FRICTION AND WEAR PROPERTIES OF SURFACE PLASMA Cr-W ALLOYING LAYER OFγ-TiAl ALLOY

  • WEI Xiangfei ,
  • ZHANG Pingze ,
  • WEI Dongbo ,
  • CHEN Xiaohu ,
  • WANG Qiong ,
  • WANG Ruonan
Expand
  • College of Materials Science and Engineering, Nanjing University of Aeronautics and Astronautics, Nanjing 211106

Received date: 2013-08-07

  Revised date: 2013-08-28

  Online published: 2013-11-11

Abstract

Cr-W alloying layer was prepared on the TiAl alloy by using the double glow plasma surface alloying technology (DGP). The hardness tests show that the surface micro-hardness of Cr-W alloying layer is greatly increased and the micro-hardness of diffusion layer is 648.8 HV0.1, increased two times more than the matrix. The scratch tests show that the bond between TiAl alloy and Cr-W alloying layer is very good and the layer at least can withstand 70 N vertical load. The friction and wear at room temperature tests show that the friction coefficient of Cr-W alloying layer is about 0.43, that of the matrix is 0.70. The wear scar is narrow, and the depth is small. The wear weight loss and wear rate relative to the matrix decrease greatly. The friction and wear at 500℃ tests show that the friction coefficient of Cr-W alloying layer is about 0.50, that of the body is 0.75. The wear weight loss and wear rate of Cr-W alloying layer are all less than the matrix.

Cite this article

WEI Xiangfei , ZHANG Pingze , WEI Dongbo , CHEN Xiaohu , WANG Qiong , WANG Ruonan . FRICTION AND WEAR PROPERTIES OF SURFACE PLASMA Cr-W ALLOYING LAYER OFγ-TiAl ALLOY[J]. Acta Metall Sin, 2013 , 49(11) : 1406 -1410 . DOI: 10.3724/SP.J.1037.2013.00475

References

[1] Duan L H, Liu Y P, Peng J S, Guo C L, Pan J D. Surf Technol, 2007; 36(1): 5

(段良辉, 刘亚萍, 彭建盛, 郭朝丽, 潘俊德. 表面技术, 2007; 36(1): 5)
[2] Hu K J. China Met Bull, 2007; 16: 2
(胡克俊. 中国金属通报, 2007; 16: 2)
[3] Paul J D H, Apple F, Wagner R. Acta Mater, 1988; 46: 1075
[4] Liu Z C, Lin J P, Chen G L. Trans Met Heat Treat, 2001; 22(1): 7
(刘自成, 林均品, 陈国良. 金属热处理学报, 2001; 22(1): 7)
[5] Appel F, Wagner R. Mater Sci Eng, 1998; R22(5): 187
[6] Li X Y, Taniguchi S. Mater Sci Eng, 2005; A398: 268
[7] Mukherjee S, Maitz M F, Pham M T, Richter E, Prokert F, Moeller W.Surf Coat Technol, 2005; 196: 312
[8] Li X Y, Taniguchi S, Zhu Y C, Fujita K, Iwamoto N, Matsunaga Y, Nakagawa K.Intermetallics, 2001; 9: 443
[9] Gray S, Jacobs M H, Ponton C B, Voice W, Evans H E. Mater Sci Eng, 2004; A384: 77
[10] Lee J K, Lee H N, Lee H K, Oh M H, Wee D M. Surf Coat Technol, 2002; 155: 59
[11] Wang D S, Tian Z J, Chen Z Y, Shen L D, Wu H Y, Zhang P Z, Liu Z D, Xu Z,Huang Y H. J Chin Soc Corros Prot, 2009; 29: 1
(王东生, 田宗军, 陈志勇, 沈理达, 吴红艳, 张平则, 刘志东, 徐重, 黄因慧.中国腐蚀与防护学报, 2009; 29: 1)
[12] Wu H Y, Zhang P Z, Ma S J, Xu Z. Lubr Eng, 2007; 32(6): 68
(吴红艳, 张平则, 马士剑, 徐重. 润滑与密封, 2007; 32(6): 68)
[13] Liang W P, Xu Z, Miu Q, Liu X P, He Z Y. Rare Met Mater Eng, 2006; 35: 1827
(梁文萍, 徐重, 缪强, 刘小萍, 贺志勇. 稀有金属材料与工程, 2006; 35: 1827)
[14] Music D, Kreissig U. Phys Let, 2004; 326A: 473
[15] Loria E A.  Intermetallics, 2000; 8: 1339
[16] Tedmon Jr C S. J Less Con Met, 1966; 10(5): 301
[17] Gao Y, Xu J Y, Gao Q, Cheng J, Xu Z. Hot Work Technol, 2006; 35(6): 56
(高原, 徐晋勇, 高清, 成均, 徐重. 热加工工艺, 2006; 35(6): 56)
[18] Ma S J, Zhang P Z, Miu Q, Xu Z. Heat Treat, 2007; 22(5): 26
(马士剑, 张平则, 缪强, 徐重. 热处理, 2007; 22(5): 26)
[19] Liu X B, Yu L G, Wang H M. Chin J Nonferrous Met, 2000; 10: 785
(刘秀波, 于利根, 王华明. 中国有色金属学报 2000; 10: 785)
[20] Zheng C L, Xu Z, Xie X S, He Z Y, Dong J X, Zhang M C. Rare Met Mater Eng, 2003; 32: 32
(郑传林, 徐重, 谢锡善, 贺志勇, 董建新, 张麦仓. 稀有金属材料与工程, 2003; 32: 32)
[21] Zheng C L, Xu Z, He Z Y, Xie X S, Cui F Z. Mater Rev, 2002; 16(11): 14
(郑传林, 徐重, 贺志勇, 谢锡善, 崔福斋. 材料导报, 2002; 16(11): 14)
Outlines

/