Original Articles

EFFECT OF GRAIN BOUNDARY ANGLE ON STRESS RUPTURE PROPERTIES OF A Ni-BASED BICRYSTAL SUPERALLOY

  • Liang CAO ,
  • Yizhou ZHOU ,
  • Tao JIN ,
  • Xiaofeng SUN
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
null

曹亮, 女, 1981 年生, 博士生

Received date: 2013-06-24

  Revised date: 2013-06-24

  Online published: 2014-01-11

Supported by

Supported by National Natural Science Foundation of China (Nos.U1037601, 51271186 and 51001103), National Basic Research Program of China (No.2010CB631206) and Program of “One Hundred Talented People” of the Chinese Academy of Sciences

Abstract

Bicrystal slabs with different grain boundary angles were cast to study the effect of varied grain boundary angle on stress rupture properties of a Ni-based bicrystal superalloy. It was found that the stress rupture lives of single crystal specimens were superior to those with grain boundaries. With the increase of grain boundary angle, the stress rupture life was decreased and the fracture type was transferred from trans-granular to inter-granular fracture. The reduced rupture properties was attributed to the inhabitation of grain boundary on slip deformation. With the rise of temperatures, the effect of grain boundaries on rupture properties was enhanced and the critical value of grain boundary angle from trans-granular to inter-granular fracture was decreased. Inter-granular fracture occurred from 12° grain boundary in the rupture test of 871 ℃ and 552 MPa, and it occurred from 4.5° grain boundary in the rupture test of 1100 ℃ and 120 MPa. Since the grain boundary became weaker at higher temperature, the angle of low-angle boundary in single crystal superalloys should be controlled strictly.

Cite this article

Liang CAO , Yizhou ZHOU , Tao JIN , Xiaofeng SUN . EFFECT OF GRAIN BOUNDARY ANGLE ON STRESS RUPTURE PROPERTIES OF A Ni-BASED BICRYSTAL SUPERALLOY[J]. Acta Metall Sin, 2014 , 50(1) : 11 -18 . DOI: 10.3724/SP.J.1037.2013.00342

References

[1] Jia Y X, Jin T, Liu J L, Sun X F, Hu Z Q.Acta Metall Sin, 2009; 45: 1364
[1] (贾玉贤, 金 涛, 刘金来, 孙晓峰, 胡壮麒. 金属学报, 2009; 45: 1364)
[2] Zhou Y Z, Jin T, Sun X F.Acta Metall Sin, 2010; 46: 1327
[2] (周亦胄, 金 涛, 孙晓峰. 金属学报, 2010; 46: 1327)
[3] Pollock T M, Murphy W H, Goldman E H, Uram D L, Tu J S. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Champion, PA: TMS, 1992: 125
[4] Bussac A, Gandin C.Mater Sci Eng, 1997; A237: 35
[5] Tamaki H, Yoshinari A, Okayama A, Nakamura S, Kageyama K, Sato K, Ohno T. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000. Reno, NV: TMS, 2000: 757
[6] Chandra N, Dang P.J Mater Sci, 1999; 34: 655
[7] Gottstein G, Shvindlerman L S.Scr Metall Mater, 1992; 27: 1515
[8] Tavakkoli M M, Abbasi S M.Mater?Des, 2013; 46: 573
[9] Zheng L, Xu T D, Deng Q, Dong J X.Mater Lett, 2008; 62: 54
[10] Ping D H, Gu Y F, Cui C Y, Harada H.Mater Sci Eng, 2007; A456: 99
[11] Ross E W, O′hara K S. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollok T M, Woodford D A eds., Superalloys 1996, Champion, PA: TMS, 1996: 19
[12] Shah D M, Cetel A. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, Mclean M, Olson S, Schirra J J eds., Superalloys 2000, Reno, NV: TMS, 2000: 295
[13] Nitta H, IijimaY, Tanaka K, Yamazaki Y, Lee CG, Matsuzaki T, Watanabe T.Mater Sci Eng, 2004; A382: 250
[14] Zhou Y Z.Scr Mater, 2011; 65: 281
[15] Zhou Y Z, Volek A, Green N R.Acta Mater, 2008; 56: 2631
[16] Zhou Y Z, Green N R. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds., Superalloys 2008, Champion, PA: TMS, 2008: 317
[17] Zhou Y Z, Volek A.Scr Mater, 2006; 54: 2169
[18] Peralta P, Schober A, Laird C.Mater Sci Eng, 1993; A169: 43
[19] Wang G J.Central Iron Steel Res Inst Tech Bull, 1986; 6(4): 25
[19] (王桂金. 钢铁研究学报, 1986; 6(4): 25)
[20] Liu L R. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2004
[20] (刘丽荣. 中国科学院金属研究所博士学位论文, 沈阳, 2004)
[21] Maclachlan D W, Knowles D M.Mater Sci Eng, 2001; A302: 275
[22] Savitsky E M,translated by Duan Z. Effect of Temperature on the Metal and Alloy Mechanical Properties Beijing: China Industry Press, 1965: 33
[22] (Савицкий E M著,段 中 译. 温度对金属及合金机械性能的影响. 北京: 中国工业出版社, 1965: 33)
[23] Friedel J,translated by Wang Y. Dislocations. Beijing: Science Press, 1980: 215
[23] (Friedel J 著,王 煜 译. 位错. 北京: 科学出版社, 1980: 215)
Outlines

/