论文

EFFECT OF HAFNIUM CONTENT ON MORPHOLOGY EVOLUTION OF γ′ PRECIPITATES IN P/M Ni–BASED SUPERALLOY

  • ZHANG Xi-Wen ,
  • YU Fu-Meng ,
  • HU Ben-Fu
Expand
  • 1. School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083
    2. High Temperature Material Institute, Central Iron and Steel Research Institute, Beijing 100081
    3. School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Received date: 2012-03-14

  Revised date: 2012-05-19

  Online published: 2012-08-11

Supported by

Supported by National Key Basic Research Program of China (No.2010CB631204) and Sino–Russian Intergovernmental Cooperation in Science and Technology Project (No.CR14–20)

Abstract

The cubic γ′ particle morphology evolution was studied during long time aging process in a powder metallurgy (P/M) Ni–based superalloy with Hf addition. The results show that, during long time aging process, the cubic  γ′ particle splits into a doublet of plantes or an octet of cubes. The octet of cubes with low energy is a preferred shape, it splits no longer. The γ/γ′ lattice misfit varies with different Hf contents. The growth or coarsening process of  γ′ precipitate can be roughly divided into interface controlling and strain controlling stages, the  γ′ precipitate morphology is greatly influenced by the elastic interaction energy between  γ′ particles.

Cite this article

ZHANG Xi-Wen , YU Fu-Meng , HU Ben-Fu . EFFECT OF HAFNIUM CONTENT ON MORPHOLOGY EVOLUTION OF γ′ PRECIPITATES IN P/M Ni–BASED SUPERALLOY[J]. Acta Metall Sin, 2012 , 48(8) : 1011 -1017 . DOI: 10.3724/SP.J.1037.2012.00136

References

[1] Maniar G N, Bridge J E. Metall Trans, 1971; 2: 95

[2] Muzyka D R. Met Eng Q, 1971; 11: 12

[3] Hu B F, Liu G Q, Wu K, Tian G F. Acta Metall Sin, 2012; 48: 257

(胡本芙, 刘国权, 吴 凯, 田高峰. 金属学报, 2012; 48: 257)

[4] Kotval P S, Venables J D, Calder R W. Metall Trans, 1972; 3: 453

[5] Duhl D N, Sullivan C P. J Met, 1971; 23: 38

[6] Dahl J M, Danesi W F, Dunn R G. Metall Trans, 1973; 4: 1087

[7] Maslenkov S B, Burova N N, Khangulov V V. Met Sci Heat Treat, 1980; 22: 283

[8] Miner R V. Metall Trans, 1977; 8A: 259

[9] Khachaturyan A G, Airapetyan V M. Phys Status Solidi, 1974; 26: 611

[10] Qiu Y Y. Acta Mater, 1996; 44: 4969

[11] Yoo Y S. Scr Mater, 2005; 53: 81

[12] Zhang Y W, Wang F M, Hu B F. Acta Metall Sin, 2012; 48: 187

(张义文, 王福明, 胡本芙. 金属学报, 2012; 48: 187)

[13] Lifshitz I M, Slyozov V V. J Phys Chem Solids, 1961; 19: 35

[14] Khachaturyan A G, Semenovskaya S V, Morris Jr J W. Acta Metall, 1988; 36: 1563

[15] Kaufman M J, Voorhees P W, Johnson W C, Biancaniello F S. Metall Mater Trans, 1989; 20A: 2171

[16] Grosdidier T, Hazotte A, Simon A. Mater Sci Eng, 1998; A256: 183

[17] Banerjee D, Banerjee R, Wang Y. Scr Mater, 1999; 41: 1023

[18] Qiu Y Y. J Alloys Compd, 1998; 270: 145

[19] Cha P R, Yeon D H, Chung S H. Scr Mater, 2005; 52: 1241

[20] Miyazaki T, Imamura H, Kozakai T. Mater Sci Eng, 1982; 54: 9

[21] Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1984; 67: 247
Outlines

/