Abstract

The uniaxial compression tests of AZ31 magnesium alloy at different strain rates of 0.01-10 s-1 and different deformation temperatures of 523-723 K were performed by using Gleeble-1500 simulator with a maximum strain of 0.916. The influences of deformation temperature and strain rate on the flow stress were investigated. The fine microstructure is attributed to dynamic recrystallization during compression process at 523 K. The stretched grains of dynamic recrystallization and growth up along radial direction were founded in microscopic observation at 723 K. Considering plasticity deformation and friction induced temperature rise, the flow stress was corrected at high strain rate by using temperature compensation. The peak flow stress and unified constitutive model were established based on hyperbolic sine model. Strain sensitivity of flow stress was studied to describe the coupling of materials parameters on the strain, and then the relationship between deformation temperature, strain rate and strain during hot deformation was obtained. Comparing with experimental results, the correlation coefficient and average relative error of predicted and measured values are 0.976 and 5.07\% respectively, it is proved that the model reflects the real deformation feature of the AZ31 magnesium alloy.

Cite this article

XUN Zhao-Yang , LUAN Jing-Dong , LIU Geng , LI Rui , ZHANG Qing-Dong . PREDICTED CONSTITUTIVE MODELING OF HOT DEFORMATION FOR AZ31 MAGNESIUM ALLOY[J]. Acta Metall Sin, 2012 , 48(7) : 853 -860 . DOI: 10.3724/SP.J.1037.2011.00641

References

[1] Liu Q. Acta Metall Sin, 2010; 46: 1458

(刘庆. 金属学报, 2010; 46: 1458)

[2] Xiao P, Liu T M, Jiang D. J Chongqing Univ (Nat Sci Ed), 2006; 29(11): 81

(肖 盼, 刘天模, 姜丹.重庆大学学报(自然科学版), 2006; 29(11): 81)

[3] Guo Q, Zhang H, Chen Z H, Yan H G, Xia W J, Fu D F. Nat Sci J Xiangtan Univ, 2004; 26: 108

(郭强, 张辉, 陈振华, 严红革, 夏伟军, 傅定发.湘潭大学自然科学学报, 2004; 26: 108)

[4] Carl M, Korzekw A C, Cerreta E, Lopez F. J Miner Met Mater Soc, 2004; 56(11): 31

[5] Takuda H. J Mater Process Technol, 1998; 80/81: 513

[6] Galiyev A, Kaibyshev R, Sakai T. Mater Sci Forum, 2003; 419–422: 419

[7] Barnett M R. J Light Met, 2001; 1: 167

[8] Fan Y G, Wang L Y, Huang G S, Huang G J. J Chongqing Univ (Nat Sci Ed), 2003; 26(2): 9

(范永革, 汪凌云, 黄光胜, 黄光杰.重庆大学学报(自然科学版), 2003; 6(2): 9)

[9] Wang Z T, Zhang S H, Qi G X, Wang F, Li Y J. Chin J Nonferrous Met, 2008; 18: 1977

(王忠堂, 张士宏, 齐广霞, 王芳, 李艳娟.中国有色金属学报, 2008; 18: 1977)

[10] Huang G S, Wang L Y, Huang G J, Lu Z W, Song M J. Met Form Technol, 2004; 22(2): 42

(黄光胜, 汪凌云, 黄光杰, 卢志文, 宋美娟. 金属成形工艺, 2004; 22(2): 42)

[11] Guo Q, Yan H G, Chen Z H, Zhang H. Chin J Nonferrous Met, 2005; 15: 900

(郭 强, 严红革, 陈振华, 张辉. 中国有色金属学报, 2005; 15: 900)

[12] Zhang X H, Cui Z S, Ruan X Y. J Shanghai Jiaotong Univ, 2003; 37: 1874

(张先宏, 崔振山, 阮雪榆. 上海交通大学学报, 2003; 37: 1874)

[13] Yu K, Shi T, Wang R C, Li W X, Wang X Y, Cai Z Y. J Cent South Univ (Sci Technol), 2008; 39: 216

(余琨, 史禔, 王日初, 黎文献, 王晓艳, 蔡志勇. 中南大学学报(自然科学版), 2008; 39: 216)

[14] Sun C Y, Liu J R, Li R, Zhang Q D, Dong J X. Real Met, 2011; 30: 81

[15] Luan N, Li L X, Li G Y, Zhong Z H. Chin J Nonferrous Met, 2007; 17: 1678

(栾娜, 李落星, 李光耀, 钟志华. 中国有色金属学报, 2007; 17: 1678)

[16] Luo Z J, Yang Q, Ji W H. Chin J Nonferrous Met, 2000; 10: 804

(罗子健, 杨旗, 姬婉华. 中国有色金属学报, 2000; 10: 804)

[17] Zhang W H, Zhang S H. Acta Metall Sin, 2006; 42: 1036

(张伟红, 张士宏. 金属学报, 2006; 42: 1036)

[18] Wang Z X, Liu X F, Xie J X. Acta Metall Sin, 2008; 44: 1378

(王智祥, 刘雪峰, 谢建新. 金属学报, 2008; 44: 1378)

[19] Sellars C M, McTegart W J. Acta Metall, 1966; 14: 1136

[20] Mcqueen H J, Ryan N D. Mater Sci Eng, 2002; A322: 43

[21] Gronostajski Z J. J Mater Process Technol, 1998; 78: 84

[22] Whittenberger J D. Mater Sci Eng, 1986; 77: 103

[23] Zener C, Hollomon H. J Appl Phys, 1944; 15: 22

[24] Sun C Y, Liu J R, Li R, Zhang Q D. Acta Metall Sin, 2011; 47: 191

(孙朝阳, 刘金榕, 李瑞, 张清东. 金属学报, 2011; 47: 191)

[25] Ismael A M, Ahmed H, Johannes R. Mater Sci Eng, 2009; A504: 40
Outlines

/

〈 〉