EFFECTS OF ANTIBACTERIAL AGING TREATMENT ON MICROSTRUCTURE AND PROPERTIES OF COPPER-CONTAINING DUPLEX STAINLESS STEEL
II. Corrosion Resistance and Antibacterial Properties

  • XIANG Hong-Liang ,
  • FAN Jin-Chun ,
  • LIU Dong ,
  • GU Xin
Expand
  • School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350108

Received date: 2012-04-06

  Revised date: 2012-07-10

  Online published: 2012-09-11

Supported by

Supported by Program for New Century Excellent Talents in University of Fujian Province (No.JA10014)

Abstract

Effects of antibacterial aging treatment on the corrosion resistance of copper-bearing duplex stainless steels were investigated by electrochemical methods. The film-cover method was used to test the antibacterial effect of the materials. The polarization curve test results show ε-Cu and other copper-rich phases become the weak point of the passive film on the surface of the duplex stainless steel, and the sites where the coarse copper-rich phases are precipitated from the matrix are apt to become pitting nucleation source. The proportion of coarse copper-rich phase increases, which makes pitting resistance of the materials worse. EIS test reveals that the presence of ε-Cu and other copper-rich phases in passive film reduces the overall potential and passive film resistance, decreasing the stability of passive film. D-EPR tests show that ε-Cu and other copper-rich phases in grain boundary makes it take on anode characteristic in corrosion process, leading to selectively intergranular corrosion. Compared with austenite, the intergranular corrosion resistance of ferrite decreases seriously because the copper-rich phases are mainly precipitated from ferrite matrix. Antibacterial tests show that the microstructure and volume fraction of copper-rich phases are the key factors affecting the antibacterial properties of the materials. ε-Cu displays the best antibacterial effect, followed by metastable copper-rich phase, solid solution copper is the worst. The more ε-Cu phases are, the more antibacterial effect is.

Cite this article

XIANG Hong-Liang , FAN Jin-Chun , LIU Dong , GU Xin . EFFECTS OF ANTIBACTERIAL AGING TREATMENT ON MICROSTRUCTURE AND PROPERTIES OF COPPER-CONTAINING DUPLEX STAINLESS STEEL
II. Corrosion Resistance and Antibacterial Properties[J]. Acta Metall Sin, 2012
, 48(9) : 1089 -1096 . DOI: 10.3724/SP.J.1037.2012.00178

References

[1] Suzuki S, Nakamura S, Ookubo N, Hasegawa M, Miyakuso K. CAMP–ISIJ, 1999; 12: 518

[2] Chen S H, L¨u M Q, Zhang J D, Dong J S, Yang K. Acta Metall Sin, 2004; 40: 314

(陈四红, 吕曼祺, 张敬党, 董加胜, 杨 柯. 金属学报, 2004; 40: 314)

[3] Nan L, Liu Y Q, Yang W C, Xu H, Li Y, Lu M Q, Yang K. Acta Metall Sin, 2007; 43: 1065

(南黎, 刘永前, 杨伟超, 徐慧, 李瑛, 吕曼祺, 杨 柯. 金属学报, 2007; 43: 1065)

[4] Zhang Z X, Lin G, Xu Z. J Mater Process Technol, 2008; 205: 419

[5] Nan L, Yang K. J Mater Sci Technol, 2010; 26: 941

[6] Yang K, Dong J S, Chen S H, L¨u M Q. Chin J Mater Res, 2006; 20: 523

(杨 柯, 董加胜, 陈四红, 吕曼棋. 材料研究学报, 2006; 20: 523)

[7] Nan L, Yang W C, Liu Y Q, Xu H, Li Y, L¨u M Q, Yang K. J Mater Sci Technol, 2008; 24: 197

[8] Hong I T, Koo C H. Mater Sci Eng, 2005; A393: 213

[9] Wang X L, Zhao R D, Zhang W Q, Zhu H F. Spec Steel, 2006; 27(5): 35

(王小丽, 赵荣达, 张伟强, 朱宏飞. 特殊钢, 2006; 27(5): 35)

[10] Xiang H L, Fan J C, Liu D, Guo P P. Acta Metall Sin, 2012; 48: 1081

(向红亮, 范金春, 刘东, 郭培培. 金属学报, 2012; 48: 1081)

[11] Gong J, Jiang Y M, Deng B, Xu J L, Hu J P, Li J. Electroc Acta, 2010; 55: 5077

[12] Yang K, Lu M Q. J Mater Sci Technol, 2007; 23: 333

[13] Fu Y, Lin C J, Cai W D. Acta Metall Sin, 2005; 41: 302

(付 燕, 林昌健, 蔡文达. 金属学报, 2005; 41: 302)

[14] Jinil S, Sangshik K, Jehyun L, Byunghak C. Metall Mater Trans, 2003; 34A: 1617

[15] Sourisseau T, Chauveau E, Baroux B. Corros Sci, 2005; 47: 1097

[16] Banas J, Mazurkiewicz A. Mater Sci Eng, 2000; A277: 183

[17] Wei B M. The Theory of Metal Corrosion and Application. Beijing: Chemical Industry Press, 1984: 37

(魏宝明. 金属腐蚀理论及应用. 北京: 化学工业出版, 1984: 37)

[18] Trethewey K R, Paton M. Mater Lett, 2004; 58: 3381

[19] Lo I H, Fu Y, Lin C J, Tsai W T. Corros Sci, 2006; 48: 696

[20] Xiao J M. The Metallurgical Problems of Stainless Steels. Beijing: Metallurgy Industry Press, 2006: 164

(肖纪美. 不锈钢的金属学问题. 北京: 冶金工业出版社, 2006: 164)

[21] Zhang Z X, Lin G, Jiang L Z, Xu Z. Mater Chem Phys, 2008; 111: 238

[22] Ren H P, Liu Z C, An Z G, Wang H Y. Trans Mater Heat Treat, 2006; 27(4): 49

(任慧平, 刘宗昌, 安治国, 王海燕. 材料热处理学报, 2006; 27(4): 49)

[23] Ren H, Mao W. J Univ Sci Technol Beijing, 2002; 9(3): 185
Outlines

/

〈 〉