Abstract

Arc ion plating (AIP) has been widely used for depositing various kinds of coatings due to the excellent characteristics of high deposition rate, convenient parameter control, high degree of ionization in the target material, good coating--substrate adhesion, flexibility of target arrangements and merits of producing coatings with high packing density. Magnetic films, with a few micrometers or less, could be utilized in the electronics industry, such as magnetic recording, magnetic microelectromechanical systems, magneto optical modulator, and so on. In AIP process, due to magnetic shielding and self--induced magnetic field, arc spot on the surface of the magnetic target moved outside all the time, and the erosion of the magnetic target could not be stable. In this study, arc spot outside moving and unstable erosion of the magnetic target in arc ion plating have been investigated. The distribution of the magnetic field of the nonmagnetic target and the magnetic target under an additional magnetic field was simulated by the finite element method (FEM). The effect of magnetic field on the arc spot movement was researched. With the physical mechanism of the arc spot discharge, the feasibility on the solution of the application problem of the magnetic target has been discussed by the program of the composited structure target, which were composed of magnetic target materials and target shell of low saturation vapor pressure metal, target shell of insulating ceramics, or target shell of soft magnetic metal. The results showed that all these solutions could solve the problem of arc spot outside moving efficiently. In the study, the transition temperature is (136.6±23.0) ℃ in the solutions of the target shell of low saturation vapor pressure metal or insulating ceramics, during which the arc striking frequently transformed to the controlled movement of arc spot.

Cite this article

CHANG Zheng-Kai , XIAO Jin-Quan , CHEN Yo-Qiu , LIU Shan-Chuan , GONG Jun , XUN Tiao . STUDY ON DEPOSITION OF MAGNETIC FILMS USING ARC ION PLATING[J]. Acta Metall Sin, 2012 , 48(5) : 547 -554 . DOI: 10.3724/SP.J.1037.2012.00056

References

[1] Ueda K, Tabata H, Kawai T.  Appl Phys Lett, 2001; 79: 988

[2] Ramesh R, Spaldin N A.  Nat Mater, 2007; 6: 21

[3] Sharma P, Gupta A, Rao K V, Owens F J, Sharma R, Ahuja R, Guillen J M O, Johansson B, Gehring G A. Nat Mater, 2003; 2: 673

[4] Bakonyi I, Burgstaller A, Socher W, Voitlander J,Toth-Kadar E, Lovas A, Ebert H, Wachtel E, Willmann N, Liebermann H H. Phys Rev, 1993; 47B: 14961

[5] Kashiwagi M, Ido S.  Vacuum, 1999; 53: 33

[6] Huang J C A, Hu Y M, Yu C C.  J Appl Phys, 1998; 83: 7046

[7] Di G Q.  Chin Pat, CN101570851A, 2009

    (狄国庆. 中国专利, CN101570851A, 2009)

[8] Chen J S, Lau S P, Zhang Y B, Sun Z, Tay B K, Sun C Q.  Thin Solid Films, 2003; 443: 115

[9] Wang Q M, Kim K H.  Acta Mater, 2009; 57: 4974

[10] Sun L, Li H K, Lin G Q, Dong C.  J Vac Sci Technol, 2010; 28A: 1299

[11] Chang Z K, Wan X S, Pei Z L, Gong J, Sun C.  Surf Coat Technol, 2011; 205: 4690

[12] Wang T G, Jeong D, Liu Y, Wang Q, Iyengar S, Melin S, Kim K H.  Surf Coat Technol, 2012; 206: 2638

[13] Lieberman M A, Lichtenberg A J, translated by Pu Y K, Zhu X M, Guo Z G, Wang J L, Mao Z G, Feng Y, Wang X,Song X B, Ma J, Zhang G L, Ma J X, Chen Y.  Priciples of Plasma Discharges and Materials Processing. 2nd Ed.,Beijing: Science Press, 2007: 9

(Lieberman M A, Lichtenberg A J著, 蒲以康, 朱悉铭, 郭志刚, 王久丽, 毛志国, 冯阳, 王旭, 宋旭波,马杰, 张谷令, 马锦秀, 陈宇译. 等离子体放电原理与材料处理. 第二版. 北京: 科学出版社, 2007: 9)

[14] Lang W C, Xiao J Q, Gong J, Sun C, Huang R F, Wen L S.  Acta Metall Sin, 2010; 46: 372

     (郎文昌, 肖金泉, 宫骏, 孙超, 黄荣芳, 闻立时. 金属学报, 2010; 46: 372)

[15] Daalder J E.  J Phys, 1983; 16D: L177

[16] Drouet M G.  IEEE Trans Plasma Sci, 1985; 13: 235

[17] Beilis I I.  IEEE Trans Plasma Sci, 2002; 30: 2124

[18] Hantzsche E.  IEEE Trans Plasma Sci, 2003; 31: 799

[19] Lang W C, Xiao J Q, Gong J, Sun C, Huang R F, Wen L S.  Vacuum, 2010; 84: 1111

[20] Feng D, Qiu D R.  Metal Physics. vol.4,Beijing: Science Press, 1998: 441

     (冯端, 丘第荣著. 金属物理学. 第4卷, 北京: 科学出版社, 1998: 441)

[21] Dai D S, Qian K M.  Ferromagnetics. vol.1, Beijing: Science Press, 1987: 120

     (戴道生, 钱昆明著, 铁磁学(上册). 第1卷, 北京: 科学出版社, 1987: 120)

[22] Lang Y J, Che Y C.  Thermodynamics Databook of Inorganic Matter.Shenyang: Northeast University Press, 1993: 513

     (梁英教, 车荫昌编. 无机物热力学数据手册. 沈阳: 东北大学出版社, 1993: 513)
Outlines

/

〈 〉