INFLUENCE OF MELT HOLDING TEMPERATURES ON MECHANICAL PROPERTIES AT ROOM TEMPERATURE OF Wf/Zr-BASED METALLIC GLASS COMPOSITES

  • GAO Du ,
  • CHEN Guang ,
  • FAN Cang
Expand
  • Engineering Research Center of Materials Behavior and Design,Ministry of Education, Nanjing University of Science and Technology, Nanjing 210094

Received date: 2013-09-02

  Revised date: 2013-09-23

  Online published: 2013-11-11

Abstract

The effect of the molten temperatures on the preparation of the Wf/Zr-based metallic glass composites by infiltration casting rapid quenching technique was well studied. The results of the mechanical properties at ambient temperature indicate that the composite has an optimum melt holding temperature in the preparation process. Lower or higher than the optimum temperature, the compressive plasticity of the composite deteriorated. The optical microstructure and EDS analyses indicate that the reason for the deterioration of the compressive plasticity was the resulted microstructures, which contains different precipitates with different molten temperatures. At the optimum preparation condition, a Wf/Zr--based metallic glass composite with 75% volume fraction of tungsten fiber was successfully produced with significantly improved compressive plasticity of 19.6%.

Cite this article

GAO Du , CHEN Guang , FAN Cang . INFLUENCE OF MELT HOLDING TEMPERATURES ON MECHANICAL PROPERTIES AT ROOM TEMPERATURE OF Wf/Zr-BASED METALLIC GLASS COMPOSITES[J]. Acta Metall Sin, 2013 , 49(11) : 1481 -1486 . DOI: 10.3724/SP.J.1037.2013.00541

References

[1] Johnson W L.  MRS Bull, 1999; 24: 42

[2] Inoue A.  Acta Mater, 2000; 48: 279
[3] Ashby M F, Greer A L.  Scr Mater, 2006; 54: 321
[4] Schuh C A, Hufnagel T C, Ramamurty U.  Acta Mater, 2007; 55: 4067
[5] Greer A L.  Mater Today, 2009; 12: 14
[6] Zhang Z F, Eckert J, Schultz L.  Acta Mater, 2003; 51: 1167
[7] Eckert J, Das J, Pauly S, Duhamel C.  J Mater Res, 2007; 22: 285
[8] Wu F F, Zhang Z F, Mao S X, Peker A, Eckert J.  Phys Rev, 2007; 75B: 134201
[9] Wang Z H, Chen G, Jiang F, Du Y L, Chen G L.  Rare Met Mater Eng, 2006; 35: 1568
(王志华, 陈光, 姜斐, 杜宇雷, 陈国良. 稀有金属材料与工程, 2006; 35: 1568)
[10] Conner R D, Dandliker R B, Johnson W L.  Acta Mater, 1998; 46: 6089
[11] Dandliker R B, Conner R D, Johnson W L.  J Mater Res, 1998; 13: 2896
[12] Kim C P, Busch R, Masuhr A, Choi--Yim H, Johnson W L.  Appl Phys Lett, 2001;79: 1456
[13] Bian Z, Pan M X, Zhang Y, Wang W H.  Appl Phys Lett, 2002; 81: 4739
[14] Qiu K Q, Wang A M, Zhang H F, Ding B Z, Hu Z H.  Intermetallics, 2002; 10: 1283
[15] Wang G, Chen D M, Shen J, Stachurski Z H, Qin Q H, Sun J F, Zhou B D.J Non-Cryst Solids, 2006; 352: 3872
[16] Wadhwa P, Heinrich J, Busch R.  J Alloys Compd, 2007; 434--435: 259
[17] Zhang H, Zhang Z F, Wang Z G, Zhang H F.  Mater Sci Eng, 2008; A483--484: 164
[18] Zhang X C, Chen X H, Zhang Y, Chen G L.  Rare Met Mater Eng, 2008; 37: 786
(张兴超, 陈晓华, 张勇, 陈国良. 稀有金属材料与工程, 2008; 37: 786)
[19] Lee K, Son C Y, Lee S B, Lee S K, Lee S.  Mater Sci Eng, 2010; A527: 941
[20] Deng S T, Diao H, Chen Y L, Yan C, Zhang H F, Wang A M, Hu Z H.  Scr Mater, 2011; 64: 85
[21] Choi-Yim H, Johnson W L.  Appl Phys Lett, 1997; 71: 3808
[22] Kato H, Inoue A.  Mater Trans JIM, 1997; 38: 793
[23] Choi-Yim H, Busch R, K\"{oster U, Johnson W L.  Acta Mater, 1999; 47: 2455
[24] Choi-Yim H, Conner R D, Szuecs F, Johnson W L.  Scr Mater, 2001; 45: 1039
[25] Choi-Yim H, Schroers J, Johnson W L.  Appl Phys Lett, 2002; 80: 1906
[26] Li H, Subhash G, Kecskes L J, Dowing R J.  Mater Sci Eng, 2005; A403: 134
[27] Chen G, Bei H, Cao Y, Gali A, Liu C T, George E P.  Appl Phys Lett, 2009; 95: 081908
[28] Cheng J L, Chen G, Xu F, Du Y L, Li Y S, Liu C T.  Intermetallics, 2010; 18: 2425
[29] Hays C C, Kim C P, Johnson W L.  Phys Rev Lett, 2000; 84: 2901
[30] Szuecs F, Kim C P, Johnson W L.  Acta Mater, 2001; 49: 1507
[31] Sun G Y, Chen G, Liu C T, Chen G L.  Scr Mater, 2006; 55: 375
[32] Hofmann D C, Suh J Y, Wiest A, Duan G, Lind M L, Demetriou M D, Johnson W L.  Nature, 2008; 451: 1085
[33] Fan C, Li C F, Inoue A, Haas V.  Phys Rev, 2000; 61B: R3761
[34] Leonhard A, Xing L Q, Heilmaier M, Gebert A, Eckert J, Schultz L.Nanostruct Mater, 1998; 10: 805
[35] Stawovy M T, Aning A O.  Mater Sci Eng, 1998; A256: 138
[36] Lee M H, Kim J--H, Park J S, Kim J C, Kim W T, Kim D H.  Scr Mater, 2004; 50: 1367
[37] Yu P, Kim K B, Das J, Baier F, Xu W, Eckert J.  Scr Mater, 2006; 54: 1445
[38] Zhang Z H, Han B Q, Witkin D, Ajdelsztajn L, Laverna E J.  Scr Mater, 2006; 54: 869
[39] Conner R D, Dandliker R B, Scruggs V, Johnson W L.  Int J Impact Eng, 2000; 24: 435
[40] Zhou X, Kou H C, Wang J, Li J S, Zhou L.  Intermetallics, 2012; 28: 45
[41] Fan C, Liu C T, Chen G, Chen D, Yang X, Liaw P K, Yan H G.  Intermetallics, 2013; 38: 19
[42] Schroers J, Busch R, Masuhr A, Johnson W L.  Appl Phys Lett, 1999; 74: 2806
[43] Dandliker R B.  PhD Dissertation, California Institute of Technology, Pasadena, 1998
[44] Qiu K Q, Wang A M, Zhang H F, Qiao D C, Ding B Z, Hu Z H.  Acta Metall Sin, 2002; 38: 1091
(邱克强, 王爱民, 张海峰, 乔东春, 丁炳哲, 胡壮麒.金属学报, 2002; 38: 1091)
[45] Qiu K Q.  PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2002
(邱克强. 中国科学院金属研究所博士学位论文, 沈阳, 2002)
[46] Zhang H, Zhang Z F, Wang Z G, Qiu K Q, Zhang H F, Zang Q S, Hu Z Q.  Mater Sci Eng, 2006; A418: 146
[47] Wang M L, Chen G L, Hui X, Zhang Y, Bai Z Y.  Intermetallics, 2007; 15: 1309
[48] Wang M L, Hui X D, Kou H C, Chen G L.  Rare Met Mater Eng, 2005; 34: 1102
(王美玲, 惠希东, 寇宏超, 陈国良. 稀有金属材料与工程, 2005; 34: 1102)
Outlines

/

〈 〉