论文

EFFECTS OF Nb ON RECOVERY OF HOT-DEFORMED AUSTENITE

  • ZHE Wen-Jin ,
  • CHANG Cheng-Jia ,
  • WU Ku-Jie ,
  • YI Pei-Jian ,
  • CHENG Jun-Jie ,
  • ZHANG Xiao-Bing
Expand
  • 1) School of Material Science and Technology, University of Science and Technology Beijing, Beijing 100083
    2) Chief engineer office, Jiangsu Sha Steel Group, Zhangjiagang 215625

Received date: 2012-04-10

  Revised date: 2012-05-09

  Online published: 2012-07-11

Abstract

Solute and precipitates of Nb can effectively affect stastic recrystallization and recoverry of austnite in steels during hot rolling process. However, more research is concerned about the role of Nb precipitation on the strain accumulation in finish rolling process, the solute drag effect of Nb is neglected comparing with precipitates. In this paper, the stress-relaxation curves of the low C high Mn steels with different Nb content were investigated by thermal simulation test, the evolution of dislocation and its interaction with Nb solute and precipitate during recovery process of deformed autentie in a Fe-40%Ni-0.1%Nb (mass fraction) modle steel was also studied by transmission electron microscopy (TEM). Thereby, a theoretical model about recovery of deformed austenite was developed according to the slip of dislocations and the solute drag. The values calculated by the model are consistent with the experimental results and the metallurgic principles. It is shown that both solute and precipitation of Nb can slow down the recovery and enhance the strain accumulation. The Nb solute drag can increase the activation free energy of the recovery U0 and decrease the activation length. It is believed that for Nb micro-alloyed steels with low C and high Mn, the strain accumulation during finish rolling process would be relied on the Nb solute drag effect in hot-strip mill, and both solute drag and precipitation pin effects in heavy plate mill.

Cite this article

ZHE Wen-Jin , CHANG Cheng-Jia , WU Ku-Jie , YI Pei-Jian , CHENG Jun-Jie , ZHANG Xiao-Bing . EFFECTS OF Nb ON RECOVERY OF HOT-DEFORMED AUSTENITE[J]. Acta Metall Sin, 2012 , 48(7) : 775 -781 . DOI: 10.3724/SP.J.1037.2012.00189

References

[1] Cuddy L J. Proceedings of an International Conference on the Themo-Mechanically Processing of Microalloyed Austenite, Metallurgical Society of AIME, 1981: 129

[2] DeArdo A J, Gray J M, Meyer L. In: Stuart H ed., Fundamental Metallurgy of Niobium in Steel, Niobium: AIME, 1981: 685

[3] Miao C L, Shang C J, Zhang G D, Zhu G H, Zurob H S, Subramanian S V. Frontiers Mater Sci China, 2010; 4: 197

[4] Miao C L, Shang C J, Zhang G D, Subramanian S V. Mater Sci Eng, 2010; A527: 4985

[5] Zurob H S, Zhu G, Subramanian S V, Purdy G R, Hutchinson C R, Brechet Y. ISIJ Int, 2005; 45: 713

[6] Zurob H S, Zhu G, Subramanian S V, Purdy G R, Hutchinson C R, Brechet Y. Mater Sci Forum, 2005; 500–501: 123

[7] Hutchinson C R, Zurob H S, Sinclair C W, Brechet Y. Scr Mater, 2008; 59: 635

[8] Nie W J, Xin W F, Xu T M, Shi P J, Zhang X B. Adv Mater Res, 2011; 194–196: 1183

[9] Nie W J, Wang Z F, Li R, Li Y C, Zhang X B. Iron Steel, 2009; 44(8): 76

(聂文金, 王志福, 李冉, 李玉藏, 张晓兵. 钢铁, 2009; 44(8): 76)

[10] Yoshitaka A. In: Enomoto M ed., New Structure Steels and New Design of Conatructions, 6th Workshop on the Ultra–Steel, Tsukuba: The Iron and Steel Institute of Japan, 2002: 91

[11] Liu W J, Jonas J J. Metall MaterTrans, 1988; 19A: 1403

[12] Yang S W, Shang C J, Wang X M, He X L. J Univ Sci Technol Beijing, 2001; 3: 214

[13] Yuan S Q, Yang S W, Shang C J, He X L. Mater Sci Forum, 2003; 426–432: 1307

[14] Yuan S Q, Yang S W, NieWJ, He X L. J Univ Sci Technol Beijing, 2003; 10: 76

[15] Yuan S Q, Yang S W, Nie W J, He X L. Acta Metall Sin, 2004; 40: 887

(苑少强, 杨善武, 聂文金, 贺信莱. 金属学报, 2004; 40: 887)

[16] Karjalainen L P, Perttula J. ISIJ Int, 1996; 36: 729

[17] Zhao J S. Theory Basis of Dislocations, Beijing: National Defence Industry Press, 1989: 125

(赵敬世. 位错理论基础, 北京: 国防工业出版社, 1989: 125)

[18] Verdier M, Brechet Y, Guyot P. Acta Mater, 1999; 47: 127

[19] Feng D. Physics of Metals, Vol.3, Beijing: Science Press, 2000: 373

(冯端, 金属物理学, 第三卷, 北京: 科学出版社, 2000: 373)

[20] Frost H J, Ashby M F. Deformation Mechanism Maps, Oxford: Pergamon Press, 1982: 21

[21] Furu T, Qrsund R, Nes E. Acta Metall Mater, 1995; 43: 2209

[22] Zurob H S, Hutchinson C R, Brechet Y, Purdy G R. Acta Mater, 2002; 50: 3075

[23] Feng D. Physics of Metals, Vol.1, Beijing: Science Press, 2000: 543

(冯端, 金属物理学, 第一卷, 北京: 科学出版社, 2000: 543)

[24] Friedel J. Dislocations. Oxford: Pergamon Press, 1964: 187

[25] Liu W J. Metall Mater Trans, 1995; 26A: 1641

[26] Hou H X, Yang Y, Zhang T, Liu M. Iron Steel, 2009; 44(8): 72

(侯华兴, 杨 颖, 张涛, 刘 明. 钢铁, 2009; 44(8): 72)
Outlines

/

〈 〉