Original Articles

PHASE FIELD CRYSTAL SIMULATION OF DISLOCA- TION MOVEMENT AND REACTION

  • Yingjun GAO ,
  • Chengjian LU ,
  • Lilin HUANG ,
  • Zhirong LUO ,
  • Chuanggao HUANG
Expand
  • 1 College of Physics Science and Engineering, Guangxi University, Nanning 530004
    2 Guangxi Key Laboratory for Non-ferrous Metal and Featured Materials, Guangxi University, Nanning 530004
    3 Institute of Physics Science and Engineering Technology, Yulin Normal University, Yulin 537000

Received date: 2013-06-04

  Revised date: 2013-06-04

  Online published: 2014-01-11

Supported by

Supported by National Natural Science Foundation of China (Nos.51161003 and 50661001), Natural Science Foundation of Guangxi Province (No.2012GXNSFDA053001), Foundation of Guangxi Key Laboratory of Processing for Non-ferrous Metal and Featured Materials (No.GXKFJ12-01) and Science Foundation of Guangxi University (No.XJZ110611)

Abstract

Transformations of grain boundaries often strongly influence both the structure and the properties of polycrystalline and nanocrystalline materials. Thus, plastic deformation processes in fine-grained polycrystals and nanocrystalline solids are associated with transformations of grain boundaries, which crucially affect the structure and mechanical characteristics of such solids. Motion of grain boundary dislocations in plastically deformed materials is commonly considered to be the absorption of lattice dislocations by grain boundaries. In order to reveal the mechanism of motion of a low-angle symmetric tilt grain boundary (STGB) associated with the emission and absorption of lattice dislocation, the emission and evolution of a STGB under strain were simulated by phase-field crystal (PFC) model. The decay of STGB and dislocation reactions of separation, annihilation and mergence and their mechanisms were analyzed from the energy point of view, furthermore, the active energy of the dislocation separation was calculated. The research results show that the low-angle STGB is composed of pair dislocations in a line arrangement in two dimensions of triangular atomic lattice, in which there are two sets of basic Burgers vectors. The evolution process of STGB decay can be divided into six typical stages which includes the detail features as: dislocation climbs firstly along the STGB under strain, then the dislocation occurs to break up into two new dislocations after it gets enough energy to overcome the active potential barrier of dislocation, at this time the STGB emits pair dislocations to move in gliding in grain instead of climbing along STGB; gliding for while, the dislocation crosses the grain until it is annihilated by another dislocation at the STGB right in the front, i.e. the Grain boundary absorbs or merges the gliding dislocation. The remain of dislocation in the STGB can still climb along the grain boundary in which splits off again into two dislocations when it gets enough energy, at the same time it looks as if STGB emits the dislocations and changes the dislocation movement from climbing to gliding again. The dislocation continues gliding until it meets another gliding dislocation in grain to be annihilated, finally the total dislocations are annihilated and the STGB disappears. The two grain systems with STGB become one grain system. The two sets of basic Burgers vectors of lattice dislocation in triangular lattice can validly be used to express the dislocation reaction of emission, separation, mergence, absorption, annihilation, and also can reveal the creation of new Burgers vector and the annihilation of old Burgers vectors and mechanism of the directional change of Burgers vectors during the dislocation reaction.

Cite this article

Yingjun GAO , Chengjian LU , Lilin HUANG , Zhirong LUO , Chuanggao HUANG . PHASE FIELD CRYSTAL SIMULATION OF DISLOCA- TION MOVEMENT AND REACTION[J]. Acta Metall Sin, 2014 , 50(1) : 110 -120 . DOI: 10.3724/SP.J.1037.2013.00308

References

[1] Xu H J,Liu G X. Fundamentals of Materials Science. Beijing: Beijing University of Technology Press, 2001: 265
[1] (徐恒均,刘国勋. 材料科学基础. 北京: 北京工业大学出版社, 2001: 265)
[2] Hu G X,Cai X. Fundamentals of Materials Science. Shanghai:Shanghai Jiao Tong University Press, 2010: 99
[2] (胡赓祥,蔡 珣. 材料科学基础. 上海: 上海交通大学出版社, 2010: 99)
[3] Bobylev S V, Ovid’ko I A.Phys Rev, 2003; 67B: 132506
[4] Ovidko I A, Skiba N V.Scr Mater, 2012; 67: 13
[5] Gukkin M Y, Ovidko I A.Phys Rev, 2001; 63B: 064515
[6] Gukkin M Y, Ovidko I A.Acta Mater, 2004; 52: 3793
[7] Hayakawa M, Yamaguchi K, Kimura M.Mater Lett, 2004; 58: 2565
[8] Elder K R, Katakowski M, Haataja M, Grant M.Phys Rev Lett, 2002; 88: 245701
[9] Elder K R, Grant M. Phys Rev, 2004; 70E: 51605
[10] Stefanovic P, Haataja M, Provatas N.Phys Rev, 2009; 80E: 046107
[11] Berry J, Grant M, Elder K R.Phys Rev, 2006; 73E: 31609
[12] Pan S Y, Zhu M F.Acta Phys Sin, 2012; 61: 228102
[12] (潘诗琰, 朱鸣芳. 物理学报, 2012; 61: 228102)
[13] Chen Y, Kang X H, Li D Z.Acta Phys Sin, 2009; 58: 390
[13] (陈 云, 康秀红, 李殿中. 物理学报, 2009; 58: 390)
[14] Gao Y J, Luo Z R, Zhang S Y, Huang C G.Acta Metall Sin, 2010; 46: 1473
[14] (高英俊, 罗志荣, 张少义, 黄创高. 金属学报, 2010; 46: 1473)
[15] Yang T, Chen Z, Dong W P.Acta Metall Sin, 2011; 47: 1301
[15] (杨 涛, 陈 铮, 董卫平. 金属学报, 2011; 47: 1301)
[16] Ren X, Wang J C, Yang Y J, Yang G C.Acta Phys Sin, 2010; 59: 3595
[16] (任 秀, 王锦程, 杨玉娟, 杨根仓, 物理学报, 2010; 59: 3595 )
[17] Gao Y J, Wang J F, Luo Z R, Lu Q H, Liu Y. Chin J ComputPhys, 2013; 30: 577
[17] (高英俊, 王江帆, 罗志荣, 卢强华, 刘 瑶. 计算物理, 2013; 30: 577)
[18] Elder K R, Huang Z, Provatas N.Phys Rev, 2010; 81E: 11602
[19] Yu Y M, Backofen R, Voigt A.J Cryst Growth, 2011; 318: 18
[20] Elder K R, Rossi G, Kanerva P, Sanches F, Ying S C, Granato E, Achim C V, Ala-Nissila T.Phys Rev Lett, 2012; 108: 226102
[21] Gao Y J, Luo Z R, Huang C G, Lu Q H, Lin K.Acta Phys Sin, 2013; 62: 050507
[21] (高英俊, 罗志荣, 黄创高, 卢强华, 林 葵. 物理学报, 2013; 62: 050507)
[22] Greenwood M, Rottler J, Provatas N. Phys Rev, 2011; 83B: 031601
[23] Berry J, Elder K R, Grant M. Phys Rev, 2008; 77B: 224114
[24] Gao Y J, Luo Z R, Huang L L, Lin K.Chin J Nonferrous Met, 2013; 23: 1892
[24] (高英俊, 罗志荣, 黄礼琳, 林 葵. 中国有色金属学报, 2013; 23: 1892)
[25] Chen L Q, Shen J.Comput Phys Commun, 1998; 108: 147
[26] Hirouchi T, Takaki T, Tomita Y.Int J Mech Sci, 2010; 52: 309
[27] Gao Y J, Luo Z R, Hu X Y, Huang C G.Acta Metall Sin, 2010; 46: 1161
[27] (高英俊, 罗志荣, 胡项英, 黄创高. 金属学报, 2010; 46: 1161)
[28] Gao Y J, Luo Z R, Huang L L, Hu X Y.Acta Metall Sin, 2012; 48: 1215
[28] (高英俊, 罗志荣, 黄礼琳, 胡项英. 金属学报, 2012; 48: 1215)
[29] Wu K A, Voorhees P W.Acta Mater, 2012; 60: 407
[30] Mills M J, Daw M S, Foiles S M.Ultramicroscopy, 1994; 56: 79
[31] Shao Y F, Yao X, Zhao X, Wang S Q.Chin Phys, 2012; 21B: 083101
Outlines

/

〈 〉