论文

EFFECTS OF ANTIBACTERIAL AGING TREATMENT ON MICROSTRUCTURE AND PROPERTIES OF COPPER-CONTAINING DUPLEX STAINLESS STEEL
I. Microstructure and Evolution of Copper-Rich Phase

  • XIANG Hong-Liang ,
  • FAN Jin-Chun ,
  • LIU Dong ,
  • GUO Pei-Pei
Expand
  • School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350108

Received date: 2012-04-06

  Revised date: 2012-07-10

  Online published: 2012-09-11

Supported by

Supported by Program for New Century Excellent Talents in University of Fujian Province (No.JA10014)

Abstract

Nowadays, the events of bacterial infection are increasingly arising. It is urgent to develop new antibacterial material to fight against the bacteria having resistance to drug. Because the antibacterial stainless steels have both antibacterial property and other excellent combination ones, their development has been obtained rapidly. At present, the copper-containing antibacterial stainless steels are the research focus. It has been reached that the antibacterial effect of those materials is due to the copper-rich phases precipitated from the matrix by aging treatment. Most of studies were performed at single-phase stainless steels, but rarely at duplex stainless steels. It is necessary to study the precipitation process of copper-rich phases in duplex stainless steels for the development of antibacterial duplex stainless steels. In this work, the microstructure and precipitating evolution law of copper-rich phases in the copper-containing duplex stainless steels during antibacterial aging treatment has been analyzed in detail by SEM, XRD and TEM. The results indicate that antibacterial copper-rich phases are precipitated from ferrite and α/γ interfaces, no precipitation in austenite when the duplex stainless steels are aged at temperature ranging from 540 to 580 ℃. The technique parameters of the aging treatment have important effect on the volume fraction and morphologies of precipitated phase. With aging time increasing, the precipitates coarsen, and their morphologies gradually change from spherical particle to rod-like or long-stripe-like grain. When the aging temperature is raised, precipitation speed of copper-rich phases accelerates and they make the change like before. At the same time,  the copper-rich phases gradually turn from metastable state to steady ε-Cu phase with the composition close to pure copper, which has complicated multilayer structure with twisting layers. The Kurdjumov--Sachs orientation relationships between ε-Cu phases and the ferrite matrix followed: (111)ε-Cu//(110)α-Fe, [011]ε-Cu//[001]α-Fe, (111)ε-Cu//(121)α-Fe, [011]ε-Cu//[012]α-Fe.

Cite this article

XIANG Hong-Liang , FAN Jin-Chun , LIU Dong , GUO Pei-Pei . EFFECTS OF ANTIBACTERIAL AGING TREATMENT ON MICROSTRUCTURE AND PROPERTIES OF COPPER-CONTAINING DUPLEX STAINLESS STEEL
I. Microstructure and Evolution of Copper-Rich Phase[J]. Acta Metall Sin, 2012
, 48(9) : 1081 -1088 . DOI: 10.3724/SP.J.1037.2012.00177

References

[1] Nakamura S, Suzuki S, Ookubo N, Hasegawa M, Miyakusu K. CAMP–ISIJ, 1998; 11: 1147

[2] Ookubo N, Nakamura S, Yamamoto M, Miyakusu K, Hasegawa M. Nisshin Steel Rep Jpn, 1998; 77: 69

[3] Toyokihara C, Nakamura S, Suzuki S, Miyakusu K, Ookubo S, Hasegawa M. CAMP–ISIJ, 1999; 12: 1179

[4] Chen S H, L¨u M Q, Zhang J D, Dong J S, Yang K. Acta Metall Sin, 2004; 40: 314

(陈四红, 吕曼祺, 张敬党, 董加胜, 杨 柯. 金属学报, 2004; 40: 314)

[5] Hong I T, Koo C H. Mater Sci Eng, 2005; A393: 213

[6] Lu M Q, Chen S H, Dong J S, Yang K. Chin J Mater Res, 2005; 19: 581

(吕曼祺, 陈四红, 董加胜, 杨柯. 材料研究学报, 2005; 19: 581)

[7] Li H W, Zhang T B, Zhang T Y. Acta Metall Sin, 2008; 44: 39

(李恒武, 张体宝, 张体勇. 金属学报, 2008; 44: 39)

[8] Li N, Yang K. J Mater Sci Technol, 2010; 26: 941

[9] Robert N G. Duplex Stainless Steels: Microstructure, Properties and Applications. Cambridge: Woodhead Publish Ltd, 1997: 3

[10] Sun W S, Ding G R, Luo M W, Wang Z H, Song A Y. Acta Metall Sin, 1996; 32: 245

(孙文山, 丁桂荣, 罗铭蔚, 王智慧, 宋爱英. 金属学报, 1996; 32: 245)

[11] Xiang H L, Huang W L, Liu D, He F S. Acta Metall Sin, 2010; 46: 304

(向红亮, 黄伟林, 刘东, 何福善. 金属学报, 2010; 46: 304)

[12] Xiang H L, He F S, Liu D. Acta Metall Sin, 2009; 45: 1456

(向红亮, 何福善, 刘 东. 金属学报, 2009; 45: 1456)

[13] Xiang H L, Huang W L, Liu D, He F S, Ruan F R. Trans Mater Heat Treat, 2010; 31(12): 85

(向红亮, 黄伟林, 刘东, 何福善, 阮方如.材料热处理学报, 2010; 31(12): 85)

[14] Martins M, Roossitti S M, Ritoni M. Mater Charact, 2007; 58: 909

[15] Russell S W, Lundin C D. Final Report for the Development of Qualification Standards for Cast Duplex Stainless Steel. Vol.2, Knoxville: University of Tennessee, 2005: 14

[16] Jacek B, Andrzej M. Mater Sci Eng, 2000; A277: 183

[17] Hughes D D. Mater Sci Eng, 1993; A168: 35

[18] Dhua S K, Mukerjee D, Sarma D S. Metall Mater Trans, 2001; 32A: 2259

[19] Murayama M, Hono K, Katayama Y. Metall Mater Trans, 1999; 30A: 345

[20] Zhang Z X, Lin G, Xu Z. Chin J Mater Res, 2008; 29: 93

(张志霞, 林 刚, 徐 洲. 材料研究学报, 2008; 29: 93)

[21] Aaronson H I, Lee J K. In: Aaronson H I ed., Lectures on the Theory of Phase Transformations. Warrendale: TMS–AIME, 1975: 83

[22] Zhang Z X, Lin G, Xu Z. J Mater Sci Technol, 2008; 24: 775

[23] Kolli R P, Seidman D N. Acta Mater, 2008; 56: 2073
Outlines

/

〈 〉