岐龙, 李昭东, 张 熹, 江 陆. 金属学报, 2013; 49: 399)
[5] Shanmugam S, Ramisetti N K, Misra R D K, Hartmann J, Jansto S G. Mater Sci Eng, 2008; A478: 26
[6] Xu Y B, Hou X Y, Wang Y Q, Wu D. Acta Metall Sin, 2012; 48: 176
[6] (徐云波, 侯晓英, 王业勤, 吴 迪. 金属学报, 2012; 48: 176)
[7] Jacoues P J, Girault E, Harlef P, Delannay F. ISIJ Int, 2001; 41: 1061
[8] Luo H W, Zhao L, Kruijver S O, Sietsma J, Zwaag S V D. ISIJ Int, 2003; 43: 1219
[9] Eui P K, Shun F, Kozo S, Shigeru S. Mater Sci Eng, 2011; A528: 5007
[10] Chiang J, Lawrence B, Boyd J D K, Pilkey A K. Mater Sci Eng, 2011; A528: 4516
[11] Liu J Y, Zhang Z C, Zhu F X, Li Y M, Manabe K I. J Iron Steel Res Int, 2012; 19: 41
[12] Zhang W N, Liu Z Y, Wang G D. Acta Metall Sin, 2010; 46: 1230
[12] (张维娜, 刘振宇, 王国栋. 金属学报, 2010; 46: 1230)
[13] Funakawa Y, Shiozaki T, Tomita K, Yamamoto T, Maeda E. ISIJ Int, 2004; 44: 1945
[14] Chen J, Lv M Y, Tang S, Liu Z Y, Wang G D. Mater Sci Eng, 2014; A594: 389
[15] Lan H F, Du L X, Wang X N, Liu X H. Steel Res Int, 2012; 83: 139
[16] Wang X P, Du L X, Zhou M. J Northeastern Univ (Nat Sci), 2012; 33: 1137
[16] (王晓鹏, 杜林秀, 周 民. 东北大学学报(自然科学版), 2012; 33: 1137)
[17] Asoo K, Tomota Y, Harjo S, Okitsu Y. ISIJ Int, 2011; 51: 145
[18] Han D, Sun X J, Hui W J, Zhang S L, Shi J, Wang M Q. ISIJ Int, 2008; 48: 1126
[19] Sugimoto K, Murata M, Muramatsu T, Mukai Y. ISIJ Int, 2007; 47: 1357
[20] Lee C G, Kim S J, Oh C S, Lee S. ISIJ Int, 2002; 42: 1162
[21] Zwaag S, Wang J. Scr Mater, 2002; 47: 169
[22] Cui Z Q,Qin Y C. Metallography and Heat Treatment. Beijing: China Machine Press, 2007: 262
[22] (崔忠圻,覃耀春. 金属学与热处理. 北京: 机械工业出版社, 2007: 262)
[23] Tirumalasetty G K, Van Huis M A, Kwakernaak C, Sietsma J, Sloof W G, Zandbergen H W. Acta Mater, 2012; 60: 1311
[24] Jimenez-Melero E, Van Dijk N H, Zhao L, Sietsma J, Offerman S E, Wright J P, Zwaag S. Acta Mater, 2007; 55: 6713
[25] Zaefferer S, Ohlert J, Bleck W. Acta Mater, 2004; 52: 2765
Outlines

/

〈 〉