论文

MICROSTRUCTURAL CHARACTERIZATION OF A Ru-CONTAINING SINGLE CRYSTAL NICKEL-BASED SUPERALLOY

  • TAN Xi-Peng ,
  • LIU Jin-Lai ,
  • SONG Xiao-Beng ,
  • JIN Shou ,
  • XUN Xiao-Feng ,
  • HU Zhuang-Qi
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2. Graduate University of Chinese Academy of Sciences, Beijing 100049

Received date: 2011-10-09

  Revised date: 2012-04-06

  Online published: 2012-05-11

Supported by

Project supported by the National Basic Research Program of China

Abstract

The microstructure of a Ru--containing single crystal nickel-based superalloy, which is a potential fourth generation single crystal nickel-based superalloy heat treated, has been investigated. The X--ray diffraction (XRD) results indicate that this single crystal superalloy is not a perfect monocrystal, which is comprised of many subgrains with an average neighboring misorientation difference about 0.5° and the maximum misorientation deviation about 3°; and each subgrain includes large numbers of mosaic structures with misorientation difference of 0.1°---0.2° between each other. It is found that the microstructure of the heat treated alloy is of heterogeneity, where the volume fraction of γ' phase increases and the γ' lattice misfit decreases. It is shown that the average size of γ' phase is 0.39 μm, the average γ' volume fraction 70% and the average γ' lattice misfit --2.0×10$-3. The evolution of this microstructure was also briefly described.

Cite this article

TAN Xi-Peng , LIU Jin-Lai , SONG Xiao-Beng , JIN Shou , XUN Xiao-Feng , HU Zhuang-Qi . MICROSTRUCTURAL CHARACTERIZATION OF A Ru-CONTAINING SINGLE CRYSTAL NICKEL-BASED SUPERALLOY[J]. Acta Metall Sin, 2012 , 48(5) : 569 -574 . DOI: 10.3724/SP.J.1037.2011.00629

References

[1] Gell M, Duhl D N, Giamei A F. In: Tien J, Wlodek S, Morrow H, Gell M, Maurer G E, eds., Superalloys 1980, Champion, PA: TMS, 1980: 205

[2] Hu Z Q, Liu L R, Jin T, Sun X F.  Aerial Eng, 2005; 31(3): 1

    (胡壮麒, 刘丽荣, 金涛, 孙晓峰. 航空发动机, 2005; 31(3): 1)

[3] Leverant G, Kear B, Oblak J.  Metall Mater Trans, 1973; 4B: 355

[4] Nathal M V, Ebert L.  Metall Mater Trans, 1985; 16A: 427

[5] Pollock T M, Argon A S.  Acta Metall Mater, 1992; 40: 1

[6] Reed R C, Matan N, Cox D C, Rist M A, Rae C M F.  Acta Mater, 1999; 47: 3367

[7] Reed R C, Cox D C, Rae C M F.  Mater Sci Eng, 2007; A448: 88

[8] Caron P, Khan T.  Mater Sci Eng, 1983; 61: 173

[9] Nathal M V.  Metall Mater Trans, 1987; 18A: 1961

[10] Nathal M V, MacKay R, Miner R.  Metall Mater Trans, 1989; A20: 133

[11] Tan X P, Liu J L, Jin T, Hu Z Q, Hong H U, Choi B G, Kim I S, Jo C Y.  Mater Sci Eng, 2011; A528: 8381

[12] Caron P. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J, eds., Superalloys 2000, Champion, PA: TMS, 2000: 737

[13] Koizumi Y, Kobayashi T, Yokokawa T, Zhang J X, Osawa M, Harada H, Aoki Y, Arai M.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S, eds., Superalloys 2004, Champion, PA: TMS, 2004: 35

[14] Han Y, Ma W, Dong Z, Li S, Gong S. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S,Woodard S A, eds.,  Superalloys 2008, Champion, PA: TMS, 2008: 91

[15] Chen J Y, Zhao B, Feng Q, Cao L M, Sun Z Q.  Acta Metall Sin, 2010; 46: 897

     (陈晶阳, 赵宾, 冯强, 曹腊梅, 孙祖庆. 金属学报, 2010; 46: 897)

[16] Chen J--Y, Feng Q, Cao L--M, Sun Z--Q.  Progress Nat Sci: Mater Int, 2010; 20: 61

[17] Warren B E.  X-ray Diffraction. New York: Dover Publications, 1990: 331

[18] Bruckner U, Epishin A, Link T.  Acta Mater, 1997; 45: 5223

[19] Tan X P, Liu J L, Song X P, Jin T, Sun X F, Hu Z Q.  J Mater Sci Technol, 2011; 27: 899

[20] Zhang J X, Wang J C, Harada H, Koizumi Y.  Acta Mater, 2005; 53: 4623

[21] Yeh A C, Rae C M F, Tin S. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J,Walston S, eds.,  Superalloys 2004, Champion, PA: TMS, 2004: 677

[22] Fan X.  Metal X-ray Analysis. Bejing: Mechanical Industry Press, 1998: 43

     (范雄. 金属X射线学. 北京: 机械工业出版社, 1998: 43)

[23] Ibers J A, Hamilton W C.  International Tables for X-ray Crystallography Vol.IV.Birmingham: Kynoch Press, 1974: 71

[24] Murakami H, Saito Y, Harada H. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M,Woodford D A, eds.,  Superalloys 1996, Champion, PA: TMS, 1996: 249

[25] Ofori A, Rossouw C, Humphreys C.  Acta Mater, 2005; 53: 97

[26] Murakumo T, Kobayashi T, Koizumi Y, Harada H.  Acta Mater, 2004; 52: 3737

[27] Pan J S, Jian M T, Tian M B.  Fundamentals of Materials Science. Beijing: Tsinghua Press, 1998: 563

     (潘金生, 健民仝, 田民波. 材料科学基础. 北京: 清华大学出版社, 1998: 563)

[28] Reed R C.  The Superalloys: Fundamentals and Applications. Cambridge: Cambridge University Press, 2006: 141

[29] Feng Q, Nandy T K, Rowland L J, Tryon B, Banerjee D, Pollock T M.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S, eds., Superalloys 2004, Champion, PA: TMS, 2004: 769
Outlines

/

〈 〉