Original Articles

ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY MONITORING ON MILD STEEL Q235 IN SIMULATED INDUSTRIAL ATMOSPHERIC CORROSION ENVIORNMENT

  • Xinxin FU ,
  • Junhua DONG ,
  • En-hou HAN ,
  • Wei KE
Expand
  • State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-05-22

  Revised date: 2013-05-22

  Online published: 2014-01-11

Supported by

Supported by National Natural Science Foundation of China (No.50499336)

Abstract

As mild steels are the most widely used structure materials, it is no doubt that the study on their atmospheric corrosion mechanism is of great significance. Traditional study on atmospheric corrosion of mild steels emphasized more on on-site experiments and data collection and physical analysis. Relatively, application of electrochemical researching methods has not been frequently used in this field. Electrochemical impedance spectroscopy (EIS) method has been highly valued by electrochemists due to its multiple advantages. However, it has been less used in study of corrosion process of mild steels after the rust has been generated. As a matter of fact, during the service life of mild steel in atmospheric environments, the rust period is much longer than naked steel period due to the low corrosion resistance of these steels. Therefore, it is more meaningful to study the corrosion behavior of steels with rusts both for development of new weathering steels and for the prediction of the service life of weathering steels. In this work, the corrosion behavior of mild steel Q235 under simulated industrial atmospheric corrosive condition was monitored and studied by EIS method, with a focus on the evolution of cathode reactions. The result showed that there existed a critical condition of electrolyte film for corrosion rate of mild steel Q235 both for the substrate and rusted surface during wet-dry cycles. Comparison and analysis showed that, two parallel reactions, the reduction of oxygen and the reduction of rust, existed at the cathode during the corrosion process. With the increase of the wet-dry cycles, the activity of oxygen reduction tended to decrease, and almost disappeared in the end; while the activity of rust deduction tended to increase and became the main cathode reaction in a short period. In each wet-dry cycle, the corrosion rate first increased then decreased with the decrease of the electrolyte layer thickness, which was caused by the two synchronous and opposite effects on the corrosion reactions.

Cite this article

Xinxin FU , Junhua DONG , En-hou HAN , Wei KE . ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY MONITORING ON MILD STEEL Q235 IN SIMULATED INDUSTRIAL ATMOSPHERIC CORROSION ENVIORNMENT[J]. Acta Metall Sin, 2014 , 50(1) : 57 -63 . DOI: 10.3724/SP.J.1037.2013.00278

References

[1] Ke W. China Corrosion Survey Report. Beijing: Chemical Industry Press, 2003: 1
[1] (柯 伟. 中国腐蚀调查报告. 北京: 化学工业出版社, 2003: 1)
[2] Leygraf C,Graedel T,Translated byHan E H,et al. Atmospheric Corrosion. Beijing: Chemical Industry Press, 2005: 2
[2] (Leygraf C,Graedel T 著;韩恩厚 等译. 大气腐蚀. 北京: 化学工业出版社, 2005: 2)
[3] Nishimura T, Katayama H, Noda K, Kodama T.Corrosion, 2000; 56: 934
[4] Friel J J.Corrosion, 1986; 42: 422
[5] Munier G B, Psota L A, Reagor B T, Russiello B, Sinclair J D.J Electrochem Soc, 1980; 127: 265
[6] Oesch S.Corros Sci, 1996; 38: 1357
[7] ?zcan M, Dehri ?, Erbil M.Prog Org Coat, 2002; 44: 279
[8] Abdel S H, Sa’eh A G, Shoeib M A, Barakat Y.Electrochim Acta, 2007; 52: 7068
[9] Peter S, Sudipta R, David S, Stephen M, David P, John L.Chem Eng Sci, 2011; 66: 5775
[10] Zhang X Y, Han E H, Li H X.J Chin Soc Corros Prot, 2002; 22: 316
[10] (张学元, 韩恩厚, 李洪锡. 中国腐蚀与防护学报, 2002; 22: 316)
[11] An B G, Zhang X Y, Han E H, Li H X.Acta Metall Sin, 2002; 38: 755
[11] (安百刚, 张学元, 韩恩厚, 李洪锡. 金属学报, 2002; 38: 755)
[12] Scully J C,Translated by Li Q Z . The Fundamentals of Corrosion. Beijing: China Water Power Press, 1984: 108
[12] (J C 斯库里 著;李启中 译. 腐蚀原理. 北京: 水利电力出版社, 1984: 108)
[13] Evans U R, Taylor C A.Corros Sci, 1972; 12: 227
[14] Evans U R, Taylor C A.Corros Sci, 1986; 8: 447
[15] Evans U R.Corros Sci, 1969; 9: 813
[16] Nishikata A, Ichihara Y, Tsuru T.Corros Sci, 1995; 6: 897
[17] Nishikata A, Yamashita Y, Katayama H, Tsuru T. Corros Sci,1995; 12: 2059
[18] Nishikata A, Ichihara Y, Tsuru T. Electrochim Acta, 1996; 7-8:1057
[19] Nishikata A, Ichihara Y, Hayashi Y, Tsuru T.J Electrochem Soc, 1997; 4: 1244
[20] Katayama H, Noda K, Masuda H, Nagasawa M, Itagaki M, Watanabe K.Corros Sci, 2005; 47: 2599
[21] Dong J, Dong J H, Han E H, Liu C M, Ke W.Corros Sci Prot Technol, 2006; 18: 414
[21] (董 杰, 董俊华, 韩恩厚, 刘春明, 柯 伟. 腐蚀科学与防护技术, 2006; 18: 414)
[22] Fu X X, Dong J H, Han E H, Ke W.Sensors, 2009; 9: 10400
[23] Tomashov N D.Corrosion, 1964; 20: 7t
[24] Zhang Q C, Wu J S, Zheng W L, Chen J G, Li A B, Wang J J, Yang X F.Mater Rev, 2000; 14(7): 12
[24] (张全成, 吴建生, 郑文龙, 陈家光, 李爱柏, 王建军, 杨晓芳. 材料导报, 2000; 14(7): 12)
[25] Cao C N,Zhang J Q. Introduction to Electrochemical Impedance Spectroscopy. Beijing: Science Press, 2002: 20
[25] (曹楚南,张鉴清. 电化学阻抗谱导论. 北京: 科学出版社, 2002: 20)
Outlines

/

〈 〉