INFLUENCE OF HEAT TREATMENT ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A HIGH-STRENGTH Zr-Ti ALLOY

  • Ye LI ,
  • Long ZHANG ,
  • Zhengwang ZHU ,
  • Hong LI ,
  • Aimin WANG ,
  • Haifeng ZHANG
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-08-19

  Revised date: 2013-08-19

  Online published: 2014-01-11

Supported by

Supported by National Basic Research Program of China (No.2010CB731602)

Abstract

Due to the high stress, relative low density and excellent resistance of radiation, Zr-based alloys have become promising structural materials used in the space environment. The relationship between microstructure and mechanical properties is the key issue for designing Zr-based alloy in different alloy systems and has attracted extensive research interests. The microstructures could be adjusted by different processes of heat treatment and thus realizing the optimization of mechanical properties. In this work, the initial microstructure and mechanical properties of a high strength Zr47Ti45Al5V3 (mass fraction, %) alloy was investigated. The XRD results reveal that the initial Zr-based alloy is consisted of α (hcp) and β (bcc) phases. Transmission electron microscopy result shows that the lathy α phase homogenously distributed within the β phase matrix. Mechanical tests of this alloy show very high strength but limited plasticity. The tensile strength is 1648 MPa. However, the tensile elongation is only 0.8%. DSC trace indicates that the transition temperature of α phase to β phase is located between 560~750 ℃ that provides the possibility to adjust the microstructures through different processes of heat treatment. In order to optimize the mechanical properties, several different processes of heat treatment were conducted on this Zr-based alloy, and the relative volume fraction of α and β phase is successfully adjusted. According to the mechanical tests, the plasticity becomes larger as the amount of β phase increases with a slight decrease in strength. When the volume fraction of β phase is about 60%, the alloy exhibits the optimal mechanical performance with a tensile strength of 1398 MPa and an elongation of 3.1%.

Cite this article

Ye LI , Long ZHANG , Zhengwang ZHU , Hong LI , Aimin WANG , Haifeng ZHANG . INFLUENCE OF HEAT TREATMENT ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A HIGH-STRENGTH Zr-Ti ALLOY[J]. Acta Metall Sin, 2014 , 50(1) : 19 -24 . DOI: 10.3724/SP.J.1037.2013.00498

References

[1] Wang S H, Yang D Z, He S Y, Lv G.Mater Sci Technol, 2004; 6: 579
[1] (王淑花, 杨德庄, 何世禹, 吕 钢. 材料科学与工艺, 2004; 6: 579)
[2] Li X, Wang L, Yu X M.Mater Sci Eng, 2013; A33: 2987
[3] Tribble A. The Space Environment-Implications for Spacecraft Design. New Jersey: Princeton University Press, 1995: 1
[4] Lowenstein D I, Rusek A.Ridiat Environ Bioph, 2007; 46: 91
[5] Shilobreeva S N, Kashkarov L L, Barabanenkov M Y, Pustovit A N, Zinenko V I, Agafonov Y A.Dokl?Earth?Sci, 2006; 411: 9
[6] Qian J,Zhu Y L,Feng Y Y,Li F B. The Basic of Space Technology. Beijing: Science Press, 1986: 520
[6] (钱 骥,朱毅麟,冯英远,李凡本. 空间技术基础. 北京: 科学出版社, 1986: 520)
[7] Zhao W J, Zhou B X, Miao Z, Peng F, Jiang Y R, Jiang H M, Pang H.Atom Energy Sci Technol, 2005; 39(suppl): 2
[7] (赵文金, 周邦新, 苗 志, 彭 傅, 蒋有荣, 蒋宏曼, 庞 华. 原子能科学与技术, 2005; 39(增刊): 2)
[8] Wicklein M, Ryan S, White D M, Clegg R A.Int J Impact Eng, 2008; 35: 1861
[9] Sakuraba K, Tsuruda Y, Hanada T, Liou J C, Akahoshi Y.Int J Impact Eng, 2008; 35: 1567
[10] Sorensen B R, Kimsey K D, Love B M.Int J Impact Eng, 2008; 35: 1808
[11] Nomura N, Oya K, Tanaka Y, Kondo R, Doi H,TsutsumiY,HanawaT.ActaBiol,2010:6:1033
[12] Hsu H C, Wu S C, Sung Y C, Ho W F.J Alloys Compd, 2009; 488: 279
[13] Dey G K, Banerjee S.Mater Sci Eng, 1985; A73: 187
[14] Lee M H, Kim J H, Choi B K, Jeong Y H.J Alloys Compd, 2007; 428: 99
[15] Dobromyslov A V, Kazantseva N V.Scr Mater, 1997; 37: 615
[16] Liang S X, Ma M Z, Jing R, Zhang X Y, Liu R P.Mater Sci Eng, 2012; A532: 1
[17] Ho W F, Cheng C H, Chen W K, Wu S C, Lin H C, Hsu H C.J Alloys Compd, 2009; 471: 185
[18] Thibon I, Ansel D, Gloriant T. J Alloys Compd, 2009; 470: 127
[19] Nakasuji K, Okada M.Mater Sci Eng, 1996; A213: 162
[20] Ho W F, Chen W K, Wu S C, Hsu H C.J Mater Sci, 2008; 19: 3179
[21] Sauer C, Luetjering G. J Mater Process Technol, 2001; 117: 311
[22] Liang S X, Ma M Z, Jing R, Zhang X Y, Liu R P.Mater Sci Eng, 2012; A539: 42
[23] Lu G. Mater Sci Eng, 1998; A243: 32
[24] Wang J, Zhang H W, Wang A M, Li H, Fu H M, Zhu Z W, Zhang H F.Acta Metall Sin, 2012; 48: 636
[24] (王 杰, 张宏伟, 王爱民, 李 宏, 付华萌, 朱正旺, 张海峰. 金属学报, 2012; 48: 636)
[25] Kim T K, Choi B S, Jeong Y H, Lee D J, Chang M H. J Nucl Mater, 2002; 301: 81
Outlines

/

〈 〉