EXPERIMENTAL STUDIES AND CONSTITUTIVE MODELING FOR CREEP AGING OF 2124 Al ALLOY

  • ZHANG Jin ,
  • DENG Yunlai ,
  • YANG Jinlong ,
  • ZHANG Xinming
Expand
  • 1) School of Materials Science and Engineering, Central South University, Changsha 410083
    2) The Key Laboratory of Nonferrous Materials Science and Engineering of Ministry of Education, Central South,University, Changsha 410083

Received date: 2012-10-27

  Revised date: 2012-12-07

  Online published: 2013-03-11

Abstract

A series of creep ageing tests under different temperatures and stresses have been designed to characterize the creep aging behavior of 2124 Al alloy, and the microstructure and properties of the samples in the interrupted tests have been observed. On the basis of the experimental results, combining the creep mechanism and age strengthening theory, a unified constitutive model has been developed for creep age forming of 2124 Al alloy. The constitutive relations, aging strengthening effect and the microstructure are closely correlated in the model, which could be suitable for different ageing temperatures and stress levels. Finally, the model hasbeen used to predict the creep strain curves of added creep aging tests with different temperature, the computed results tally well with the experimental data.

Cite this article

ZHANG Jin , DENG Yunlai , YANG Jinlong , ZHANG Xinming . EXPERIMENTAL STUDIES AND CONSTITUTIVE MODELING FOR CREEP AGING OF 2124 Al ALLOY[J]. Acta Metall Sin, 2013 , 49(3) : 379 -384 . DOI: 10.3724/SP.J.1037.2012.00642

References

[1]Williams J C, Starke E A.Acta Mater, 2003; 51: 5775


[2]Zhan L, Lin J, Dean T A.Int J Mach Tool Manu, 2011; 51: 1

[3]Liu X Y, Pan Q L, Lu Z L, Cao S F, He Y B, Li W B.Acta Metall Sin, 2011; 47: 53

(刘晓艳, 潘清林, 陆智伦, 曹素芳, 何运斌, 李文斌. 金属学报, 2011; 47: 53)

[4]Li C, Wan M, Wu X D, Huang L.Mater Sci Eng, 2010; A527: 3623

[5]Zhan L, Lin J, Dean T A, Huang M.Int J Mech Sci, 2011; 53: 595

[6]Spigarelli S.Mater Sci Eng, 2008; A492: 153

[7]Ho K C, Lin J, Dean T A.Int J Plast, 2004; 20: 733

[8]Ho K C, Lin J, Dean T A.J Mater Process Technol, 2004; 153--154: 122

[9]Li B, Lin J, Yao X.Int J Mech Sci, 2002; 44: 987

[10]Lin J, Yang J.Int J Plast, 1999; 15: 1181

[11]Kowalewski Z L.J Strain Anal Eng, 1994; 29: 309

[12]Muthu K S.Mater Sci Eng, 2011; A528: 4152

[13]Badini C, Marino F, Verne E.Mater Sci Eng, 1995; A191: 185

[14]Zhu A W, Starke E A.Acta Mater, 1999; 47: 3263

[15]Barlat F, Glazov M V, Brem J C.Int J Plast, 2002; 18: 919

[16]da Costa T J, Cram D G, Bourgeois L, Bastow T J, Hill A J, Hutchinson C R.Acta Mater, 2008; 56: 6109

[17]Deschamps A, Brechet Y.Acta Mater, 1998; 47: 293

[18]Myhr O R, Grong φ, Fj H G, Marioara C D.Acta Mater, 2004; 52: 4997

[19]Starink M J, Wang P, Sinclair I, Gregson P J.Acta Mater, 1999; 47: 3855

[20]Liu G, Ding X D, Sun J, Chen K H.Trans Nonferrous Met Soc China, 2001; 11: 337

[21]Liu G, Zhang G J, Ding X D, Sun J, Chen K H.Mater Sci Eng, 2003; A344: 113

[22]Nie J F, Muddle B C.Acta Mater, 2008; 56: 3490

[23]Barlat F, Glazov M V, Brem J C, Lege D J.Int J Plast, 2002; 18: 919

[24]Esmaeili S, Lloyd D J, Poole W J.Acta Mater, 2003; 51: 2243

[25]Cao J, Lin J.Int J Mech Sci, 2008; 50: 193
Outlines

/