RESEARCH ON DYNAMIC RECRYSTALLIZATION BEHAVIOR OF INCOLOY 800H

  • CAO Yu DI Hongshuang ZHANG Jiecen ZHANG Jingqi MA Tianjun
Expand
  • 1.State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
    2.Special Steel Business Unit, Baoshan Iron&Steel Co., Ltd., Shanghai 200940

Received date: 2012-04-27

  Revised date: 2012-06-14

  Online published: 2012-10-11

Supported by

Supported by National Basic Research Program of China (No.2011CB606306–2)

Abstract

In order to optimize the hot working technology of Incoloy 800H, the dynamic recrystallization (DRX) behavior of Incoloy 800H at temperatures ranging from 850 ℃ to 1100 ℃ and strain rates from 0.01 s-1 to 10 s-1 was investigated by single–pass compression tests on MMS–300 thermo–mechanical simulator. The evolutions of microstructure and nucleation mechanisms of DRX were analyzed combined with the technique of EBSD and TEM. The results show that when the deformation temperature is below 950 ℃, the behavior of DRX is obviously restrained by precipitation of Cr23C6 and Ti(C,N). Therefore the hot deformation constitutive equations in two temperature intervals (from 850 ℃ to 950 ℃and from 950 ℃ to 1100 ℃) were established by regression analysis with the deformation activation energy of 465.394 kJ/mol and 427.360 kJ/mol respectively. The inflection points were determined by fitting a third order polynomial to the lnθ–ε curves, which makes the prediction for the ratios of critical stress to peak stress and critical strain to peak strain more accurately. Accordingly, the mathematical models of critical stress and critical strain vs Z parameter were deduced. The DRX nucleation mechanisms of Incoloy 800H during hot deformation mainly include strain induced grain boundary migration, grain fragmentation and subgrain coalescence.

Cite this article

CAO Yu DI Hongshuang ZHANG Jiecen ZHANG Jingqi MA Tianjun . RESEARCH ON DYNAMIC RECRYSTALLIZATION BEHAVIOR OF INCOLOY 800H[J]. Acta Metall Sin, 2012 , 48(10) : 1175 -1185 . DOI: 10.3724/SP.J.1037.2012.00236

References

[1] Tan L, Rakotojaona L, Allen T R, Nanstad R K, Busby J T. Mater Sci Eng, 2011; A528: 2755

[2] Br¨unger E, Wang X, Gottstein G. Scr Mater, 1998; 38: 1843

[3] Wang X, Br¨unger E, Gottstein G. Mater Sci Eng, 2000; A290: 180

[4] Wang X, Br¨unger E, Gottstein G. Scr Mater, 2002; 46: 875

[5] Gottstein G, Frommert M, Goerdeler M, Sch¨afer N. Mater Sci Eng, 2004; A387–389: 604

[6] Abd El–Azim M E. J Nucl Mater, 1996; 231: 146

[7] Frommert M, Gottstein G. Mater Sci Eng, 2009; A506: 101

[8] Sun C Y, Liu J R, Li R, Zhang Q D. Acta Metall Sin, 2011; 47: 191

(孙朝阳, 刘金榕, 李瑞, 张清东. 金属学报, 2011; 47: 191)

[9] McQueen H J, Ryan N D. Mater Sci Eng, 2002; A322: 43

[10] Venugopal S, Mannan S L, Rodriguez P. J Mater Sci, 2004; 39: 5557

[11] Naderi M, Durrenberger L, Bleck W. Mater Sci Eng, 2008; A478: 130

[12] McQueen H J. Mater Sci Eng, 2004; A387: 203

[13] Spigarelli S, Evangelista E, McQueen H J. Scr Mater, 2003; 49: 179

[14] Chen L Q, Zhao Y, Xu X Q, Liu X H. Acta Metall Sin, 2010; 46: 1219

(陈礼清, 赵阳, 徐香秋, 刘相华. 金属学报, 2010; 46: 1219)

[15] Momeni A, Dehghani K, Keshmiri H, Ebrahimi G R. Mater Sci Eng, 2010; A527: 1607

[16] Zhang M J, Li F G, Wang S Y, Liu C Y. Mater Sci Eng, 2010; A527: 6778

[17] Cao Y, Di H S, Ma T J, Zhang J Q. J Northeastern Univ (Nat Sci Ed), 2012; 33: 215

(曹宇, 邸洪双, 马天军, 张敬奇. 东北大学学报(自然科学版), 2012; 33: 215)

[18] Poliak E I, Jonas J J. Acta Mater, 1996; 44: 127

[19] Ryan N D, McQueen H J. Can Metall Q, 1990; 29: 150

[20] Barnett M R, Kelly G L, Hodgson P D. Scr Mater, 2000; 43: 366

[21] Gottstein G, Frommert M, Goerdeler M. Mater Sci Eng, 2004; A387–389: 604

[22] Poliak E I, Jonas J J. ISIJ Int, 2003; 43: 684

[23] Najafizadeh A, Jonas J J. ISIJ Int, 2006; 46: 1679

[24] Mirzadeh H, Najafizadeh A. Mater Des, 2010; 31: 1174

[25] McQueen H J, Yue S, Ryan N D, Fry E. J Mater Process Technol, 1995; 53: 295

[26] Hansen N, Huang X. Acta Metall, 1998; 46: 1827

[27] Yu J W, Liu X F, Xie J X. Acta Metall Sin, 2011; 47: 486

(余均武, 刘雪峰, 谢建新. 金属学报, 2011; 47: 486)

[28] Winning M. Scr Mater, 2008; 58: 86

Outlines

/

〈 〉