CORROSION BEHAVIOR OF LONG–TIME IMMERSED RUSTED CARBON STEEL IN FLOWING SEAWATER

  • PENG Xin WANG Jia SHAN Chuan WANG Haijie LIU Zaijian ZOU Yan
Expand
  • 1.The College of Chemistry and Chemical Engineering, Ocean University of China, Qingdao 266100
    2. State Key Laboratory for Corrosion and Protection of Metals, Shenyang 110016
    3. Shandong Provincial Key Laboratory of Ocean Environment Monitoring Technology, Institute of Oceanographic Instrumentation, Shandong Academy of Sciences, Qingdao 266100

Received date: 2012-05-08

  Revised date: 2012-06-04

  Online published: 2012-10-11

Supported by

Supported by National Natural Science Foundation of China (No.50971118)

Abstract

The rust/metal structure is one of the multiphase and multiple interface complex systems. The corrosion under rust is the uppermost and longest form of metallic corrosion evolution process. It is difficult to accurately determine the electrochemical parameters because the existence of rust complicates the electrochemical corrosion process. Based on the result of the previous studies of quiescent seawater, the weight–loss method and different electrochemical tests such as polarization curves (PC), electrochemical impedance spectra (EIS) and linear polarization resistance (LPR) were carried out to study the corrosion behavior of A3 carbon steel immersed in flowing seawater for about 280 d. After very short immersing time, there is a thin yellow rust layer on carbon steel, but as time prolonged, the yellow corrosion products are rushed away quickly, and a tense black rust layer cover about the whole electrode. The corrosion rate obtained by weight–loss method show a steady decline and keep stable after about 84 d, but it is higher than that of the static state system data. The cathodic polarization curves show an obvious reduction current peak at about −950 mV, which makes a remarkable overestimating of the cathodic corrosion current. Polarization resistance (Rp), determined by LPR and EIS, increases during the merely short–initial immersion period, then, it decreases gradually with immersion time. This means that the corrosion rate determined by electrochemical tests shows an another pattern compared with the weight–loss result. After a very short immersion time (about 14 d), there is a remarkable deviation between the weight–loss and electrochemical test results, and the longer immersed the greater of this deviation is. So no matter in static state or flowing seawater, electrochemical methods can not get an accurate corrosion rate of carbon steel. And reliable electrochemical measurement and analysis for rusted steel need much more attention.

Cite this article

PENG Xin WANG Jia SHAN Chuan WANG Haijie LIU Zaijian ZOU Yan . CORROSION BEHAVIOR OF LONG–TIME IMMERSED RUSTED CARBON STEEL IN FLOWING SEAWATER[J]. Acta Metall Sin, 2012 , 48(10) : 1260 -1266 . DOI: 10.3724/SP.J.1037.2012.00258

References

[1] Javaherdashti R. Anti corros Methods Mater, 2000; 47(1): 30

[2] Zheng W L, Yu Q. Environment Sensitive Fraction of Steel. Beijing: Chemical Industry Press, 1988: 12

(郑文龙, 于 青. 钢的环境敏感断裂. 北京: 化学工业出版社, 1988: 12)

[3] Zhu Y L, Zhou J, Xiong C J, Ma Z F, Liu Z S. PetrolChem Equip, 2002; 31(1): 14

(朱岳麟, 周健, 熊常健, 马志锋, 刘中生. 石油化工设备, 2002; 31 (1): 14)

[4] Yan M, Huang G Q. Marine Sci, 2005; 29(7): 73

(颜 民, 黄桂桥. 海洋科学, 2005; 29(7): 73)

[5] Cao C N. Corrosion of Chinese Materials in Nature Environment. Beijing: Chemical Industry Press, 2005: 1

(曹楚南. 中国材料的自然环境腐蚀. 北京: 化学工业出版社, 2005: 1)

[6] Xia L T, Huang G Q, Ding L P. Res Studies Foundry Equip, 2002; 4: 14

(夏兰廷, 黄桂桥, 丁路平. 铸造设备研究, 2002; 4: 14)

[7] Huang G Q. Corros Sci Prot Technol, 2001; 13: 81

(黄桂桥. 腐蚀科学与防护技术, 2001; 13: 81)

[8] Qiu Y B, Qi G T, Guo Z H. China Offshore Oil Gas, 1996;8(5): 18

 (邱于兵, 齐公台, 郭稚弧. 中国海上油气, 1996; 8(5): 18)

[9] Zhang W, Wang J, Li Y N, Wang W. Acta Phys Chim Sin, 2010; 26: 2941

(张 伟, 王佳, 李玉楠, 王伟. 物理化学学报, 2010; 26: 2941)

[10] Bousselmi L, Fiaud C, Tribollet B, Triki E. Electrochim Acta, 1999; 44: 4357

[11] John D G, Searosn P C, Dawson J L. Br Corros J, 1981; 16(2): 102

[12] Liu G Z, Wang J M, Zhang J Q, Cao C N. Acta Metall Sin, 2011; 47: 1600

(刘光洲, 王建明, 张鉴清, 曹楚南. 金属学报, 2011; 47: 1600)

[13] Zhang J B, Wang J, Wang Y H. Acta Phys Chim Sin, 2005; 21: 993

(张际标, 王佳, 王燕华. 物理化学学报, 2005; 21: 993)

[14] Gonz´alez J A, Miranda J M, Otero E, Feliu S. Corros Sci, 2007; 49: 436

[15] Zou Y, Zheng Y Y, Wang Y H, Wang J. Acta Metall Sin, 2010; 46: 123

(邹妍, 郑莹莹, 王燕华, 王佳. 金属学报, 2010; 46: 123)

[16] Zou Y, Wang J, Zheng Y Y. Acta Phys Chim Sin, 2010;26: 2361

 (邹妍, 王佳, 郑莹莹. 物理化学学报, 2010; 26: 2361)

[17] Zou Y, Wang J, Zheng Y Y. Corros Sci, 2011; 53: 208

[18] Antony H, Perrin S, Dillmann P, Legrand L, Chauss´e A. Electrochim Acta, 2007; 52: 7754

[19] Andrade C, Keddam M, N´ovoa X R, P´erez M C, Rangel C M, Takenouti H. Electrochim Acta, 2001; 46: 3905

[20] Nov´ak P, Mal´aR, Joska L. Cement Concrete Res, 2001; 31: 589

[21] Copson H R. Corrosion, 1960; 16: 130

[22] Shalaby H M, Attari S, Riad W T. Corrosion, 1992; 48: 206

[23] Nesic S, Solvi G T, Enerhaug J. Corrosion, 1995; 51: 773

[24] Huang G Q. Corros Sci Prot Technol, 2001; 22: 384

(黄桂桥. 腐蚀科学与防护技术, 2001; 22: 384)

[25] Martinez S. Mater Chem Phys, 2002; 77: 97

[26] Stern M, Geary A L. J Electrochem Soc, 1957; 104: 56

Outlines

/

〈 〉