FINITE ELEMENT SIMULATION OF THE EFFECT OF STRESS RELAXATION ON STRAIN-INDUCED MARTENSITIC TRANSFORMATION

  • Rui FENG ,
  • Meihan ZHANG ,
  • Nailu CHEN ,
  • Xunwei ZUO ,
  • Yonghua RONG
Expand
  • School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240
null

冯 瑞, 男, 1988年生, 硕士生

Received date: 2013-09-05

  Revised date: 2013-09-05

  Online published: 2014-04-20

Supported by

Supported by National Natural Science Foundation of China (Nos.51031001 and 51371117)

Abstract

Near 50 years ago, transformation induced plasticity (TRIP) effect was proposed and TRIP steels as an advanced high strength one are widely investigated. However, the mechanism of TRIP effect can be only qualitatively explained, and has not been experimentally and theoretically verified so far. In this work, a strain equivalent model for strain-induced martensitic transformation was built in a microstructure-based finite element model of novel quenching-partitioning-tempering (Q-P-T) steel. With the model, the TRIP effect under the condition of uniaxial tension was simulated, from which the micro-mechanism of TRIP effect is revealed. Stress relaxation from TRIP relieves the stresses within untransformed retained austenite and its adjacent martensite and blocks the formation of cracks, meanwhile, a considerable retained austenite still exists at higher strain level, which is the origin of TRIP effect. Compared with original (thermal-induced) martensite, fresh (strain-induced) martensite bears higher stress. Therefore, it could be predicted that cracks form at first in fresh martensite or its boundaries. Moreover, stress relaxation makes strain-induced martensite formed in intermittent and slow way, and this is consistent with experimental results. However, in stress-free relaxation state fresh martensite appears in successive and quick way, not consistent with experiments, and thus this verifies in opposite way that TRIP effect inevitably produces stress relaxation.

Cite this article

Rui FENG , Meihan ZHANG , Nailu CHEN , Xunwei ZUO , Yonghua RONG . FINITE ELEMENT SIMULATION OF THE EFFECT OF STRESS RELAXATION ON STRAIN-INDUCED MARTENSITIC TRANSFORMATION[J]. Acta Metall Sin, 2014 , 50(4) : 498 -506 . DOI: 10.3724/SP.J.1037.2013.00559

References

[1] Zackay V F, Parker E R, Fahr D, Busch R. ASM Trans Quart, 1967; 60: 252
[2] Bhadeshia H K D H. ISIJ Int, 2002; 42: 1059
[3] Wang X D, Huang B X, Rong Y H, Wang L. J Mater Sci Technol, 2006; 22: 625
[4] Zhou S, Zhang K, Wang Y, Gu J F, Rong Y H. Metall Mater Trans, 2012; 43A: 1026
[5] Olson G B, Cohen M. Metall Trans, 1975; 6A: 791
[6] Stringfellow R G, Parks D M, Olson G B. Acta Metall Mater, 1992; 40: 1703
[7] Tomita Y, Iwamoto T. Int J Mech Sci, 2001; 43: 2017
[8] Iwamoto T, Tsuta T. Int J Plast, 2002; 18: 1583
[9] Serri J, Cherkaoui M. J Eng Mater Technol, 2008; 130: 031009-1
[10] Choi K S, Liu W N, Sun X, Khaleel M A. Acta Mater, 2009; 57: 2592
[11] Choi K S, Liu W N, Sun X, Khaleel M A. Metall Mater Trans, 2009; 40A: 796
[12] Rong Y H. Int Heat Treat Surf Eng, 2011; 5: 145
[13] Zhang K, Zhang M H, Guo Z H, Chen N L, Rong Y H. Mater Sci Eng, 2011; A528: 8486
[14] Uthaisangsuk V, Prahl U, Bleck W. Comp Mater Sci, 2008; 43: 27
[15] Ludwik P. Elemente der Technologischen Mechanik. Berlin: Julius Springer, 1909: 32
[16] Pickering F B. Physical Metallurgy and the Design of Steels. London: Applied Science Publishers, 1978: 1
[17] Sugimoto K, Iida T, Sakaguchi J, Kashima T. ISIJ Int, 2000; 40: 902
[18] Zhang K. PhD Dissertation. Shanghai Jiao Tong University, 2011
[18] (张 柯. 上海交通大学博士学位论文, 2011)
[19] Delannay L, Jacques P, Pardoen T. Int J Solids Struct, 2008; 45: 1825
[20] Leal R H. PhD Dissertation. Massachusetts Institute of Technology, 1984
[21] Zhang W F, Zhu J H, Cao C X. Heat Treat Met, 2005; 30(2): 62
[21] (张旺峰, 朱金华, 曹春晓. 金属热处理, 2005; 30(2): 62)
[22] Muránsky O, ?ittner P, Zrník J, Oliver E C. Acta Mater, 2008; 56: 3367
[23] Hsu T Y. Martensitic Transformation and Martensite. Beijing: Science Press, 1999: 147
[23] (徐祖耀. 马氏体相变与马氏体. 北京: 科学出版社, 1999: 147)
[24] Bhadeshia H K D H. Mater Sci Eng, 2004; A378: 34
[25] Park K K, Oh S T, Baeck S M, Kim D I, Han J H, Han H N, Park S, Lee C G. Mater Sci Forum, 2002; 408-412: 571
Outlines

/

〈 〉