论文

MICROSTRUCTURES AND MECHANICAL PROPERTIES OF CNT/Al COMPOSITES FABRICATED BY HIGH ENERGY BALL-MILLING METHOD

  • XU Shi-Jiao ,
  • XIAO Ba-Lv ,
  • LIU Zhen-Yu ,
  • YU Wen-An ,
  • MA Zong-Xi
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2012-03-16

  Revised date: 2012-05-15

  Online published: 2012-07-11

Abstract

The mixture powders of carbon nanotubes (CNTs) and aluminum were high-energy ball-milled, and then the CNT/Al composites with different CNT contents were fabricated using a power metallurgy method. Microstructure examinations show that a certain volume of CNTs can be uniformly dispersed in the Al matrix by ball-milling and the CNTs have a close bonding with the Al matrix. By using an appropriate ball-milling process flow, the CNTs suffer no serious damage. Tensile tests indicate that the composite reinforced by 1.5% (volume fraction) CNTs exhibits the best mechanical performance, and the yield strength is improved by 53.6% compared with the Al matrix. When the CNT volume fraction reaches 3%, lots of clusters are formed in the composite, and therefore the tensile properties are significantly reduced. Both grain refinement and load transfer are proved to be the strengthening mechanisms of the CNT/Al composites.

Cite this article

XU Shi-Jiao , XIAO Ba-Lv , LIU Zhen-Yu , YU Wen-An , MA Zong-Xi . MICROSTRUCTURES AND MECHANICAL PROPERTIES OF CNT/Al COMPOSITES FABRICATED BY HIGH ENERGY BALL-MILLING METHOD[J]. Acta Metall Sin, 2012 , 48(7) : 882 -888 . DOI: 10.3724/SP.J.1037.2012.00140

References

[1] Pan F S, Zhang D F. Aluminum Alloy and Its Application. Beijing: Chemical Industry Press, 2006: 414

(潘复生, 张丁非. 铝合金及应用. 北京: 化学工业出版社, 2006: 414)

[2] Iijima S. Nature, 1991; 354: 56

[3] Wong E W, Sheehan P E, Lieber C M. Science, 1997; 277: 1971

[4] Treacy M M J, Ebbesen T W, Gibson J M. Nature, 1996; 381: 678

[5] Baughman R H, Zakhidov A A, de Heer W A. Science, 2002; 297: 787

[6] Breuer O, Sundararaj U. Polym Compos, 2004; 25: 630

[7] Zhong R, Cong H T, Hou P. Carbon, 2003; 41: 848

[8] Jiang L, Fan G L, Li Z Q, Kai X Z, Zhang D, Chen Z X, Humphries S, Heness G, Yeung W Y. Carbon, 2011; 49: 1965

[9] Esawi A, Morsi K. Composites, 2007; 38A: 646

[10] Esawi A, Morsi K, Sayed A, Tacher M, Lanka S. Compos Sci Technol, 2010; 70: 2237

[11] Kim K T, Eckert J, Menzel S B, Gemming T, Hong S H. Appl Phys Lett, 2008; 92: 121901

[12] Choi H J, Shin J Y, Min B H, Park J, Bae D H. J Mater Res, 2009; 24: 2610

[13] Liu Z Y, Wang Q Z, Xiao B L, Ma Z Y, Liu Y. Mater Sci Eng, 2010; A527: 5582

[14] Casiraghi C, Ferrari A C, Robertson J. Phys Rev, 2005; 72B: 085401

[15] McGuire K, Gothard N, Gai P L, Dresselhaus M S, Sumanasekera G, Rao A M. Carbon, 2005; 43: 219

[16] Delhaes P, Couzi M, Trinqucoste M, Dentzer J, Hamidou H, Vix–Guterl C. Carbon, 2006; 44: 964

[17] Dominique P, Raynald G, Robin A L D. Composites, 2009; 40A: 1482

[18] Ci L J, Ryu Z Y, Jin–Phillipp N Y, Ruhle M. Acta Mater, 2006; 54: 5367

[19] Esawi A M K, Morsi K, Sayed A, Taher M, Lanka S. Composites, 2011; 42A: 234

[20] Deng C F, Zhang X X, Wang D Z. Mater Lett, 2007; 61: 904

[21] George R, Kashyap K T, Rahul R, Yamdagni S. Scr Mater, 2005; 53: 1159

[22] Kaneko S, Murakami K, Sakai T. Mater Sci Eng, 2009; A500: 8

[23] Liu Z Y, Xiao B L, Wang W G, Ma Z Y. Carbon, 2012; 50: 1843

[24] Wilcox B A, Clauer A H. Acta Metall, 1972; 20: 743

[25] Choi H J, Kwon G B, Lee G Y, Bae D H. Scr Mater, 2008; 59: 360
Outlines

/

〈 〉