COMBUSTION SYNTHESIS OF TiC-TiB2 PARTICU- LATES LOCALLY REINFORCED STEEL MATRIX COMPOSITES FROM AN Al-Ti-B4C SYSTEM DURING CASTING
Received date: 2013-09-04
Revised date: 2013-12-16
Online published: 2014-03-20
Supported by
Supported by National Natural Science Foundation of China (No.51101143)
From the point of view of the application, the service life of component usually relies on the wear resistance of local region, and it is desirable that the local region of component rather than the whole component is reinforced by ceramic particulate to offer high-wear resistance. In this study, the TiC-TiB2 particulates locally reinforced steel matrix composites were fabricated by an SHS-casing route using an Al-Ti-B4C system. The effects of the Al content on the microstructure and wear resistance of the composites were investigated. The results show that the TiC and TiB2 particulates were formed in all the preforms with various Al contents (0~50%, mass fraction) after the high temperature (about 1873 K ) steel melt was poured into the mold and the molten steel, to the different extents, penetrates into the synthesized samples. The Al content in the preforms has a large effect on the constitute of the synthesized products and the quantity, size and distribution of the ceramic phases in both the reinforced region and the transition region. With the increase of the Al content, the quantity and average size of the ceramic particles as well as holes decrease, the type and quantity of the intermetallic compounds in the products increase and the gradient distribution of the ceramic particles in the transition region weakens and finally disappears. The wear resistance of the locally reinforced composites is much superior to that of the unreinforced steel matrix, and the best appears in the sample free of Al composition, and then followed by the samples of 30%Al, 10%Al and 50%Al in turn.
Key words: combustion synthesis; composite; microstructure; wear
Ying WANG , Binglin ZOU , Xueqiang CAO . COMBUSTION SYNTHESIS OF TiC-TiB2 PARTICU- LATES LOCALLY REINFORCED STEEL MATRIX COMPOSITES FROM AN Al-Ti-B4C SYSTEM DURING CASTING[J]. Acta Metall Sin, 2014 , 50(3) : 367 -372 . DOI: 10.3724/SP.J.1037.2013.00548
| [1] | Xu K D. Iron Steel, 2008; 43(2): 1 |
| [1] | (徐匡迪. 钢铁, 2008; 43(2): 1) |
| [2] | Guo Z C, Fu Z X. Energy, 2010; 35: 4356 |
| [3] | Yin R Y. Acta Metall Sin, 2002; 38: 561 |
| [3] | (殷瑞钰. 金属学报, 2002; 38: 561) |
| [4] | Zhang Y H, Yuan X Z, Luo D M, Nie X T, Zhao X J. Ind Furn, 2013; 35(3): 12 |
| [4] | (张永红, 袁熙志, 罗冬梅, 聂雪涛, 赵熙锦. 工业炉, 2013; 35(3): 12) |
| [5] | Tjong S C, Lau K C. Compos Sci Technol, 2000; 60: 1141 |
| [6] | Degnan C C, Shipway P H. Wear, 2002; 252: 832 |
| [7] | Pagounis E, Lindroos V K. Mater Sci Eng, 1998; A246: 221 |
| [8] | Liu J J, Liu Z D. Mater Lett, 2010; 64: 684 |
| [9] | Cook B A, Peters J S. Wear, 2011; 271: 640 |
| [10] | Jiang Q C, Ma B X, Wang H Y, Wang Y, Dong Y P. Composites Part A, 2006; 37: 133 |
| [11] | Liang Y H, Han Z W, Zhang Z H, Li X J, Ren L Q. Mater Des, 2012; 40: 64 |
| [12] | Wang Y, Zhang Z Q, Wang H Y, Ma B X, Jiang Q C. Mater Sci Eng, 2006; 422: 339 |
| [13] | Pan Y. Manuf Inf Eng China, 1995; (3): 5 |
| [13] | (潘 冶. 机械设计与制造工程,1995; (3): 5) |
| [14] | Zhang D M, Li F Z, Liu Z J, Han Y Y. J Harbin Univ Sci Technol, 2002; 7(4): 22 |
| [14] | (章德铭, 李凤珍, 刘兆晶, 韩媛媛. 哈尔滨理工大学学报, 2002; 7(4): 22) |
| [15] | Zeng S Y, Zhang E L, Li Q C. Aero Mater Technol, 1995; (5): 27 |
| [15] | (曾松岩, 张二林, 李庆春. 宇航材料工艺, 1995; (5): 27) |
| [16] | Yan Y W, Wei B K, Fu Z Y. Acta Metall Sin, 1999; 35: 909 |
| [16] | (严有为, 魏伯康, 傅正义. 金属学报, 1999; 35: 909) |
| [17] | Wang H Y, Jiang Q C, Ma B X, Wang Y, Zhao F. J Alloys Compd, 2005; 391: 55 |
| [18] | Li B H, Liu Y, Li J, Gao S J, Cao H, He L. Mater Des, 2010; 31:877 |
| [19] | Jiang Q C, Ma B X, Wang H Y, Wang Y, Dong Y P. Composites Part A, 2006; 37: 133 |
| [20] | Zou B L, Shen P, Cao X Q, Jiang Q C. Mater Chem Phys, 2012; 132: 51 |
| [21] | Moore J J, Feng H J. Mater Sci, 1995; 39: 243 |
| [22] | Munir Z A,Tamburuni U A. Mater Sci Rep, 1989; 3: 277 |
| [23] | Gusev A I. Solid State Chem, 1997; 133: 205 |
| [24] | Liang Y J,Che Y C. Handbook of Thermodynamic Data of Inorganics. Shenyang: Northeastern University Press, 1993: 1 |
| [24] | (梁英教,车荫昌. 无机物热力学数据手册. 沈阳: 东北大学出版社, 1993: 1) |
| [25] | Tang W M, Tang H J, Zheng Z Q, Ding H F, Lv J, Liu J W. Chin J Nonferrous Met, 2003; 13: 811 |
| [25] | (汤文明, 唐红军, 郑治群, 丁厚福, 吕 珺, 刘君武. 中国有色金属学报, 2003; 13: 811) |
| [26] | Zhang Y J, Jun Y S, Bao Z C. Bull Chin Ceram Soc, 2000; (4): 39 |
| [26] | (张玉军, 君衍升, 包志臣. 硅酸盐通报, 2000; (4): 39) |
/
| 〈 |
|
〉 |