Abstract

DZ468 alloy is a promising candidate in turbine blade serving in marine atmosphere because of its superior mechanical properties and good hot corrosion resistance. And brazing technology is indispensable to produce turbine blade because of its complicated hollow structure. Therefore, for accelerating the application of DZ468 superalloy, a new type Co-based filler named BCo46 was developed. Due to serving in marine atmosphere, the attack of hot corrosion can be inevitable. Frequently, the quality of turbine blade depends on the joining region, and the joining region has a lot to do with the filler used to braze the base alloy. Therefore, in this work, the hot corrosion behavior and mechanism of BCo46 alloy in the mixture of 75%Na2SO4 + 25%NaCl (mass fraction) at 900 ℃ was investigated, and compared with a common Ni-based filler BNi-2, and the base alloy DZ468. Moreover, the hot corrosion resistance of the joint bonded with BCo46 was evaluated. XRD, SEM, EDS and ICP spectrograph were employed to study the corrosion products of the tested alloys. The results show that the hot corrosion processes of BCo46, BNi-2 and DZ468 alloys are all accompanied with the dissolution of oxide scale and the formation of sulfide, which support the model of sulfidation-(acid-based) melting model. For filler alloy BCo46, Cr2O3, Co3BO5 and (Ni, Co)Cr2O4 mainly exist in the outer corrosion layer and some CrS is formed in the inner corrosion layer; the external corrosion products of BNi-2 are NiO, (Ni, Co)Cr2O4, Ni2FeBO5 and Cr2O3, and the internal precipitation is Ni2S3. The hot corrosion resistance of filler alloy BCo46 is superior to DZ468 superalloy and BNi-2 filler, it is because (1) BCo46 contains 22% Cr which can form dense and continuous oxide scale Cr2O3; (2) the diffusion rates of O and S are slower in Co- than Ni-based alloy; (3) Co can increase the adhesion of the oxide scale-base metal; (4) collaboration dissolution doesn't occur in BCo46. Furthermore, the formation of boride can deteriorate the hot corrosion resistance of alloy by forming oxides of boron which can dissolve oxide scale, consume Cr and increase phase interfacial area to accelerate the diffusion of S and O. The joint after heat treatment can reach the level of the hot corrosion resistance of the base metal DZ468.

Key words: BCo46; DZ468; hot corrosion; filler

Cite this article

Yanhong JING , Enze LIU , Zhi ZHENG , Jian TONG , Likui Ning , Ping HE . HOT CORROSION RESISTANCE OF FILLER ALLOY BCo46[J]. Acta Metall Sin, 2014 , 50(1) : 79 -87 . DOI: 10.3724/SP.J.1037.2013.00216

References

[1] Zhao D Z.Equip Environ Eng, 2011; 8(5): 100
[1] (赵德孜. 装备环境工程, 2011; 8(5): 100)
[2] Ning L K, Zheng Z, Tan Y, Liu E Z, Tong J, Yu Y S, Wang H.Acta Metall Sin, 2009; 45:161
[2] (宁礼奎, 郑 志, 谭 毅, 刘恩泽, 佟 健, 于永泗, 王 华. 金属学报, 2009; 45: 161)
[3] Liu E Z, Sun S C, Tu G F, Zheng Z, Ning L K, Zhang L F.Acta Metall Sin, 2009; 45: 1217
[3] (刘恩泽, 孙树臣, 涂赣峰, 郑 志, 宁礼奎, 张凌峰. 金属学报, 2009; 45: 1217)
[4] Jing Y H,Zheng Z,Liu E Z,Guo Y. J Mater Sci Technol, 2014; 30(in press)
[5] Stringer J.Mater Sci Technol, 1987; 3: 482
[6] Lee W H, Lin R Y.Mater Chem Phys, 2002; 77: 86
[7] Li M H, Sun X F, Hu W Y, Guan H R, Chen S G. Oxid Met, 2006; 65: 137
[8] Simons E L, Browning G V, Liebhafsky H A.Corrosion, 1955; 11: 505
[9] Zhu R Z, Zuo Y, Guo M J.Acta Matell Sin, 1985; 21: 451
[9] (朱日彰, 左 禹, 郭曼玖. 金属学报, 1985; 21: 451)
[10] Bornstein N S, Decrescent M A.Trans AIME, 1969; 245: 583
[11] Quets J M, Dresher W H.J Mater, 1969; 4: 583
[12] Rapp R A, Goto K S. In: Braunstein J, Selman J R eds., Proceedings of the Second International Symposium on Molten Salts, Pennington: the Electrochemical society, 1981: 159
[13] Park C O, Rapp R A.Electrochem Sci Technol, 1986; 133: 1636
[14] Tzvetkoff T Z, Girginov A.J Mater Sci, 1995; 30: 5561
[15] Liu E Z, Sun S C.Heat Treat Met, 2009; 34(6): 84
[15] (刘恩泽, 孙树臣. 金属热处理, 2009; 34(6): 84)
[16] Lu S P, Guo Y, Chen L S.Mater Rev, 1999; 13(6): 58
[16] (陆善平, 郭 义, 陈亮山. 材料导报, 1999; 13(6): 58)
[17] Zhuang H S,Lugscheider E. High Temperature Brazing. Beijing: National Defence Industry Press, 1989: 46
[17] (庄鸿寿,Lugscheider E. 高温钎焊. 北京: 国防工业出版社, 1989: 46)
[18] Ning L K. Master Thesis, Dalian University of Technology, 2008
[18] (宁礼奎. 大连理工大学硕士学位论文, 2008)
[19] Fryburg G C, Kohl F J, Stearns C A.J Electrochem Soc, 1984; 131: 2985
[20] Fryburg G C, Kohl F J, Stearns C A.J Electrochem Soc, 1982; 129: 571
[21] Gupta D K.J Electrochem Soc, 1980; 127: 2194
[22] Rapp R A.Mater Sci Eng, 1987; 87: 568
[23] Li T F. High Temperature Oxidation and Hot Corrosion of Metal. Beijing: Chemical Industrial Press, 2003: 203
[23] (李铁藩. 金属高温氧化和热腐蚀. 北京: 化学工业出版社, 2003: 203)
[24] Guan D L, Lu Z H, Xiao Y T, Shi C X.J Chin Soc Corros Prot, 1981; 1: 49
[24] (关德林, 陆之汉, 肖耀天, 师昌绪. 中国腐蚀与防护学报, 1981; 1: 49)
[25] Goebel J A, Pettit F S.Metall Trans, 1970; 1: 1943
[26] Beltran A M. Superalloys II. New York: Wiley, 1987: 135
[27] Chao J H, Kim T W, Son K S.Met Mater Int, 2003; 9: 303
Outlines

/

〈 〉