THE FORMATION MECHANISM OF AUSTENITE STRUCTURE WITH MICRO/SUB-MICROMETER BIMODAL GRAIN SIZE DISTRIBUTION

  • Huibin WU ,
  • Fengjuan WU ,
  • Shanwu YANG ,
  • Di TANG
Expand
  • 1 National Engineering Research Center for Advanced Rolling Technology, University of Science and Technology Beijing, Beijing 100083
    2 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Received date: 2013-09-09

  Revised date: 2013-12-13

  Online published: 2014-03-20

Supported by

Supported by National Science and Technology Major Project of the Ministry of Science and Technology of China (No.2011ZX05016-004)

Abstract

Nano-crystalline (<100 nm) and ultrafine grained (100~500 nm) materials have high strength and toughness, but its work hardening ability and uniform elongation decreased relative to the coarse grained material. Through the deformation, phase transformation and recrystallisation combination mode of development of bimodal grain size distribution of ferrite, bainite steel, the elongation rate is greatly improved. These studies are generally in order to improve the mechanical properties of material through change microstructure, but lack of study for the bimodal grain size distribution formation mechanism. This research work by cold rolling with annealing at 820~870 ℃, in 316L austenitic stainless steel to achieve micro (3~5 μm) and sub-micro (300~500 nm) bimodal grain size distribution. In the austenite deformation process, deformation twinning and strain induced martensite transformation occurred in large deformation stage. Accordingly inferred austenite deformation twinning is the micro mechanism of strain induced martensite. Annealing at 820~870 ℃, the hardness of the samples and the grain size distribution remains nearly constant. Through the comparative analysis of induced martensite austenite evolution driving force and strain deformation during annealing, determined the source of bimodal grain size distribution. The micro scale grains came from the recrystallization of deformed austenite in the cold deformation does not change, and sub-micron grain size is mainly composed of strain induced martensite reverse transformation.

Cite this article

Huibin WU , Fengjuan WU , Shanwu YANG , Di TANG . THE FORMATION MECHANISM OF AUSTENITE STRUCTURE WITH MICRO/SUB-MICROMETER BIMODAL GRAIN SIZE DISTRIBUTION[J]. Acta Metall Sin, 2014 , 50(3) : 269 -274 . DOI: 10.3724/SP.J.1037.2013.00571

References

[1] Hwang B, Lee C G. Mater Sci Eng, 2010; A527: 4341
[2] Chen J, Li F, Liu Z Y, Tang S, Wang G D. ISIJ Int, 2013; 53: 1070
[3] Weng Y Q. Ultrafine Grained Steel. Beijing: Metallurgical Industry Press, 2003: 9
[3] (翁宇庆. 超细晶钢. 北京: 冶金工业出版社, 2003: 9)
[4] Misra R D K, Zhang Z, Venkatasurya P K C, Somani M C, Karjalainen L P. Mater Sci Eng, 2011; A528: 1889
[5] Garcia M C, Caballero F G, Bhadeshia H K D H. ISIJ Int, 2003; 43: 1238
[6] Huang C X, Yang G, Gao Y L, Wu S D, Li S X, Zhang Z F. Philos Mag, 2007; 87: 4949
[7] Huang C X, Gao Y L, Yang G, Wu S D, Li G Y, Li S X. J Mater Res, 2006; 21: 1687
[8] Yang G, Huang C X, Wu S D, Zhang Z F. Acta Metall Sin, 2009; 45: 906
[8] (杨 钢, 黄崇湘, 吴士丁, 张哲峰. 金属学报, 2009; 45: 906)
[9] Etiennea A, Radigueta B, Genevoisa C, Bretona J M, Valievb R, Pareigea P. Mater Sci Eng, 2010; A527: 5805
[10] Misra R D K, Zhang Z, Jia Z, Somani M C, Karjalainen L P. Scr Mater, 2010; 63: 1057
[11] Zhang K M, Zou J X. Thin Solid Films, 2012; 526: 28
[12] Rezaee A, Kermanpur A, Najafizadeh A, Moallemi M. Mater Sci Eng, 2011; A528: 5025
[13] Misra R D K, Zhang Z, Jia Z, Surya V, Somani M C, Karjalainen L P. Mater Sci Eng, 2011; A528: 6958
[14] Koeh C C. J Metast Nanocryst Mater, 2003; 18: 9
[15] KarimPoor A A, Erb U, Austetal K T. Mater Sci Forum, 2002; 415: 38
[16] Wang Y M, Chen M W, Zhou F. Nature, 2002; 419: 912
[17] Wang T S, Zhang F C, Zhang M, Lvb B. Mater Sci Eng, 2008; A485: 456
[18] Alizamini H A, Militzer M, Poole W J. Scr Mater, 2007; 57: 1065
[19] Chakrabarti D, Davis C, Strangwood M. Mater Charact, 2007; 58: 423
Outlines

/

〈 〉