EFFECT OF Bi ADDITION ON THE CORROSION RESISTANCE OF Zr-4 IN SUPERHEATED STEAM AT 400 ℃/10.3 MPa

  • YAO Mei-Yi ,
  • ZOU Ling-Hong ,
  • XIE Xin-Fei ,
  • ZHANG Jin-Long ,
  • PENG Jian-Tiao ,
  • ZHOU Bang-Xin
Expand
  • 1) Laboratory for Microstructures, Shanghai University, Shanghai 200444
    2) Institute of Materials, Shanghai University, Shanghai 200072

Received date: 2012-04-06

  Revised date: 2012-06-14

  Online published: 2012-09-11

Supported by

Supported by National Natural Science Foundation of China (No.50971084), National Advanced Pressurized Water Reactor Project of China (No.2011ZX06004-023) and Shanghai Leading Academic Discipline Project (No.S30107)

Abstract

The effect of Bi contents on the corrosion resistance of Zr-4+xBi (x=0.1%-0.5%, mass fraction)
alloys, which were prepared by adding Bi to Zr-4, was investigated in superheated steam at 400 ℃ and
10.3 MPa by autoclave tests. The microstructures of the alloys and fracture surface morphology of the oxide film
formed on the alloys were observed by TEM, EDS and SEM. The results show that with the increase of Bi content,
the second phase particles (SPPs) are almost the same in size and shape, but increase in amount and vary in
composition, including Zr(Fe, Cr)2, Zr-Fe-Cr-Bi, Zr-Fe-Sn-Bi and Zr-Fe-Cr-Sn-Bi. Even in the
Zr-4+0.1Bi alloy, Bi--containing SPPs were detected. This indicates that the solid solubility of Bi in α-Zr
matrix of Zr-4+xBi alloys is less than 0.1% at 580 ℃. Moreover, the addition of Bi promotes the precipitation
of Sn which originally dissolved in the α-Zr matrix of Zr-4. Compared with Zr-4, the addition
of Bi makes the corrosion resistance worse, and it becomes more obvious with the increase of Bi content. This
illustrates that the addition of Bi can not improve the corrosion resistance, on the contrary, it brings a harmful
influence. This may be related to the precipitation of the Bi-containing and Bi-Sn-containing SPPs.

Cite this article

YAO Mei-Yi , ZOU Ling-Hong , XIE Xin-Fei , ZHANG Jin-Long , PENG Jian-Tiao , ZHOU Bang-Xin . EFFECT OF Bi ADDITION ON THE CORROSION RESISTANCE OF Zr-4 IN SUPERHEATED STEAM AT 400 ℃/10.3 MPa[J]. Acta Metall Sin, 2012 , 48(9) : 1097 -1102 . DOI: 10.3724/SP.J.1037.2012.00176

References

[1] Sabol G P. In: Rudling P, Kammenzind B eds., Zirconium in the Nuclear Industry: Fourteenth International Symposium, ASTM STP 1467, Stockholm: ASTM International, 2004: 3

[2] Sabol G P, Comstock R J, Weiner R A. In: Garde A M, Bradley E R eds., Zirconium in the Nuclear Industry: Tenth International Symposium, ASTM STP 1245, Baltimore, MD: ASTM International, 1994: 724

[3] Nikulina A V, Markelov V A, Peregud M M. In: Bradley E R, Sabol G P eds., Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295, Garmisch–Partenkirchen, Germany: ASTM International, 1996: 785

[4] Zhao W J, Miao Z, Jiang H M, Yu X W, Li W J, Li C, Zhou B X. J Chin Soc Corros Prot, 2002; 22: 124

(赵文金, 苗志, 蒋宏曼, 于晓卫, 李卫军, 李聪, 周邦新. 中国腐蚀与防护学报, 2002; 22: 124)

[5] Park J–Y, Yoo S J, Choi B–K, Jeong Y H. J Nucl Mater, 2008; 373: 343

[6] Hong H S, Moon J S, Kim S J, Lee K S. J Nucl Mater, 2001; 297: 113

[7] Yao M Y, Li S L, Zhang X, Peng J C, Zhou B X, Zhao X S, Shen J Y. Acta Metall Sin, 2011; 47: 865

(姚美意, 李士炉, 张欣, 彭剑超, 周邦新, 赵旭山, 沈剑韵. 金属学报, 2011; 47: 865)

[8] Li S L, Yao M Y, Zhang X, Geng J Q, Peng J C, Zhou B X. Acta Metall Sin, 2011; 47: 163

(李士炉, 姚美意, 张欣, 耿建桥, 彭剑超, 周邦新. 金属学报, 2011; 47: 163)

[9] Li P Z, Li Z K. Rare Met Mater Eng, 1998; 27: 356

(李佩志, 李中奎. 稀有金属材料与工程, 1998; 27: 356)

[10] Zhou B X, Li Q, Yao M Y, Liu W Q. Nucl Power Eng, 2005; 26(4): 364

(周邦新, 李 强, 姚美意, 刘文庆. 核动力工程, 2005; 26(4): 364)

[11] Li C, Li P, Zhou B X, Zhao W J, Peng Q, Ying S H, Shen B L. Nucl Power Eng, 2002; 23(4): 20

(李聪, 李蓓, 周邦新, 赵文金, 彭 倩, 应诗浩, 沈保罗. 核动力工程, 2002; 23(4): 20)

[12] Foster J P, Dougherty J, Burke M G. J Nucl Mater, 1990; 173: 164

[13] Charquet D. In: Sabol G P, Moan G D eds., Zirconium in the Nuclear Industry: Twelfth International Symposium, ASTM STP 1354, West Conshohocken: ASTM International, 2000: 3

[14] Eucken C M, Finden P T. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry: Eighth International Symposium, ASTM STP 1023, Philadelphia: ASTM International, 1989: 113

[15] Takeda K, Anada H. In: Sabol G P, Moan G D eds., Zirconium in the Nuclear Industry: Twelfth International Symposium, ASTM STP 1354, West Conshohocken: ASTM International, 2000: 592

[16] Garzarolli F, Broy Y, Busch R A. In: Bradley E R, Sabol G P Eds., Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295, Garmisch– Partenkirchen, Germany: ASTM International, 1996: 850

[17] Graham R A, Tosdale J P, Finden P T L F P. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry: Eighth International Symposium, ASTM STP 1023, Philadelphia: ASTM International, 1989: 334

[18] Yang W D. Reactor Materials Science. 2nd Ed., Beijing: Atomic Energy Press, 2006: 260

(杨文斗. 反应堆材料学. 第二版, 北京: 原子能出版社, 2006: 260)

[19] Zhou B X, Li Q, Liu W Q, Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 35: 1009

(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009)

[20] Cox B. J Nucl Mater, 1969; 29: 50

[21] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. J ASTM Int, 2008; 5: 360

[22] Charquet D, Hanh R, Ortlib E. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry, Eighth International Symposium, ASTM STP 1023, Philadelphia: ASTM International, 1989: 405

[23] Yao M Y, Zhou B X, Li Q, Liu W Q, Yu W J, Chu Y L. J Nucl Mater, 2008; 374: 197

[24] Shen Y F, Yao M Y, Zhang X, Li Q, Zhou B X, Zhao W J. Acta Metall Sin, 2011; 47: 899

(沈月锋, 姚美意, 张 欣, 李强, 周邦新, 赵文金. 金属学报, 2011; 47: 899)
Outlines

/