3D ATOM PROBE CHARACTERIZATION OF MICRO-STRUCTURE OF TiBx/Al SUPERSATURATED SOLID SOLUTE COMPOSITE FILMS

  • Hailong SHANG ,
  • Wenqing LIU ,
  • Yujun DONG ,
  • Anming ZHANG ,
  • Bingyang MA ,
  • Geyang LI
Expand
  • 1 State Key Laboratory of Metal Matrix Composites, Shanghai Jiao Tong University, Shanghai 200240
    2 Key Laboratory for Microstructure, Shanghai University, Shanghai 201306

Received date: 2013-07-29

  Revised date: 2013-10-20

  Online published: 2014-04-20

Supported by

Supported by National Basic Research Program of China (No.2012CB619601) and National Natural Science Foundation of China (No.51071104 )

Abstract

In order to reveal the solute existing form and its effect on the microstructure and mechanical properties in the supersaturated solid solute films, TiBx/Al composite film with 7.1%TiBx (atomic fraction) was synthesized by magnetron co-sputtering using Al and TiB2 targets. The microstructure and mechanical properties of the film were characterized by 3D atom probe cambined with X-ray diffraction, transmission electron microscopy and nanoindentation. The results reveal that TiBx compounds were largely dissolved in the Al lattice due to atomic mixing and sufficiently low mobility of the atoms during growth. The film grain was refined to nanoscale and amorphous gradually result from the severe lattice distortion. The film consisted of a two-phase structure in which lower solute content (about 2%TiBx) nanocrystals dispersed in amorphous matrix with a higher solute content and gained high hardness. Combined with the experimental results, the microstructure formation of the composite films was discussed from thermodynamic and kinetic aspects. This study provided the direct experimental evidence of compound dissolved in highly supersaturated solid solution.

Cite this article

Hailong SHANG , Wenqing LIU , Yujun DONG , Anming ZHANG , Bingyang MA , Geyang LI . 3D ATOM PROBE CHARACTERIZATION OF MICRO-STRUCTURE OF TiBx/Al SUPERSATURATED SOLID SOLUTE COMPOSITE FILMS[J]. Acta Metall Sin, 2014 , 50(4) : 395 -399 . DOI: 10.3724/SP.J.1037.2013.00447

References

[1] Lewin E, Buchholt K, Lu J, Hultman L, Spetz L A, Jansson U. Thin Solid Films, 2010; 518: 5104
[2] Sui M L, Lu K. Acta Metall Sin, 1994; 30: 413
[2] (隋曼龄, 卢 柯. 金属学报, 1994; 30: 413)
[3] Sanchette F, Billard A. Surf Coat Technol, 2001; 142: 218
[4] Perez A, Sanchette F, Billard A, Rébéré C, Berziou C, Touzain S, Creus J. Mater Chem Phys, 2012; 132: 154
[5] Naka M, Shibayanag T, Maed M, Zhao S, Mori H. Vacuum, 2000; 59: 252
[6] Chandra T, Tsuzaki K, Militzer M, Ravindran C. Scr Mater, 2001;44: 2035
[7] Boukhris N, Lallouche S, Debilia M Y, Draissia M. Eur Phys J Appl Phys, 2009; 45: 30501
[8] Draissia M, Boudemagh H, Debili Y M. Phys Scr, 2004; 69: 348
[9] Rupert J T, Trenkle C J, Schuh A C. Acta Mater, 2011; 59: 1619
[10] Yang D, Zhong N, Shang H L, Sun S Y, Li G Y. Acta Phys Sin,2013; 62: 036801
[10] (杨 铎, 钟 宁, 尚海龙, 孙士阳, 李戈扬. 物理学报, 2013; 62: 036801)
[11] Shang H L, Shen J, Yang D, Sun S Y, Li G Y. Acta Metall Sin,2013; 49: 320
[11] (尚海龙, 沈 洁, 杨 铎, 孙士阳, 李戈扬. 金属学报, 2013; 49: 320)
[12] Liu Q D, Liu W Q, Wang Z M, Zhou B X. Acta Metall Sin, 2008;44: 786
[12] (刘庆冬, 刘文庆, 王泽民, 周邦新. 金属学报, 2008; 44: 786)
[13] Liu Q D, Liu W Q, Wang Z M, Zhou B X. Acta Metall Sin, 2009;45: 1281
[13] (刘庆冬, 刘文庆, 王泽民, 周邦新. 金属学报, 2009; 45: 1281)
[14] Mayrhofer H P, Mitterer C, Hultman L, Clemens H. Prog Mater Sci, 2006; 51: 1032
[15] Silva M, Wille C, Klement U, Choi P, Al-Kassab T. Mater Sci Eng,2007; A445: 31
[16] Liu F. Appl Phys, 2005; 81A: 1095
[17] Yue N L, Lu L, Lai M O. Compos Struct, 1999; 47: 691
[18] Meng Q P, Rong Y H, Hsu T Y. Mater Sci Eng, 2007; A471: 22
[19] Fleischer R L. The Strengthening of Metals. New York: Reinhold Publishing Corp, 1964: 93
[20] Labusch R. Phys Status Solidi, 1970; 41: 659
[21] Suzuki H. Dislocations and Mechanical Properties of Crystals. New York: J. Wiley, 1957: 361
[22] Meng Q P, Zhou N, Rong Y H, Chen S P, Hsu T Y (Xu Z Y). Acta Mater, 2002; 50: 4563
[23] Wu X L, Zhu Y T. Appl Phys, 2006; 89A: 031922
[24] Legros M, Gianola S D, Hemker J K. Acta Mater, 2008; 56: 3380
Outlines

/

〈 〉