A THERMODYNAMIC MODEL FOR DIRECTIONAL SOLIDIFICATION OF METAL-HYDROGEN EUTECTIC

  • Zaijiu LI ,
  • Qinglin JIN ,
  • Tianwu YANG ,
  • Rong ZHOU ,
  • Yehua JIANG
Expand
  • Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093

Received date: 2013-09-23

  Revised date: 2013-09-23

  Online published: 2014-04-20

Supported by

Supported by National Natural Science Foundation of China and Yunnan Provincial Government (No.u0837603) and National Natural Science Foundation of China (No.51164018)

Abstract

With the thermodynamic analysis on directional solidification of metal-hydrogen eutectic, a theoretical model was developed to predict the effect of the Gasar processing parameters on the pore diameter and inter-pore spacing. The model was applied for the Gasar porous Cu fabricated by continuous casting process. The average pore diameter and inter-pore spacing decrease as increasing withdrawal rate. The theoretical relationship between the inter-pore spacing l and the withdrawal rate v can be described by a simple equation vl2=B, where B is a constant depending on the melt temperature and hydrogen gas pressure. The model can predict the overall tendency of the experimental results. The deviation between the calculated and experimental values in the case of lower withdrawal rate is considered to be associated with the difference between the real pore structure and ideal pore structure, and the melt convection in the vicinity of solid/liquid interface.

Cite this article

Zaijiu LI , Qinglin JIN , Tianwu YANG , Rong ZHOU , Yehua JIANG . A THERMODYNAMIC MODEL FOR DIRECTIONAL SOLIDIFICATION OF METAL-HYDROGEN EUTECTIC[J]. Acta Metall Sin, 2014 , 50(4) : 507 -514 . DOI: 10.3724/SP.J.1037.2013.00606

References

[1] Shapovalov V I. US Pat, 5181549, 1993
[2] Liu Y, Li Y X, Zhang H W. Acta Metall Sin, 2004; 40: 1121
[2] (刘 源, 李言祥, 张华伟. 金属学报, 2004; 40: 1121 )
[3] Liu P S. Introduction to Cellular Materials. Beijing: Tsinghua University Press, 1999: 6
[3] (刘培生. 多孔材料引论. 北京: 清华大学出版社, 1999: 6)
[4] Simone A E, Gibson L J. Acta Mater, 1996; 44: 1437
[5] Nakajima H, Hyun S K, Ohashi K, Ota K, Murakami K. Colloids Surf, 2001; 179A: 209
[6] Li Z J, Jin Q L, Yang T W, Jiang Y H, Zhou R. Acta Metall Sin, 2013; 49: 757
[6] (李再久, 金青林, 杨天武, 蒋业华, 周 荣. 金属学报, 2013; 49: 757)
[7] Liu Y, Li Y X, Zhang H W, Wan J. Acta Metall Sin, 2005; 41: 886
[7] (刘 源, 李言祥, 张华伟, 万 疆. 金属学报, 2005; 41: 886 )
[8] Xie J X, Liu X H, Liu X F, Fang Y C, Wang H. Chin J Nonferrous Met, 2005; 15: 1869
[8] (谢建新, 刘新华, 刘雪峰, 方玉诚, 王 浩. 中国有色金属学报, 2005; 15: 1869)
[9] Simone A E, Gibson L J. J Mater Sci, 1997; 32: 451
[10] Nakajima H. Progr Mater Sci, 2007; 52: 1091
[11] Peng Z, Yang T W, Li Z J, Li Z H, Jin Q L, Zhou R. Chin J Nonferrous Met, 2011; 21: 1045
[11] (彭 震, 杨天武, 李再久, 黎振华, 金青林, 周 荣. 中国有色金属学报, 2011; 21: 1045)
[12] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2006; 42: 1165
[12] (张华伟, 李言祥, 刘 源. 金属学报, 2006; 42: 1165)
[13] Liu Y, Li Y X. Scr Mater, 2003; 49: 379
[14] Upadhyaya G S,Dube R K. Problems in Metallurgical Thermodynamics and Kinetics. Oxford: Pergamon Press, 1977: 144
[15] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2007; 43: 113
[15] (张华伟, 李言祥, 刘 源. 金属学报, 2007; 43: 113)
[16] Zhang H W. PhD Dissertation, Tsinghua University, Beijing, 2006
[16] (张华伟. 清华大学博士学位论文, 北京, 2006)
[17] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2005; 41: 55
[17] (张华伟, 李言祥, 刘 源. 金属学报, 2005; 41: 55)
[18] Flemings M C. Solidification Processing. Newyork: McGraw-Hill Book Company, 1974: 264
[19] Nishizawa T. Translated by Hao S M. Thermodynamics of Microstructure. Beijing: Chemical Industry Press, 2006: 264
[19] (Nishizawa T著. 郝士明 译. 微观组织热力学. 北京: 化学工业出版社, 2006: 264)
[20] Liu Y, Li Y X, Liu R F, Zhou R, Jiang Y H, Li Z H. Acta Metall Sin, 2010; 46: 129
[20] (刘 源, 李言祥, 刘润发, 周 荣, 蒋业华, 黎振华. 金属学报, 2010; 46: 129)
[21] Yamamura S, Shiota H, Murakami K, Nakajima H. Mater Sci Eng, 2001; A318: 137
[22] Drenchev L, Sobczak J, Sobczak N, Sha W, Malinov S. Acta Mater, 2007; 55: 6459
[23] Sacris E M, Parlee A D. Metall Trans, 1970; 1: 3377
[24] Martin J W,Doherty. Stability of Microstructure in Metallic System. London: Cambridge University Press, 1976: 159
[25] Park J S, Hyun S K, Suzuki S, Nakajima H. Acta Mater, 2007; 55: 5646
Outlines

/

〈 〉