ELECTRODEPOSITION OF PtRu/MWCNTs AND PtRuNi/MWCNTs AND THEIR PERFORMANCE IN DIRECT METHANOL FUEL CELLS

  • ZHAO Yue ,
  • HONG Bo ,
  • FAN Louzhen
Expand
  • 1)College of Environmental Science and Engineering, Ocean University of China, Tsingtao 266100
    2)College of Chemistry, Beijing Normal University, Beijing 100875

Received date: 2012-11-19

  Revised date: 2013-04-12

  Online published: 2013-06-11

Abstract

PtRu catalyst has long application history in electrochemical field due to the wide prospect in direct methanol fuel cells (DMFCs), but its performance remains to be improved further. There are usually two ways to enhance the catalytic activity of PtRu bimetallic catalyst. One is to add the third metal into alloy; the other is to improve the properties of carbon support. In this work, PtRu and PtRuNi nanoparticle clusters were electrochemically deposited on multi-walled carbon nanotubes (MWCNTs) through a three-step process, including an electrochemical treatment of MWCNTs, electro-oxidation of metal chloride to high valence of metal complex and an electro-conversion of PtRu and PtRuNi nanoparticle clusters on MWCNTs. The structure and elemental composition of the PtRu/MWCNTs and PtRuNi/MWCNTs electrodes were characterized by transmission electron microscopy (TEM), energy dispersive X-ray spectroscopy (EDX), X-ray polycrystalline diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). The electrocatalytic properties of the PtRu/MWCNTs and PtRuNi/MWCNTs electrodes for oxygen reduction reaction (ORR) and methanol oxidation were investigated by cycle voltammetry (CV) method and current-time (CT) method. The results showed that PtRuNi/MWCNTs electrode exhibited a high I_f/Ib (the forward anodic peak/the reverse anodic peak current) value and an appreciably improved resistance to carbon  monoxide (CO) poisoning in methanol solution, so a beneficial effect on the oxygen adsorption in dilute sulphuric acid solution was observed. The high electrocatalytic activity and good stability of PtRuNi/MWCNTs was attributed to the synergetic effect of bifunctional catalysis, three dimension structure and oxygen functional groups which generated after electrochemical activation treatment on MWCNTs surface. The successful preparation of PtRu/MWCNTs and PtRuNi/MWCNTs nanocomposites opens a new path for efficient dispersion of promising electrocatalysts in DMFCs.

Cite this article

ZHAO Yue , HONG Bo , FAN Louzhen . ELECTRODEPOSITION OF PtRu/MWCNTs AND PtRuNi/MWCNTs AND THEIR PERFORMANCE IN DIRECT METHANOL FUEL CELLS[J]. Acta Metall Sin, 2013 , 49(6) : 699 -706 . DOI: 10.3724/SP.J.1037.2012.00692

References

[1] Zhao X, Li W, Fu Y, Manthiram A. Int J Hydrogen Energy, 2012; 37: 9845

[2] Bennett B, Koraishy M B, Meyers P J.J Power Sources,2012; 218: 268
[3] Zheng W, Suominen A, Tuominen A.Energy Procedia, 2012; 28: 78
[4] Umeda M, Ueda M, Shironita S.Energy Procedia, 2012; 28: 102
[5] Wang X D, Xie X F, Wang M, Liu G C, Miao R Y, Wang Y T, Yan Q. Prog Chem, 2011; 23: 509
 (王新东, 谢晓峰, 王萌, 刘桂成, 苗睿瑛, 王一拓, 阎群. 化学进展, 2011; 23: 509)
[6] Kakati N, Lee S H, Maiti J, Yoon Y S.  Surf Sci, 2012; 606: 1633
[7] Escudero-Cid R, Hernandez-Fernandez P, Perez-Flores J C, Rojas
S, Garcia-Rodriguez S, Fatas E, Ocon P.  Int J Hydrogen Energy, 2012; 37: 7119
[8] Kang S, Lim S, Peck D H, Kim S K, Jung D H, Hong S H, Jung H G, Shul Y.
 Int J Hydrogen Energy, 2012; 37: 4685
[9] Murthi V S, Urian R C, Mukerjee S.  J Phys Chem, 2004; 108 B: 11011
[10] Wei Z D, Li L L, Luo Y H, Yan C, Sun C X, Yin G Z, Shen P K.  J Phys Chem, 2006; 110B:26055
[11] Basnayake R, Li Z, Katar S, Zhou W, Rivera H, Smotkin E S, Casadonte D J,
Korzeniewski C.  Langmuir, 2006; 22: 10446
[12] Ahn S H, Choi I, Kwon O J, Kim J J. Chem Eng J, 2012; 181-182: 276
[13] Li B, Higgins D C, Zhu S, Li H, Wang H, Ma J, Chen Z.  Catal Commun, 2012; 18: 51
[14] Yang D S, Sim K S, Kwen H D, Choi S H.  J Ind Eng Chem, 2012; 18: 538
[15] Li Q W, Wei Z D, Chen S G, Qi X Q, Liu X, Ding W, Ma Y. Acta Phys Chim Sin, 2011; 27: 2857
 (李庆武, 魏子栋, 陈四国, 齐学强, 柳晓, 丁炜, 马宇. 物理化学学报, 2011; 27: 2857)
[16] Xiong L, Manthiram A.  J Electrochem Soc, 2005; 152: 697
[17] Guillen-Villafuerte O, Guil-Lopez R, Nieto E, Garcia G,Rodriguez J L, Pastor E, Fierro J L G.  Int J Hydrogen Energy,2012; 37: 7171
[18] Dong S A, Liu F, Hou S Q, Pan Z F.  Acta Chim Sin, 2010; 68: 1519
 (董守安, 刘锋, 侯树谦, 潘再富. 化学学报, 2010; 68: 1519)
[19] Dillon A C, Jones K M, Bekkedahl T A, Kiang C H, Bethune D S, Heben M J.
 Nature, 1997; 386: 377
[20] Collins P G, Zettl A, Bando H, Thess A, Smalley R E.  Science, 1997; 278: 100
[21] Zhao Y, Fan L Z, Zhong H Z, Li Y F, Yang S H.  Adv Funct Mater, 2007; 17: 1537
[22] Zhang Y Y, Liu M L, Wang M L, Xie Q J, Yao S Z.  Sensor Actuat, 2007; 123B: 444
[23] Fachinotti E, Guerrini E, Tavares A C, Trasatti S.  J Electroanal Chem, 2007; 600: 103
[24] Hu C C, Cheng C Y.  J Power Sources, 2002; 111: 137
[25] Vukovic M, Cukman D. J  Electroanal Chem, 1999; 474: 167
[26] Park K W, Choi J H, Kwon B K, Lee S A, Sung Y E.  J Phys Chem, 2002; 106B: 1869
[27] Demirci U B.  J Power Sources, 2007; 173: 11
[28] Wang W, Wang R, Wang H, Ji S, Key J, Li X.  J Power Sources, 2011; 196: 9346
[29] Liu F, Lee J Y, Zhou W.  J Phys Chem, 2004; 108B: 17959
[30] Zhao Y, E Y F, Fan L Z, Qiu Y F, Yang S H.  Electrochim Acta, 2007; 52: 5873
[31]Kardash D, Korzeniewski C, Markovic N.  J Electroanal Chem, 2001; 500: 518
Outlines

/