Original Articles

RESIDUAL STRESS IN THE WHEEL OF 42CrMo STEEL DURING QUENCHING

  • Yongkui LI ,
  • Jundan CHEN ,
  • Shanping LU
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-08-05

  Revised date: 2013-08-05

  Online published: 2014-01-11

Supported by

Supported by Science and Technology Projects of Liaoning Province (No.2010224008)

Abstract

42CrMo steel, a typical low alloy medium carbon structural steel, is widely used in important structural components that require high strength, plasticity and toughness, such as crane weight-on-wheel, automobile crank shaft, locomotive gear hub, oil drill pipe joints of deep well, fishing tools and so on, for its good harden ability, high temperature strength, good creep resistance and little quenching deformation. The wheels of the polar crane that used in the Chinese third generation nuclear power plant are made of steel 42CrMo. However, cracks and surface peeling normally occur after heat treatment at quenching process of wheel forgings. There is important application background and practical significance to research the effect of the heat treatment process on the microstructures and mechanical properties and the influence of porosity defects inside the forging wheel on the heat treatment process. Large numbers of research work had been focused on segregation and heat treatment process for solving this matter in passing days. This work aims to study the effects of thermal residual stress on porosity defect in a wheel, and explain the reason for cracking and surface feeling in the way of mechanical behavior during quenching. A wheel with surface peeling was analyzed by measuring chemical compositions, macro- and micro-crack observation. Random testing position for mechanical compositions showed that the effects of segregation was small in the wheel. A set of tests and measurements for thermal mechanical properties of 42CrMo steel were conducted from room temperature to 850 oC. FEM models containing porosity defects in different sizes and without defects were constructed by Abaqus for studying the residual stresses during quenching in fully coupled temperature-displacement analysis. Simulation results indicate that the porosity defects in wheel cause stress concentration within themselves. The maximum residual stress is not affected by the length of porosity region. The hoop residual stress in porosity region in the wheel due to quenching process is in the highest level and believed to be the driving force of cracks. According to the stress distribution in the wheel, the cracks caused by the hoop residual stress can not propagate out of the defects region too far. While the assumptions of surface peeling of wheel are concluded due to combined influence of the residual stress and external loads when the defects region emerges near the wheel surface border in view of the current simulation.

Cite this article

Yongkui LI , Jundan CHEN , Shanping LU . RESIDUAL STRESS IN THE WHEEL OF 42CrMo STEEL DURING QUENCHING[J]. Acta Metall Sin, 2014 , 50(1) : 121 -128 . DOI: 10.3724/SP.J.1037.2013.00476

References

[1] Li B. Master Thesis, Shanghai Jiaotong University, 2007
[1] (李 波. 上海交通大学硕士学位论文, 2007)
[2] Gong B Z.Hoisting Conveying Mach, 2002; (2): 9
[2] (宫本智. 起重运输机械, 2002; (2): 9)
[3] Zhang Q F.Hoisting Conveying Mach, 2011; (3): 26
[3] (张全福. 起重运输机械, 2011; (3): 26)
[4] Quan G Z, Li G S, Chen T, Wang W X, Zhang Y W, Zhou J. Mater Sci Eng, 2011; A528: 4643
[5] Holzapfel H, Schulze V, V?hringer O, Macherauch E.Mater Sci Eng, 1998; A248: 9
[6] Sarioglu F.Mater Sci Eng, 2001; A315: 98
[7] Lin Y C, Chen M S, Zhong J. Mech Res Commun, 2008; 35: 142
[8] Liu D Z, Li T F, Yang H.Heat Treat Technol Equip, 2008; 29(3): 74
[8] (刘多智, 李廷峰, 杨 慧. 热处理技术与装备, 2008; 29(3): 74)
[9] Gu J J, Qin Y Q, Chen Z L, Lu Q H.Hot Working Technol, 2010; 39(22): 160
[9] (顾俊杰, 秦优琼, 陈志林, 卢庆华. 热加工工艺, 2010; 39(22): 160)
[10] Chu J H, Liu S Y.Heavy Castings Forgings, 2007; (4): 6
[10] (褚锦辉, 刘时雨. 大型铸锻件, 2007; (4): 6)
[11] Wang M L, Wang J, Wang L X.Bearing, 2009; (12): 37
[11] (王明礼, 王 建, 王丽霞. 轴承, 2009; (12): 37)
[12] Li J, Chen Z W, Liu D K.Heavy Castings Forgings, 2000; (4): 25
[12] (李 进, 陈增武, 刘定坤. 大型铸锻件, 2000; (4): 25)
[13] Wang X T, Yao Y L, Shao T H.Acta Metall Sin,1990; 26: 40
[13] (王笑天, 姚引良, 邵谭华. 金属学报, 1990; 26: 40)
[14] Dhua S K, Ray A, Sarma D S. Mater Sci Eng, 2001; A318: 197
[15] Liu D Y, Xu H, Yang K, Bai B Z, Fang H S. Acta Metall Sin, 2004; 40: 882
[15] (刘东雨, 徐 鸿, 杨 昆, 白秉哲, 方鸿生. 金属学报, 2004; 40: 882 )
[16] Gao G H, Zhang H, Bai B Z.Acta Metall Sin, 2011; 47: 513
[16] (高古辉, 张 寒, 白秉哲. 金属学报, 2011; 47: 513)
[17] Zhang C Y, Wang Q F, Ren J X, Li R X, Wang M Z, Zhang F C, Yan Z S.Mater Des, 2012; 36: 220
[18] Zhang P, Zhang F C, Wang T S.Acta Metall Sin, 2011; 47: 1038
[18] (张 朋, 张福成, 王天生. 金属学报, 2011; 47: 1038)
[19] Wang R F, Xu K, Xue G.Hot Work Technol, 2007; 36(16): 43
[19] (王仁甫, 徐 科, 薛 钢. 热加工工艺, 2007; 36(16): 43)
[20] Bakhtiari R, Ekrami A.Mater Sci Eng, 2009; A525: 159
[21] Jiang W C, Gong J M, Chen H, Tu S D. Acta MetallSin, 2008; 44: 105
[21] (蒋文春, 巩建明, 陈 虎, 涂善东. 金属学报, 2008; 44: 105)
[22] Cao P Z, Liu G Z, Wu K.Int J Mater Mech Eng, 2012; (1): 16
[23] Yang X W, Zhu J C, Nong Z S, Lai Z H, He D.Comput Mater Sci, 2013; 69: 396
[24] Caner Simsir, Hakan Gur C.J Mater Process Technol, 2008; 207: 211
[25] Simulia Abaqus User Manual Version 6. 10, 2009
[26] Chen J D, Mo W L, Wang P, Lu S P.Acta Metall Sin, 2012; 48: 1186
[26] (陈俊丹, 莫文林, 王 培, 陆善平. 金属学报, 2012; 48: 1186)
[27] Cheng B S, Xiao N M, Li D Z, Li Y Y.Acta Metall Sin, 2012; 48: 696
[27] (程柏松, 肖纳敏, 李殿中, 李依依. 金属学报, 2012, 48: 696)
[28] Yin Z X, Yu W C, Yao G, Yang Z G, Li S X, Ma C X.Iron Steel, 2002; 37(10): 52
[28] (尹志新, 于维成, 姚 戈, 杨振国, 李守新, 马常祥. 钢铁, 2002; 37(10): 52)
Outlines

/

〈 〉