MICROSTRUCTURES AND PROPERTIES OF PULSED MIG ARC BRAZED–FUSION WELDED JOINT OF Al ALLOY AND GALVANIZED STEEL

  • QIN Guo-Liang ,
  • SU Yu-Hu ,
  • YU Shu-Jun
Expand
  • Key Laboratory for Liquid–Solid Structure Evolution and Processing of Materials, Ministry of Education, Shandong University, Jinan 250061

Received date: 2012-02-06

  Revised date: 2012-05-21

  Online published: 2012-08-11

Supported by

Supported by National Natural Science Foundation of China (No.50905099) and Specialized Research Fund for the Doctoral Program of Higher Education (No.20090131120027)

Abstract

Because there are great differences in physicochemical properties and mechanical properties between Al alloy and steel, their joining with high quality and high efficiency is one of difficult problems in study of welding technology. According to their difference in melting point, the brazing–fusion welding technology of Al alloy to steel was developed based on MIG welding. In pulsed MIG arc brazing–fusion welding process, the molten filler metal and Al alloy base metal will form the fusion welded joint, and will form the brazed joint together with unmelted steel plate, which can efficiently prevent the intermetallic compounds (IMCs) from the formation. With the digital pulsed MIG arc welding machine, the brazing–fusion welding of 6013–T4 Al alloy plate to galvanized steel plate was realized with the filler metal of ER4043, and the effect of welding heat input on microstructures and properties of the joint was studied. The results showed that there is a zinc–rich zone in the weld toe of fusion weld in the brazed–fusion welded joint, which is composed of Zn–Al eutectic, Al–rich α solid solutions and Fe3Al. Fe–Al IMCs layer on the brazed interface is 1.05—4.50 μm in thickness and become thicker with the welding heat input being increased. Fe–Al IMCs with sawtooth or tongue shape grow towards the weld, which mainly includes FeAl2, Fe2Al5 and Fe4Al13. With the welding heat input being increased, the tensile strength of the brazed–fusion welded joint firstly increases and then decreases. At the welding heat input of 850 J/cm, the tensile strength of the brazed–fusion welded joint can be up to 229 MPa and the ductile fracture appears in the HAZ of Al alloy. At the lower welding heat input, the brittle fracture easily occurs.

Cite this article

QIN Guo-Liang , SU Yu-Hu , YU Shu-Jun . MICROSTRUCTURES AND PROPERTIES OF PULSED MIG ARC BRAZED–FUSION WELDED JOINT OF Al ALLOY AND GALVANIZED STEEL[J]. Acta Metall Sin, 2012 , 48(8) : 1018 -1024 . DOI: 10.3724/SP.J.1037.2012.00046

References

[1] Elliott S, Wallach E R. Met Constr, 1981; 13: 221

[2] Elrefaey A, Takahashi M, Ikeuchi K. Quart J Jpn Weld Soc, 2005; 23: 186

[3] Sedykh V S. Weld Prod, 1985; 32(2): 28

[4] Calderon P D, Walmsley D R, Munlr Z A. Weld J, 1985; 64: 404

[5] Qiu R F, Iwamoto C, Satonaka S. Mater Charact, 2009; 60(2): 156

[6] Tsujino J, Hidai K, Hasegawa A, Kanai R, Matsuura H, Matsushima K, Ueoka T. Ultrasonics, 2002; 40: 371

[7] Czechowski M. Mater Corros, 2004; 55: 464

[8] Liu S Y, Suzumura A, Ikeshoji T A, Yamazki T. JSME Int J, 2005; 48A: 420

[9] Lin S Y, Qin G L, Lei Z, Wang X Y. Chin Pat, 200610007614.8, 2008

[10] J´acome L A, Weber S, Leitner A, Arenholz E, Bruckner J, Hackl H, Pyzalla A R. Adv Eng Mater, 2009; 11: 350

[11] Vraˇn´akov´a R, F¨ussel U, Zschetzsche J, Juttner S. Weld World, 2005, 49(9): 105

[12] Murakami T, Nakata K, Tong H, Ushio M. ISIJ Int, 2003; 43(10): 159

[13] Zhang H T, Feng J C, He P. Mater Charact, 2007; 58: 588

[14] Dong H G, Yang L Q, Dong C, Kou S D. Mater Sci Eng, 2010; A527: 7151

[15] Lin S B, Song J L, Yang C L, Ma G C. Acta Metall Sin, 2009; 45: 1211

(林三宝, 宋建岭, 杨春利, 马广超. 金属学报, 2009; 45: 1211)

[16] Laukant H, Wallmann E, M¨uller M, Korte W, Stirn B, Haldenwanger H G, Glatzel U. Sci Technol Weld Join, 2005; (2): 219

[17] Dharmendra C, Rao K P, Wilden J, Reich S. Mater Sci Eng, 2011; A528: 1497

[18] Torkamany M J, Tahamtan S, Sabbaghzadeh J. Mater Des, 2010; 31: 458

[19] Mathieu A, Shabadi R, Deschamps A, Suery M, Matte¨? S, Grevey D, Cicala E. Opt Laser Technol, 2007; 39: 652

[20] Bach F W, Beniyas A, Lau K, Versemann R. Adv Mater Res, 2005; (6–8): 143

[21] Lei Z, Qin G L, Lin S Y, Wang X Y. J Mech Eng, 2009; 45(3): 94

(雷振, 秦国梁, 林尚扬, 王旭友. 机械工程学报, 2009; 45(3): 94)

[22] Yang X R. Mater Sci Technol, 2006; 14: 236

(杨修荣. 材料科学与工艺, 2006; 14: 236)

[23] Shi C X, Li H D, Zhou L. The Handbook of Materials Science and Engineering, Vol.1. Bejing: Chemical Industry Press, 2004: 233

(师昌绪, 李恒德, 周廉. 材料科学与工程手册(上卷). 北京: 化学工业出版社. 2004: 233)

[24] Maitra T, Gupta S P. Mater Charact, 2003; 49: 293

[25] Gupta S P. Mater Charact, 2003; 49: 269

[26] Heumann T, Dittrich N A. Z Metallk, 1959; 50: 617

[27] Tomiad S, Nataka K. Surf Coat Technol, 2003; 174: 559
Outlines

/

〈 〉