EFFECT OF TEMPERING TEMPERATURE ON CARBIDE AND MECHANICAL PROPERTIES IN A Fe-Cr-Ni-Mo HIGH-STRENGTH STEEL

  • Tao WEN ,
  • Xiaofeng HU ,
  • Yuanyuan SONG ,
  • Desheng YAN ,
  • Lijian RONG
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-10-23

  Revised date: 2013-12-05

  Online published: 2014-04-20

Supported by

Supported by National Natural Science Foundation of China (No.91226204)

Abstract

The variation of carbides with tempering temperature in a Fe-Cr-Ni-Mo high-strength steel and their effect on mechanical properties are investigated by means of TEM and three-dimensional atom probe (3DAP). The results show that there mainly appear M3C and M7C3 when tempering temperature is rather low (400 ℃), the former is thick with a length of about 1 μm and the latter is fine and the length is less than 200 nm, and M is composed of Fe, Cr and Mn. Tempering at 500 and 600 ℃, the amount of carbide increases gradually, and there appear M2C and M6C types of carbide which are both less than 200 nm in length, simultaneously M3C becoming fine or disappear. When tempering temperature further increases to 650 ℃, besides M2C there also appears MC type of carbide. The size of both M2C and MC are less than 100 nm, meanwhile the amount of carbide decreases. The M of M2C, M6C and MC is a combination mainly of Cr, Mo and V. The strength of the Fe-Cr-Ni-Mo high-strength steel gradually reduces with increasing tempering temperature, but the downtrend of strength is rather small when tempering temperature is in the range of 500~600 ℃, owing to secondary hardening induced by the appearance of V-carbide. In short, the high-strength steel could obtain better combination of strength and impact toughness after tempering at about 530~600 ℃.

Cite this article

Tao WEN , Xiaofeng HU , Yuanyuan SONG , Desheng YAN , Lijian RONG . EFFECT OF TEMPERING TEMPERATURE ON CARBIDE AND MECHANICAL PROPERTIES IN A Fe-Cr-Ni-Mo HIGH-STRENGTH STEEL[J]. Acta Metall Sin, 2014 , 50(4) : 447 -453 . DOI: 10.3724/SP.J.1037.2013.00672

References

[1] Misra R D K, Jia Z, Malley R O, Jansto S J. Mater Sci Eng, 2011; A528: 8772
[2] Lee K H, Park S G, Kim Min C, Lee B S, Wee D M. Mater Sci Eng, 2011; A529: 156
[3] Lee B S,Kim M C,Yoon J H,Hong J H. Int J Press Ves Pip, 2010; 87: 74
[4] Han S Y, Shin S Y, Seo C H, Lee H, Bae J H, Kim K, Lee S, Kim N J. Metall Mater Trans, 2009; 40A: 1851
[5] Wang W, Shan Y Y, Yang K. Acta Metall Sin, 2007; 43: 578
[5] (王 伟, 单以银, 杨 柯. 金属学报, 2007; 43: 578)
[6] Michael D M, David N S. Acta Mater, 2011; 59: 1881
[7] Takashi O, Takashi W, Masanori A, Kazumi A. Nucl Eng Des, 2008; 238: 408
[8] Liu Q D, Liu W Q, Wang Z M, Zhou B X. Acta Metall Sin, 2008; 44: 786
[8] (刘庆东, 刘文庆, 王泽民, 周邦新. 金属学报, 2008; 44: 786)
[9] Liu Q D, Chu Y L, Wang Z M, Liu W Q, Zhou B X. Acta Metall Sin, 2008; 44: 1281
[9] (刘庆东, 楮于良, 王泽民, 刘文庆, 周邦新. 金属学报, 2008; 44: 1281)
[10] Zhang Y. PhD Dissertation, Dalian Maritime University, 2007
[10] (张 洋. 大连海事大学博士学位论文, 2007)
[11] Zhang S H. Alloy-Steel. Beijing: Metallurgical Industry Press, 1981: 10, 37
[11] (章守华. 合金钢. 北京: 冶金工业出版社, 1981: 10, 37)
[12] Qi Z F. Diffusion and Phase Transition in Solid Metals. Beijing: China Machine Press, 1998: 201
[12] (戚正风. 固态金属中的扩散与相变. 北京: 机械工业出版社, 1998: 201)
[13] Janovec J, Vyrostkova A, Svoboda M. Metall Mater Trans, 1994; 25A: 267
[14] Tao P, Zhang C, Yang Z G, Takeda H. Acta Metall Sin, 2009; 45: 51
[14] (陶 鹏, 张 弛, 杨志刚, 武田裕之. 金属学报, 2009; 45: 51)
[15] Bjarbo A, Hattestrand M. Metall Mater Trans, 2001; 32A: 19
[16] Pigrova G D. Metall Mater Trans, 1996; 27A: 498
[17] Sun S W, Mao J F, Lei T Q, He L L. Acta Metall Sin, 2000; 36: 1009
[17] (孙树文, 茅建富, 雷廷权, 贺连龙. 金属学报, 2000; 36: 1009)
[18] Liu Q D, Peng J C, Liu W Q, Zhou B X. Acta Metall Sin, 2009; 45: 1288
[18] (刘庆东, 彭建超, 刘文庆, 周邦新. 金属学报, 2009; 45: 1288)
[19] Sun S W, Lei T Q, Tang Z X, You G, Wang X, Chen J L. Iron Steel, 1998; 33: 38
[19] (孙树文, 雷廷权, 唐之秀, 犹 公, 王 欣, 陈家伦. 钢铁, 1998; 33: 38)
Outlines

/

〈 〉