Original Articles

USE OF SO2/AIR/N2 COVER GASES FOR THE PROTECTION ON MOLTEN MAGNESIUM AND AZ91D ALLOY

  • Xianfei WANG ,
  • Shoumei XIONG
Expand
  • State Key Laboratory of Automotive Safety and Energy, School of Materials Science and Engineering, Tsinghua University, Beijing 100084

Received date: 2013-07-08

  Revised date: 2013-07-08

  Online published: 2013-09-04

Supported by

Supported by National Natural Science Foundation of China (No.51275269), National Key Technologies R&D Program (No.2011BAE22B02) and International S&T Cooperation Program of China (No.2010DFA72760)

Abstract

Molten magnesium and AZ91D alloy oxidize rapidly during casting process, sulfur dioxide (SO2) mixed with carrier gases can be used to protect the melt by reacting with the melt to form a coherent protective film on the melt surface. In this work, the films formed in SO2/Air/N2 cover gases were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), Auger electron spectroscopy (AES) and X-ray photoelectron spectroscopy (XPS), the formation process and the protective mechanism of the surface film were also discussed. The results show that the protective film is composed of MgO, MgS and MgSO4. MgS increases the pilling and bedworth ratio of the surface film and enhances its protective capability. MgSO4 is the thermodynamically stable phase and its formation is important for the formation of protective film. When SO2/Air/N2 cover gases are used to protect the melt and SO2 content is fixed, air content should be controlled within a certain range.

Cite this article

Xianfei WANG , Shoumei XIONG . USE OF SO2/AIR/N2 COVER GASES FOR THE PROTECTION ON MOLTEN MAGNESIUM AND AZ91D ALLOY[J]. Acta Metall Sin, 2014 , 50(1) : 32 -40 . DOI: 10.3724/SP.J.1037.2013.00386

References

[1] Jafari H, Idris M H, Ourdjini A.Corros Sci, 2011; 53: 655
[2] Bartos S C. In: Hryn J ed., Magnesium Technology 2001, Warrendale, PA: TMS, 2001: 43
[3] Ricketts N J, Cashion S P, Bailey R. In: Dahle A ed., Proc 1st Int Light Metals Technology Conference, Brisbane, Australia: CAST, 2003: 275
[4] Mirak A, Davidson C J, Taylor J A.Corros Sci, 2010; 52: 1992
[5] Fruehling J W. PhD Dissertation, University of Michigan, America, 1970
[6] Pettersen G, ?vrelid E, Tranell G, Fenstad J, Gjestland H.Mater Sci Eng, 2002; A332: 285
[7] Aarstad K. PhD Dissertation, Norwegian Universtity of Science and Technology, Norway, 2004
[8] Ha W, Kim Y J.J Alloys Compd, 2006; 422: 208
[9] Argo D, Lefebvre M. In: Kaplan H I ed., Magnesium Technology 2003, San Diego, USA: TMS, 2003: 15
[10] Schubert W, Gjestland H. In: Kainer K U ed., Magnesium Alloy and Their Applications, Weinheim, Chichester: Wiley, 2000: 761
[11] Cashion S P. PhD Dissertation, University of Queensland, Australia, 1998
[12] Cashion S P, Ricketts N J. In: Kaplan H, Hym J, Clow B eds., Magnesium Technology 2000, Warrendale, PA: TMS, 2000: 77
[13] Moulder J F, Stickle W F, Sobol P E, Bomben K D. Handbook of X-ray Photoelectron Spectroscopy. Eden Prairie, MN: Perkin-Elmer, 1992: 45, 53
[14] Ardizzone S, Bianchi C L, Fadoni, M, Vercelli B.Appl Surf Sci, 1997; 119: 253
[15] Wang X M, Zeng X Q, Zhou Y, Wu G S, Yao S S, Lai Y J.J Alloys Compd, 2008; 460: 368
[16] Barin J, Knacke O. Thermochemical Properties of Inorganic Substances. Berlin: Springer Verlag, 1973(Suppl): 1977
[17] Liu M, Shih D S, Parish C, Atrens A.Corros Sci, 2012; 54: 139
[18] Pilling N B, Bedworth R E.J Inst Met, 1923; 28: 534
Outlines

/