EFFECT OF WELDING PARAMETERS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED AlCuLi ALLOY JOINTS

  • YU Dong ,
  • DONG Chun-Lin ,
  • XIAO Ba-Lv ,
  • HE Miao ,
  • LUAN Guo-Hong ,
  • MA Zong-Xi
Expand
  • 1) Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2) AVIC Beijing Aeronautical Manufacturing Technology Research Institute, Beijing 100024

Received date: 2012-03-31

  Revised date: 2012-05-23

  Online published: 2012-09-11

Supported by

Supported by GAD Pre-research Foundation of China (No.9140A18050109HK55)

Abstract

Friction stir welding (FSW) of a novel AlCuLi alloy was conducted to investigate the effect of welding parameters on the microstructure and mechanical properties of the joints. The fine and equiaxed dynamically rotation rate increased, the size of the grains in the NZ increased. However, with increasing the welding speed, the size of the grains in the NZ decreased slightly. TEM analyses indicated that most of the precipitates in the NZ dissolved into the matrix during FSW and some coarse precipitates formed during subsequent cooling process. Moreover, many coarse precipitates were observed in the heat affected zone (HAZ) due to the FSW thermal cycle. At a low welding speed of 80 mm/min, the ultimate tensile strength of the joints increased as the rotation rate increased, and could reach up to 442 MPa which was 87% of that of the base metal. All of the joints failed in the lowest hardness zone of the HAZ. At a high welding speed of 200 mm/min, some defects resulting from insufficient material flow were observed on the fracture surfaces. At a low rotation rate, the joints failed along the defects in the NZ and exhibited a low strength. As the rotation rate increased, the size and number of the defects decreased. Therefore, the effect of the defects on the strength of the joints was significantly reduced, and a joint efficiency of 84% was obtained.

Cite this article

YU Dong , DONG Chun-Lin , XIAO Ba-Lv , HE Miao , LUAN Guo-Hong , MA Zong-Xi . EFFECT OF WELDING PARAMETERS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED AlCuLi ALLOY JOINTS[J]. Acta Metall Sin, 2012 , 48(9) : 1109 -1115 . DOI: 10.3724/SP.J.1037.2012.00163

References

[1] Wang Z T, Tian R Z. Handbook of Aluminum Alloy and Processing. 3rd Ed., Changsha: Central South University Press, 2005: 317

(王祝堂, 田荣璋, 铝合金及其加工手册. 第3版, 长沙: 中南大学出版社, 2005: 317)

[2] Wang S C, Starink M J. Int Mater Rev, 2005; 50: 193

[3] Kostrivas A, Lippold J C. Int Mater Rev, 1999; 44: 217

[4] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1

[5] Wang D, Liu J, Xiao B L, Ma Z Y. Acta Metall Sin, 2010; 46: 589

(王东, 刘杰, 肖伯律, 马宗义. 金属学报, 2010; 46: 589)

[6] Xie G M, Ma Z Y, Geng L. Acta Metall Sin, 2008; 44: 665

(谢广明, 马宗义, 耿 林. 金属学报, 2008; 44: 665)

[7] Steuwer A, Dumont M, Altenkirch J, Birosca S, Deschamps A, Prangnell P B,Withers P J. Acta Mater, 2011; 59: 3002

[8] Wei S T, Hao C Y, Chen J C. Mater Sci Eng, 2007; A452– 453: 170

[9] Hatamleh O. Mater Sci Eng, 2008; A492: 168

[10] Shukla A K, Baeslack W A. Sci Technol Weld Joining, 2009; 14: 376

[11] Jolu T L, Morgeneyer T F, Lorenzon A F G. Sci Technol Weld Joining, 2010; 15: 694

[12] Salem H G, Reynolds A P, Lyons J S. Scr Mater, 2002; 46: 337

[13] Fonda R W, Bingert J F. Metall Mater Trans, 2006; 37A: 3593

[14] Zhang Z, Xiao B L,Wang D, Ma Z Y. Metall Mater Trans, 2011; 42A: 1717

[15] Liu F C, Ma Z Y. Acta Metall Sin, 2008; 44: 319

(刘峰超, 马宗义. 金属学报, 2008; 44: 319)

[16] Lynch S P, Muddle B C, Pasang T. Acta Mater, 2001; 49: 2863

[17] Liu F C, Ma Z Y. Metall Mater Trans, 2008; 39A: 2378

[18] Ren S R, Ma Z Y, Chen L Q, Zhang Y Z. Acta Metall Sin, 2007; 43: 225

(任淑荣, 马宗义, 陈礼清, 张玉政. 金属学报, 2007; 43: 225)

[19] Yoshimura R, Konno T J, Abe E, Hiraga K. Acta Mater, 2003; 51: 4251

[20] Mahoney M W, Rhodes C G, Flintoff J G, Spurling R A, Bingel W H. Metall Mater Trans, 1998; 29A: 1955

[21] Zhang Q, Xiao B L, Wang Q Z, Ma Z Y. Mater Lett, 2011; 65: 2070

[22] Ni D R, Xue P, Ma Z Y. Metall Mater Trans, 2011; 42A: 2125

[23] Zhang X X, Xiao B L, Ma Z Y. Metall Mater Trans, 2011; 42A: 3229

[24] Cavaliere P, Cabibbo M, Panella F, Squillace A. Mater Design, 2009; 30: 3622

[25] Qin G L, Zhang K, Zhang W B, Wu C S. Trans China Weld Inst, 2010; 31: 5

(秦国梁, 张坤, 张文斌, 武传松. 焊接学报, 2010; 31: 5)

[26] Ghosh K S, Das K, Chatterjee U K. Metall Mater Trans, 2004; 35A: 3681
Outlines

/

〈 〉