EFFECT OF ELECTROLESS Ni-P CONSUMPTION ON THE FAILURE MECHANISM OF SOLDER JOINTS DURING ELECTROMIGRATION

  • HUANG Mingliang ,
  • ZHOU Shaoming ,
  • CHEN Leida ,
  • ZHANG Zhijie
Expand
  • School of Materials Science & Engineering, Dalian University of Technology, Dalian 116024

Received date: 2012-07-06

  Revised date: 2012-09-29

  Online published: 2013-01-11

Abstract

The consumption of electroless Ni-P and its effect on the failure mechanism of solder joints duringelectromigration under a current density of 1.0×104 A/cm2 at both 150 and 200℃ wereinvestigated using line-type Cu/Sn/Ni-P solder joints. Before the electroless Ni-P was completely consumed,the microstructural evolution of the Sn/Ni-P interface (cathode) was the formation of Ni2SnP and Ni3P accompanied by the consumption of the electroless Ni-P. Ni atoms diffused from the electroless Ni--P into the Sn solder under electron current stressing. Most Ni atoms precipitated as (Cu, Ni)6Sn5 or (Ni, Cu)3Sn4 in the Sn solder, and few Ni atoms could arrive at the opposite Cu/Sn interface (anode). After the electroless Ni-P was completely consumed, the microstructural evolutions of the Sn/Ni-P interface (cathode) were the formation of voids and the transformation from Ni3P to Ni2SnP. Furthermore, cracks that resulted from the propagation of voids significantly increased the current density through solder joints, and thus greatly enhanced the Joule heating of solder joints, resulting in the failure of solder joints by the fusing of Sn solder.

 

Cite this article

HUANG Mingliang , ZHOU Shaoming , CHEN Leida , ZHANG Zhijie . EFFECT OF ELECTROLESS Ni-P CONSUMPTION ON THE FAILURE MECHANISM OF SOLDER JOINTS DURING ELECTROMIGRATION[J]. Acta Metall Sin, 2013 , 49(1) : 81 -86 . DOI: 10.3724/SP.J.1037.2012.00401

References

[1] Chen C, Tong H M, Tu K N. Annu Rev Mater Res, 2010; 40: 531


[2] Chan Y C, Yang D. Prog Mater Sci, 2010; 55: 428

[3] Zeng G, Xue S B, Zhang L, Gao L L, Dai W, Luo J D. J Mater Sci: Mater Electron, 2010; 21: 421

[4] Kumar A, He M, Chen Z, Teo P S. Thin Solid Films, 2004; 462--463: 4138

[5] Huang M L, Ye S, Zhao N. J Mater Res, 2011; 26: 3009

[6] Huang M L, Zhou S M, Chen L D. J Electron Mater, 2012; 41: 730

[7] Chen L D, Huang M L, Zhou S M. In: Scott N ed.,

 Proceedings IEEE 60th Electronic Components and Technology Conference (ECTC 2010), Las Vegas, 2010: 176

[8] Chang C W, Yang S C, Tu C T, Kao C R. J Electron Mater, 2007; 36: 1455

[9] Saunders N, Miodownik A P. Alloy Phase Diagrams, 1990; 11: 278

[10] Lu C T, Tseng H W, Chang C H, Huang T S, Liu C Y. Appl Phys Lett, 2010; 96: 232103

[11] Yang Q L, Shang P J, Guo J D, Liu Z Q, Shang J K. J Mater Res, 2009; 24: 2767

[12] Dyson B F, Anthony T R, Turnbull D. J Appl Phys, 1967; 38: 3408

[13] Lin Y H, Hu Y C, Tsai C M, Kao C R, Tu K N. Acta Mater, 2005; 53: 2029

[14] Tsai J Y, Hu Y C, Tsai C M, Kao C R. J Electron Mater, 2003; 32: 1203

[15] Huang M L, Kang N, Huang Y Z. J Mater Sci Technol, 2012; 28(in press)
Outlines

/