NUCLEATION AND COARSENING MECHANISM OF δ PHASE IN INCONEL 625 DEPOSITED METAL

  • Xinjie DI ,
  • Xixue XING ,
  • Baosen WANG
Expand
  • 1 Tianjin Key Laboratory of Advanced Joining Technology, Tianjin University, Tianjin 300072
    2 School of Materials Science and Engineering, Tianjin University, Tianjin 300072
    3 Baosteel Research Institute, Baoshan Iron & Steel Co., Ltd., Shanghai 201900

Received date: 2013-07-08

  Revised date: 2013-08-09

  Online published: 2014-03-20

Supported by

Supported by Tianjin Natural Science Foundation (No.11JCYBJC06000) and Key Project of Tianjin Municipal Science and Technology Support Program (No.11ZCGYSF00100)

Abstract

Using Inconel 625 wire to weld high yield strength steels or stainless steels that commonly used in nuclear power plant components and gas turbines can significantly improve high temperature mechanical properties and corrosion resistance of weld structure. However, toughness, fatigue strength and creep rupture strength of weld would decline obviously because of the precipitation of δ phase during service at elevated temperatures for a long time. This work aims to investigate nucleation mechanism of δ phase in Inconel 625 deposited metal by means of SEM and TEM. Meanwhile, coarsening inherent law of δ phase during post-weld heat treatment (PWHT) at 850 ℃ for 2, 4 and 8 h respectively was revealed. The results indicate that a large number of needle-like δ phase precipitates in Inconel 625 deposited metal after PWHT at 850 ℃. These δ phases appear a grid-like distribution in γ-matrix, and there are some poor γ" phase regions appearing near δ phase. Formation process of δ phase is a solid phase transformation process which is like bainite transformation in steels. Crystal nucleus of δ phase form in the close-packed plane of γ" phase by shear mode, and coarsening behavior of δ phase is a diffusion-controlled growth process. When PWHT holding time is shorter, actual average size of δ phase is in line with LSW theory. With PWHT holding time extending, its actual average size deviates from the predicted value of classical LSW theory, because of the high-density and non-directional precipitation characteristics of δ phase.

Cite this article

Xinjie DI , Xixue XING , Baosen WANG . NUCLEATION AND COARSENING MECHANISM OF δ PHASE IN INCONEL 625 DEPOSITED METAL[J]. Acta Metall Sin, 2014 , 50(3) : 323 -328 . DOI: 10.3724/SP.J.1037.2013.00383

References

[1] Special Metals Corporation Products. INCONEL? alloy 625, www.specialmetals.com/products
[2] Murr L E, Martinez E, Gaytan S M.Metall Mater Trans, 2011; 42A: 3491
[3] Xu Y L, Ran Q X, Li J, Peng J C, Xiao X S, Cao X L, Jia G Q.Mater Sci Eng, 2013; A569: 27
[4] Paul C P, Ganesh P, Mishra S K, Bhargava P, Negi J, Nath A K.Opt Laser Technol, 2007; 39: 800
[5] Evans N D, Maziase P J, Shingledecker J P, Yamamoto Y.Mater Sci Eng, 2008; A498: 412
[6] Dupont J N, Lippold J C, Kiser S D. Welding Metallurgy and Weldability of Nickel-base Alloys. New Jersey: John Wiley & Sons, 2009: 47
[7] Shankar V, Bhanu Sankara Rao K, Mannan S L.J Nucl Mater, 2001; 288: 222
[8] Smith G D, Tillack D J, Patel S J. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale PA: The Minerals Metals & Materials Society, 2001: 35
[9] Janaki Ram D J, Venugopal Reddy A, Prasad Rao K, Madhusudhan Reddy G.J Mater Proc Technol, 2005; 167: 73
[10] Shoemaker L E. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale PA: The Minerals Metals & Materials Society, 2005: 409
[11] Cortial F, Corrieu J M, Vernot-Loier C.Metall Mater Trans, 1995; 26A: 1273
[12] Mathew M D, Bhanu Sankara Rao K, Mannan S L.Mater Sci Eng, 2004; A372: 327
[13] Mathew M D, Parameswaran P, Bhanu Sankara Rao K.Mater Charact, 2008; 59: 508
[14] Sundararaman M, Mukhopadhyay P, Banerjee S.Metall Trans, 1988; A19: 453
[15] Huang Y, Langdon T G. J Mater Sci, 2007; 42: 421
[16] Zhang H Y, Zhang S H, Cheng M, Li Z X.Mater Charact, 2010; 61: 49
[17] Yeh A C, Lu K W, Kuo C M, Bor H Y, Wei C N.Mater Sci Eng, 2011; A530: 525
[18] Kuo C M, Yang Y T, Bor H Y, Wei C N, Tai C C. Mater Sci Eng, 2009; A510-511: 289
[19] Dong J X, Xie X S, Wang M.Ordnance Mater Sci Eng, 1993; 16: 51
[20] Xie X S, Dong J X, Fu S H, Zhang M C.Acta Metall Sin, 2010; 46: 1289
[20] (谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289)
[21] Footner P K, Richards B P.J Mater Sci, 1982; 17: 2141
[22] Smokingermain R E,translated by Zhang R J. Modern Physical Metallurgy. Beijing: Metallurgical Industry Press, 1980: 176
[22] (Smokingermain R E著,张人洁译. 现代物理冶金学. 北京: 冶金工业出版社, 1980: 176)
[23] Cahn J W.Acta Metall, 1966; 14: 83
[24] Orian R A.Acta Metall, 1964; 12: 1399
[25] Burke M G, Miller M K.Precipitationin Alloy 718. Pennsylvania: TMS, 1991: 3377
Outlines

/

〈 〉