The electrochemical actuation performance of nanoporous gold samples deformed by compression was investigated. Although the porosity and specific surface area decrease with increasing compression strain, the strain amplitude of actuation which were measured along the compression direction, increases and then decreases with increasing compression strain. The compression also greatly increases the strain energy density of nanoporous gold actuator. The improvement of actuation performance is attributed to the morphology change of nanoporous structure during compression. The understanding of the underlying mechanism requires quantitative characterization of morphology and morphological evolution of nanoporous structure during compression.
Xinglong YE , Feng LIU , Haijun JIN . ELECTROCHEMICAL ACTUATION OF NANOPOROUS GOLD DEFORMED BY COMPRESSION[J]. Acta Metall Sin, 2014 , 50(2) : 252 -258 . DOI: 10.3724/SP.J.1037.2013.00664
| [1] | Ding Y, Chen M W, Erlebacher J. J Am Chem Soc, 2004; 126: 6876 |
| [2] | Wittstock A, Zielasek V, Biener J, Friend C M, Baeumer M. Science, 2010; 327: 319 |
| [3] | Xu C X, Su J X, Xu X H, Liu P P, Zhao H J, Tian F, Ding Y. J Am Chem Soc, 2007; 129: 42 |
| [4] | Ye X L, Jin H J. Appl Phys Lett, 2013; 103: 201912 |
| [5] | Weissmüller J, Viswanath R N, Kramer D, Zimmer P, Wurschum R,Gleiter H. Science, 2003; 300: 312 |
| [6] | Jin H J, Weissmüller J. Science, 2011; 332: 1179 |
| [7] | Kramer D, Viswanath R N, Weissmüller J. Nano Lett, 2004; 4: 793 |
| [8] | Jin H J, Wang X L, Parida S, Wang K, Seo M, Weissmüller J. Nano Lett, 2010; 10: 187 |
| [9] | Jin H J, Weissmüller J. Adv Eng Mater, 2010; 12: 714 |
| [10] | Weissmüller J, Cahn J W. Acta Mater, 1997; 45: 1899 |
| [11] | Weissmüller J, Duan H L, Farkas D. Acta Mater, 2010; 58: 1 |
| [12] | Diao J K, Gall K, Dunn M L. Nat Mater, 2003; 2: 656 |
| [13] | Ibach H. Surf Sci Rep, 1997; 29: 193 |
| [14] | Biener J, Wittstock A, Zepeda-Ruiz L, Biener M M, Kramer D, Viswanath R N, Weissmüller J, Viswanath R N, Baümer M, Hamza A V. Nat Mater, 2009; 8: 47 |
| [15] | Erlebacher J, Aziz M J, Karma A, Dimitrov N, Sieradzki K. Nature, 2001; 410: 450 |
| [16] | Weissmüller J, Newman R C, Jin H J, Hodge A M, Kysar J W. MRS Bull, 2009; 34: 577 |
| [17] | Shao L H, Biener J, Jin H J, Biener M M, Baumann T F, Weissmüller J. Adv Funct Mater, 2012; 22: 3029 |
| [18] | Jin H J, Parida S, Kramer D, Weissmüller J. Surf Sci, 2008; 602: 3588 |
| [19] | Jin H J, Kurmanaeva L, Schmauch J, Roesner H, Ivanisenko Y, Weissmüller J. Acta Mater, 2009; 57: 2665 |
| [20] | Gibson L J,Ashby M F. Cellular Solids: Structure and Properties.Cambridge: Cambridge University Press, 1997: 186 |
| [21] | HodgeA M, DoucetteR T, Biener M M, Biener J, Cervantes O, Hamza A V. J Mater Res, 2009; 24: 1600 |
| [22] | Shao L H, Jin H J, Viswanath R N,Weissmüller J. EPL, 2010; 89: 66001 |
/
| 〈 |
|
〉 |