Abstract

The twinning induced plasticity (TWIP) steel has received more and more attention for its outstanding combination of good strength and high ductile. It has been proposed that deformation twinning plays an important role in controlling the deformation behavior. The formation of deformation twins is influenced by deformation temperature, strain rate, pre-deformation, grain size and precipitates. The generation of deformation twins in austenitic steel is closely related to precipitates. However, the relationship between strain hardening rate and precipitates in TWIP steels has not been clarified. In this work, the effect of vanadium carbides on the microstructure, strain hardening behavior and mechanical properties of Fe-Mn-C TWIP steel was investigated. The specimens of Fe22Mn0.6C and Fe22Mn0.6C0.19V TWIP steels with similar grain sizes were fabricated through solution treatments at different temperatures. Mechanical properties were measured by tensile tests, and microstructure evolution was observed by EBSD and TEM. The strain hardening rate (dσ/dε)-true strain (ε) curves of two steels were drawn. The results show that for the Fe22Mn0.6C0.19V steel, the strain hardening rate platform appear when true strain ε>0.14, while the strain hardening rate platform appear when the ε>0.12 for the Fe22Mn0.6C steel. The platform of Fe22Mn0.6C steel is significantly longer than that of Fe22Mn0.6C0.19V steel, The platform of Fe22Mn0.6C0.19V steel disappear quickly as true strain ε>0.21. Tensile specimens of Fe22Mn0.6C and Fe22Mn0.6C0.19V steels were observed by TEM, the results show that both the generation and propagation of deformation twins are inhibited significantly by vanadium carbides.

Cite this article

ZHANG Zhi-Bei , LIU Zhen-Yu , ZHANG Wei-Na . EFFECT OF VC PARTICLES ON THE STRAIN HARDENING BEHAVIOR OF TWIP STEEL[J]. Acta Metall Sin, 2012 , 48(9) : 1067 -1073 . DOI: 10.3724/SP.J.1037.2012.00094

References

[1] Frommeyer G, Br¨ux U, Neumann P. ISIJ Int, 2003; 43: 438

[2] Gr¨assel O, Kr¨uger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391

[3] Wang S H, Liu Z Y, Wang G D, Liu J L, Liang G F , Li Q L. J Iron Steel Res, 2010; 17: 70

[4] Vercammen S, Blanpai B, Cooman B C D, Wollants P. Acta Mater, 2004; 52: 2005

[5] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1

[6] Allain S, Chateau J P, Bouaziz O, Migot S, Guelton N. Mater Sci Eng, 2004; A387–389: 158

[7] Hokka M, Kuokkala V T, Curtze S, Vuoristo T, Apostol M. J Phys IV France, 2006; 134: 1301

[8] Xiong R G, Fu R Y , Su Y, Li Q , Wei X C, Li L. J Iron Steel Res, 2009; 16: 81

[9] Li N, Wang Y D, Peng R L, Sun X, Liaw P K, Wu G L, Wang L, Cai H N. Acta Mater, 2011; 59: 6369

[10] Bouaziz O, Allain S, Estrin Y. Scr Mater, 2010; 62: 713

[11] Bouaziz O, Allain S, Scott C. Scr Mater, 2008; 58: 484

[12] Gutierrez–Urrutia I, Zaefferer S, Raabe D. Mater Sci Eng, 2010; A527: 3552

[13] Wang S H, Liu Z Y, Wang G D. Acta Metall Sin, 2009; 45: 1083

(王书涵, 刘振宇, 王国栋. 金属学报, 2009; 45: 1083)

[14] Bracke L, Verbeken K, KestensL, PenningJ. Acta Mater, 2009; 57: 1512

[15] Jiang L. PhD Thesis, Montreal: Mcgill University, 2004

[16] Dumay A. PhD Thesis, Nancy: Institut National Polytechnique de Lorraine, 2008

[17] Chateau J P, Dumay A, Allain S, Jacques A. J Phys: Conf Ser, 2010; 240: 012023

[18] Scott C, Remy B, Collet J L, Cael A, Bao C, Danoix F, Malard B, Curfs C. Int J Mater Res, 2011; 102: 538

[19] Wilkens M. Phys Statd Solid, 1970; 2A: 359

[20] Furuhara T, Shinyoshi T, Miyamoto G, Yamaguchi J, Sugita N, Kimura N, Takemura N, Maki T. ISIJ Int, 2003; 43: 2028

[21] Renard K, Ryelandt S, Jacques P J. Mater Sci Eng, 2010; A527: 2969

[22] Bouaziz O, Allain S, Scott C P, Cugy P, Barbier D. Curr Opin Solid State Mater Sci, 2011; 15: 141

[23] Bouaziz O, Guelton N. Mater Sci Eng, 2001; A319–321: 246

[24] Sevillano J G. Scr Mater, 2008; 59: 135

[25] Allain S, Chateau J P, Dahmoun D, Bouaziz O. Mater Sci Eng, 2004; A387–389: 272

[26] Danaf E E, Kalidindi S R, Doherty R D. Metall Mater Trans, 1999; 30A: 1223

[27] M¨ullner P, Solcnthalcr C. Mater Sci Eng, 1997; A230: 107
Outlines

/

〈 〉