Abstract

The atom probe tomography (APT) is a developing technique to characterize and analyze materials with atomic-scale spatial resolution and high analytical sensitivity. Recently, the substantial progress has been made in technical improvement of APT equipment and data analysis software. In this paper, the new development of APT is introduced, and its unique applications in characterization of traditional structural materials of high-strength low-alloy steel and Al alloy are discussed.

Cite this article

LIU Wenqing , LIU Qingdong , GU Jianfeng . DEVELOPMENT AND APPLICATION OF ATOM PROBE TOMOGRAPHY[J]. Acta Metall Sin, 2013 , 49(9) : 1025 -1031 . DOI: 10.3724/SP.J.1037.2013.00362

References

[1] Blavette D, Deconihout B, Bostel A, Sarrau J M, Bouet M, Menand A.  Rev Sci Instrum,1993; 64: 2911

[2] Deconihout B, Bostel A, Bas P, Chambrel S, Letellier L, Danoix F,Blavette D.  Appl Surf Sci, 1994; 76-77: 145
[3] Blavette D, Deconihout B, Chambrel S, Bostel A.  Ultramicroscopy, 1998; 70: 115
[4] Muller E W, Panitz J A, McLane S B.  Rev Sci Instrum, 1968; 39: 83
[5] Cerezo A, Godfrey T J, Smith G D W.  Rev Sci Instrum, 1988; 59: 862
[6] Cerezo A, Smith G D W.  Microchim Acta, 1991; 104: 401
[7] Cerezo A, Godfrey T J, Sijbrandij S J, Smith G D W, Warren P J.  Rev Sci Instrum, 1998; 69: 49
[8] Vella A, Vurpillot F, Gault B, Menand A, Deconihout B.  Phys Rev, 2006; 73B: 165416
[9] Cerezo A, Clifton P H, Gomberg A, Smith G D W.  Ultramicroscopy, 2007; 107: 720
[10] Blavette D, Al-Kassab T, Cadel E, Mackel A, Vurpillot F, Cojocaru O,Deconihout B, Gilbert M.  Int J Mater Res, 2008; 99: 454
[11] Cerezo A, Clifton P H, Lozano-Perez S, Panayi P, Sha G, Smith G D W.Microsc Microanal, 2007; 13: 408
[12] Kelly T F.  Microsc Microanal, 2011; 17: 1
[13] Kelly T F, Thompson K, Marquis E A, Larson D J.  Microsc Today, 2006; 14: 34
[14] Miller M K.  Atom Probe Tomography: Analysis at the Atomic Level. New York: Kluwer Academic/Plenum Publishers, 2000: 1
[15] Hellman O C, Vandenbroucke J A, Blatzdu Rivage J, Seidman D N.  Mater Sci Eng, 2002; A327: 29
[16] Vaumousse D, Cerezo A, Warren P J.  Ultramicroscopy, 2003; 95: 215
[17] Vurpillot F, DeGeuser F, DaCosta G, Blavette D, Microsc J.  J Microsc, 2004; 216: 234
[18] Stephenson L T, Moody M P, Liddicoat P V, Ringer S P.  Microsc Microanal, 2007; 13: 448
[19] Lefebvre W, Philippe T, Vurpillot F.  Ultramicroscopy, 2011; 111: 200
[20] Hyde J M, Marquis E A, Wilford K B, Williams T J.  Ultramicroscopy, 2011; 111: 440
[21] Thompson K, Flaitz P L, Ronsheim P, Larson D J, Kelly T F.  Science, 2007; 317: 1370
[22] Marquis E A, Miller M K, Blavette D, Ringer S P, Sudbrack C K, Smith G D W.  MRS Bull, 2009; 34: 726
[23] Seidman D N, Stiller K.  MRS Bull, 2009; 34: 717
[24] Miller M K, Forbes R G.  Mater Charact, 2009; 60: 416
[25] Kelly T F, Larson D J, Thompson K, Alvis R L, Bunton J H, Olson J D, Gorman B P.Ann Rev Mater Res, 2007; 37: 681
[26] Kelly T F, Larson D J.  Ann Rev Mater Res, 2012; 42: 1
[27] Kelly T F, Larson D J.  MRS Bull, 2012; 37: 150
[28] Kelly T F, Miller M K, Rajan K, Ringer S P.  Microsc Microanal, 2013; 19: 652
[29] Miller M K, Kelly T F, Rajan K, Ringer S P.  Mater Today, 2012; 15: 158
[30] Gault B, Moody M P, Cairney J M, Ringer S P.  Mater Today, 2012; 15: 378
[31] Zhou B X, Liu W Q.  Mater Sci Technol, 2007; 15: 405
(周邦新,刘文庆. 材料科学与工艺, 2007; 15: 405)
[32] Zhou B X.  Chin J Nat, 2005; 27: 125
(周邦新.自然杂志, 2005; 27: 125)
[33] Liu Q D, Zhao S J.  Metall Mater Trans, 2013; 44A: 163
[34] Liu Q D, Liu W Q, Xiong X Y.  J Mater Res, 2012; 27: 1060
[35] Liu Q D, Zhao S J.  MRS Commun, 2012; 2: 127
[36] Kolli R P, Mao Z, Seidman D N, Keane D T.  Appl Phys Lett, 2007; 91: 241903
[37] Zhang Z W, Liu C T, Miller M K, Wang X, Wen Y R, Fujita T, Hirata A,Chen M W, Chen G, Chin B A.  Sci Rep, 2013; 3: 1327
[38] Clouet E, Lae L, Epicier T, Lefebvre W, Nastar M, Deschamps A.Nat Mater, 2006; 5: 482
[39] Liddicoat P V, Liao X Z, Zhao Y H, Zhu Y T, Murashkin M Y, Lavernia E J, Valiev R Z, Ringer S P.  Nat Commun, 2010; 1: 63
[40] Radmilovic V, Ophus C, Marquis E A, Rossell M D, Tolley A, Gautam A,Asta M, Dahmen U.  Nat Mater, 2011; 10: 710

[41] Zheng Z Q, Liu W Q, Liao Z Q, Ringer S P, Sha G.  Acta Mater, 2013; 61: 3724

Outlines

/