ATOMISTIC SIMULATIONS OF BAUSCHINGER EFFECT IN NANOCRYSTALLINE ALUMINUM THIN FILMS
Received date: 2013-11-15
Revised date: 2013-11-15
Online published: 2014-02-20
Supported by
Supported by National Science Foundation (Nos.DMR-0520651, CMMI-0758535 and MSS090046)
The early Bauschinger effect in nanocrystalline Al thin films with different thicknesses and microstructural orientations was investigated using large-scale atomistic simulations. The simulation results indicate that the microstructural orientation heterogeneity has a significant influence on the early Bauschinger effect and the associated plastic deformation mechanisms. The (110)-textured thin films show less Bauschinger effect compared to non-textured films despite having the same grain size, shape and thickness. The atomistic simulations reveal that the early Bauschinger effect originates from the reverse motion of dislocations and the reduction in dislocation density due to dislocation reactions during unloading, which are driven by the internal residual stress caused by the inhomogeneous deformation during loading.
Xiaoyan LI . ATOMISTIC SIMULATIONS OF BAUSCHINGER EFFECT IN NANOCRYSTALLINE ALUMINUM THIN FILMS[J]. Acta Metall Sin, 2014 , 50(2) : 219 -225 . DOI: 10.3724/SP.J.1037.2013.00737
| [1] | Lu K, Zhou F. Acta Metall Sin, 1997; 33: 99 |
| [1] | (卢 柯, 周 飞. 金属学报, 1997; 33: 99) |
| [2] | Kumar K S, Van Swygenhoven H, Suresh S. Acta Mater, 2003; 51: 5743 |
| [3] | Yamakov V, Wolf D, Philpot S R, Mukherjee A K, Gleiter H. Nat Mater, 2004; 3: 43 |
| [4] | Meyers M A, Mishra A, Benson D J. Prog Mater Sci, 2006; 51: 427 |
| [5] | Van Swygenhoven H, Weertman J R. Mater Today, 2006; 9: 24 |
| [6] | Wu X, Zhu Y T, Chen M W, Ma E. Scr Mater, 2006; 54: 1685 |
| [7] | Legros M, Gianola D S, Hemker K J. Acta Mater, 2008; 56: 3380 |
| [8] | Lu L, Sui M L, Lu K. Science, 2000; 287: 1463 |
| [9] | Shan Z W, Stach E A, Wiezorek J M K, Knapp J A, Follstaedt D M, Mao S X. Science, 2004; 305: 654 |
| [10] | Yang W, Wang H T. J Mech Phys Solids, 2004; 52: 875 |
| [11] | Wang H T, Yang W. J Mech Phys Solids, 2004; 52: 1151 |
| [12] | Hall E O. Proc Phys Soc, 1951; 51B: 747 |
| [13] | Petch H J. J Iron Steel Inst, 1953; 174: 25 |
| [14] | Chokshi A H, Rosen A, Karch J, Gleiter H. Scr Metall, 1989; 23: 1679 |
| [15] | Schiotz J, Jacobsen K W. Science, 2003; 301: 1357 |
| [16] | Jiang Z, Liu X, Li G, Jiang Q, Lian J. Appl Phys Lett, 2006; 88: 143115 |
| [17] | Schwaiger R, Moser B, Dao M, Chollacoop N, Suresh S. Acta Mater, 2003; 51: 5159 |
| [18] | Wang Y M, Hamza A V, Ma E. Acta Mater, 2006; 54: 2715 |
| [19] | Wei Y J, Bower A F, Gao H J. Acta Mater, 2008; 56: 1741 |
| [20] | Zhang K, Weertman J R, Eastman J A. Appl Phys Lett, 2005; 87: 061921 |
| [21] | Gianola D S, Van Petegem S, Legros M, Brandstetter S, Van Swygenhoven H, Hemker K J. Acta Mater, 2006; 54: 2253 |
| [22] | Rajagopalan J, Han J H, Saif M T A. Science, 2007; 315: 1831 |
| [23] | Rajagopalan J, Han J H, Saif M T A. Scr Mater, 2008; 59: 921 |
| [24] | Li X Y, Wei Y J, Yang W, Gao H J. Proc Natl Acad Sci USA, 2009; 106: 16108 |
| [25] | Margolin H, Hazaveh F, Yaguchi H. Scr Metall, 1978; 12: 1141 |
| [26] | Ono N, Tsuchikawa T, Nishimura S, Karashima S. Mater Sci Eng, 1983; 59: 223 |
| [27] | Baker S P, Keller-Flaig R M, Shu J B. Acta Mater, 2003; 51: 3019 |
| [28] | Xiang Y, Vlassak J J. Scr Mater, 2005; 53: 177 |
| [29] | Nicola, L, Xiang Y, Vlassak J J, Van der Giessen E, Needleman A. J Mech Phys Solids, 2006; 54: 2089 |
| [30] | Stoltz R E, Pelloux R M. Metall Trans, 1976; 7A: 1295 |
| [31] | Aran A, Demirkol M, Karabulut A. Mater Sci Eng, 1987; 89: L35 |
| [32] | Rajagopalan J, Rentenberger C, Karnthealer H P, Dehm G, Saif M T A. Acta Mater, 2010; 58: 4772 |
| [33] | Espinosa H D, Panico M, Berbenni S, Schwarz K W. Int J Plast, 2006; 22: 2091 |
| [34] | Fang H, Horstemeyer M F, Baskes M I, Solanki K. Comput Method Appl Mech Eng, 2004; 193: 1789 |
| [35] | Mishin M, Farkas D, Mehl M J, Papaconstantopoulos D A. Phys Rev, 1999; 59B: 3393 |
| [36] | Nose S A. J Chem Phys, 1984; 81: 511 |
| [37] | Tuckerman M, Berne B J, Mantyna G J. J Chem Phys, 1992; 97: 1990 |
| [38] | Van Swygenhoven H, Farkas D, Caro A. Phys Rev, 2000; 62B: 831 |
| [39] | Yamakov V, Wolf D, Phillpot S R, Mukherjee A K, Gleiter H. Nat Mater, 2002; 1: 45 |
/
| 〈 |
|
〉 |