STUDY OF HUMPING TENDENCY AND AFFECTING FACTORS IN HIGH SPEED LASER WELDING OF STAINLESS STEEL SHEET

  • PEI Yinglei SHAN Jiguo REN Jialie
Expand
  • 1. Department of Mechanical Engineering, Tsinghua University, Beijing 100084
    2. Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Tsinghua University, Beijing 100084

Received date: 2012-07-11

  Revised date: 2012-09-16

  Online published: 2012-12-11

Abstract

The fiber laser was used to weld austenitic stainless steel SUS304 sheet at the speed of 24 m/min. The effects of laser power, welding speed and shielding gas on humping tendency have been investigated. The melt flow in the molten pool under different welding parameters was studied by Ti tracer method and CCD visual detection system. The results show that the humping tendency is not sensitive to the laser power. The humping is formed when welding speed exceeds 18 m/min, and goes up with the increasing of welding speed. The humping tendency is completely different as changing the direction of shielding gas under constant welding speed and laser power, and it is reduced when the shielding gas direction follows the welding direction. It can be explained that, with the increasing of welding speed, the melt flow becomes fierce, and the humping tendency goes up. The weld shape turns to the "columnar weld", when the shielding gas direction against the welding direction; the weld shape turns to the "cup weld" when the shielding gas direction follows the welding direction. The "cup weld" expanded "U area" which gentles the melt flow and reduces humping tendency. Therefore, adjusting the shielding gas direction to expand the "U area" is an effective approach to reduce the humping tendency.

Cite this article

PEI Yinglei SHAN Jiguo REN Jialie . STUDY OF HUMPING TENDENCY AND AFFECTING FACTORS IN HIGH SPEED LASER WELDING OF STAINLESS STEEL SHEET[J]. Acta Metall Sin, 2012 , 48(12) : 1431 -1436 . DOI: 10.3724/SP.J.1037.2012.00416

References

[1] Albright C E, Chiang S. In: Santa C ed., ICALEO’88 proceedings, Berlin/IFS: Springer, 1988: 207

[2] Nguyen T C, Weckman D C, Johnson D A, Kerr H W. Sci Technol Weld Join, 2006; 11: 618

[3] Wei P S. J Heat Transfer, 2011; 133: 031005–1

[4] Nguyen T C, Weckman D C. Sci Technol Weld Join, 2005; 10: 447

[5] Nguyen T C, Weckman D C. Johmson D A. Weld J, 2007; 86: 360

[6] Hu Z K, Wu C S. Acta Metall Sin, 2008; 44: 1445

(胡志坤, 武传松. 金属学报, 2008; 44: 1445)

[7] Chen J, Wu C S. Acta Metall Sin, 2009; 45: 1070

(陈姬, 武传松. 金属学报, 2009; 45: 1445)

[8] Wu C S, Hu Z K, Zhang Y M. Proc Inst Mech Eng, 2009; 233B: 751

[9] Ueyama T, Ohnawa T, Tanaka M, Nakata K. Sci Technol Weld Join, 2005; 10: 750

[10] Soderstrom E, Mendez P. Sci Technol Weld Join, 2006; 11: 572

[11] Cho M H, Farson D F. Metall Mater Trans, 2007; 38B: 305

[12] Fabbro R. J Phys, 2010; 43D: 445501

[13] Katayama S, Yoheia A, Mizutania M, Kawahitoa Y. In:Elsevier P O ed., Lasers in Manufacturing 2011–Proc 6th Int WLT Conference on Lasers in Manufacturing, Netherlands:

Physics Procedia, 2011: 75

[14] Kawahito Y, Mizutani M, Katayama S. J Phys, 2007; 40D: 5854

[15] Wei P S, Chuang K C, Ku J S, Debory T. IEEE Trans Comp Packag Manufact Technol, 2012; 2: 383

[16] Kawahito Y, Mizutani M, Katayama S. Sci Technol Weld Join, 2009; 14: 588

[17] Zhang L J, Zhang J X, Wang R, Gong S L. Rare Met Mater Eng, 2006; S2: 39

(张林杰, 张建勋, 王蕊, 巩水利. 稀有金属材料与工程, 2006; S2: 39)

[18] Berger P, H¨ugel H, Hess A, Weber R, Graf T. In: Elsevier P O ed., Lasers in Manufacturing 2011 – Proc 6th Int WLT Conferenceon Lasers in Manufacturing, Netherlands: Physics Procedia, 2011: 232

[19] Eriksson I, Powell J, Kaplan A F H. Sci Technol Weld Join, 2011; 16: 636

[20] Chen J. PhD Thesis, Shandong University, Jinan, 2009

(陈姬. 山东大学博士学位论文, 济南, 2009)

[21] Amara E H, Fabbro R. Appl Phys, 2010; 101A: 111

[22] Mendez P F, Eagar T W. Weld J, 2003; 82: 296

[23] Bradstreet B J. Weld J, 1968; 47: 314

[24] Gratzke U, Kapadia P D, Dowden J, Kroos J, Simon G. J Phys, 1992; 25D: 1640

[25] Kumar A, Debroy T. Weld J, 2006; 85: 292

Outlines

/