论文

INVESTIGATION OF DYNAMIC MECHANICAL BEHAVIOR OF A NEW Zr-Ti ALLOY

  • YU Jie ,
  • ZHANG Hong-Wei ,
  • YU Ai-Min ,
  • ZHANG Hai-Feng
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research,Chinese Academy of Sciences,Shenyang 110016

Received date: 2011-12-28

  Revised date: 2012-04-12

  Online published: 2012-05-11

Abstract

Zirconium based alloy is a new type structural material with high specific strength and good comprehensive properties. In this article, quasi-static compression at room temperature and dynamic compression under various temperatures were performed to a new zirconium-titanium alloy. It was found that this alloy showed good strength and plasticity, and the strength increased and plasticity decreased with increasing strain rate or decreasing temperature. A constitutive model under dynamic compression was established based on Johnson-Cook model, and accorded well with experimental results.

Cite this article

YU Jie , ZHANG Hong-Wei , YU Ai-Min , ZHANG Hai-Feng . INVESTIGATION OF DYNAMIC MECHANICAL BEHAVIOR OF A NEW Zr-Ti ALLOY[J]. Acta Metall Sin, 2012 , 48(5) : 636 -640 . DOI: 10.3724/SP.J.1037.2011.00808

References

[1] Tribble A.  The Space Environment-Implications for Spacecraft Design. Princeton: Princeton University Press, 1995: 1

[2] Lowenstein D I, Rusek A.  Radiat Environ Biophys, 2007; 46: 91

[3] Nikiforov A,  Chumakov A. In: Daglis I A ed.,  Effects of Space Weather on Technology Infrastructure. Dordrecht: Kluwer Academic Publishers, 2004: 165

[4] Shilobreeva S N, Kashkarov L L, Barabanenkov M Y, Pustovit A N,Zinenko V I, Agafonov Y A.  Doklady Earth Sci, 2006; 411: 9

[5] Wicklein M, Ryan S, White D M, Clegg R A.  Int J Impact Eng,2008; 35: 1861

[6] Sakuraba K, Tsuruda Y, Hanada T, Liou J C, Akahoshi Y. Int J Impact Eng, 2008; 35: 1567

[7] Sorensen B R, Kimsey K D, Love B M.  Int Impact Eng, 2008; 35: 1808

[8] Zhao W J.  Rare Met Lett, 2004; 23(5): 15

    (赵文金. 稀有金属快报, 2004; 23(5): 15)

[9] Liu J Z.  Nuclear Structural Materials. Beijing: Chemical Industry Press, 2007: 5

    (刘建章. 核结构材料, 北京: 化学工业出版社, 2007: 5)

[10] Zhao W J, Zhou B X, Miao Z, Peng Q, Jiang Y R, Jiang H M, Pang H. Atom Energy Sci Technol, 2005; 39(suppl): 2

     (赵文金, 周邦新, 苗志, 彭倩, 蒋有荣, 蒋宏曼, 庞华.原子能科学技术, 2005; 39(增刊): 2)

[11] Wang R S, Weng L K, Zhang Y W, Geng J Q, Wang J H.  Mater Rev,2011; 25(13): 105

     (王荣山, 翁立奎, 张晏玮, 耿建桥, 王锦红. 材料导报, 2011; 25(13): 105)

[12] Zhang J, Wang G P, Zuo X T.  J Netshape Forming Eng, 2011; (5); 35

     (张建, 王国平, 左小涛. 精密成形工程, 2011; (5); 35)

[13] Liu W Q, Zhu X Y, Wang X J, Li Q, Yao M Y, Zhou B X. Atom Energy Sci Technol, 2010; 44: 1477

     (刘文庆, 朱晓勇, 王晓姣, 李强, 姚美意, 周邦新. 原子能科学技术,2010; 44: 1477)

[14] Peker A, Johnson W L.  Appl Phys Lett, 1993; 63: 2342

[15] Inoue A, Zhang T, Saida J, Matsushita M, Chen M W, Sakurai T. Mater Trans JIM, 1999; 40: 1137

[16] Bruck H A, Christman T, Rosakis A J, Johnson W L.  Scr Metall Mater,1994; 30: 429

[17] Inoue A.  Acta Mater, 2000; 48: 279

[18] Liang S X, Ma M Z, Jing R, Zhang X Y, Liu R P.  Mater Sci Eng,2012; A532: 1

[19] Cui Z Q, Tan Y C.  Metallography and Heat Treatment.Beijing: Mechanical Industry Press, 2007: 186

     (崔忠圻, 覃耀春. 金属学与热处理. 北京: 机械工业出版社, 2007: 186)

[20] Gao L Q, Zhu J H, Li H, Sun J K.  Rare Met Mater Eng, 2008; 37: 1051

     (高灵清, 朱金华, 李慧, 孙建科. 稀有金属材料与工程, 2008; 37: 1051)

[21] Chang L Z, Pan Y T, Zhang Z M, Xue Y.  Ordnance Mater Sci Eng,2010; 33(4): 68

     (常列珍, 潘玉田, 张治民, 薛勇. 兵器材料科学与工程, 2010; 33(4): 68)

[22] Johnson G R, Cook W H.  Proc 7th Int Symp on Ballistics,Hague, Netherlands, 1983: 541

[23] Johnson G R, Cook W H.  Eng Fract Mech, 1985; 21: 31
Outlines

/

〈 〉