论文

HOT CORROSION BEHAVIOR OF A (NiCoCrAlYSiB+AlSiY) COMPOSITE COATING

  • LV Xu-Yang ,
  • YU Tai-Qian ,
  • JIANG Su-Meng ,
  • MA Jun ,
  • LIU Shan-Chuan ,
  • GONG Jun ,
  • XUN Tiao
Expand
  • State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences,Shenyang 110016

Received date: 2012-01-13

  Revised date: 2012-02-26

  Online published: 2012-04-11

Supported by

National Basic Research Program of China;National Natural Science Foundation of China

Abstract

Two kinds of the coatings, the conventional NiCoCrAlYSiB coating and the composite coating (NiCoCrAlYSiB+AlSiY), were prepared using arc ion plating (AIP) on the Ni base single crystal superalloy substrate. Comparative studies of the hot corrosion behaviors of the substrate and two different coatings in Na2SO4 + K2SO4 and Na2SO4 + NaCl at 900 and 700 ℃ were investigated. The results showed that, during the hot corrosion at 900 ℃, NiO was formed on the surface of the substrate while Cr2O3 was formed on the surface of the conventional coating with the formation of internal oxidation and sulfidation, and Al2O3 was formed on the surface of the composite coating. Slighter internal oxidation appeared in the outer layer of the composite coating. The composite coating contained sufficient Al reservoirs to supply the formation and repair of Al2O3. During the hot corrosion at 700 ℃, NiO was formed on the surface of the substrate and Cr2O3 was formed on the surface of the conventional coating with severe internal oxidation, while internal oxidation appeared in the outer layer of the composite coating. The Cr-enriched inner layer did not suffer from corrosion damage, which can improve the corrosion resistance of the composite coating.

Cite this article

LV Xu-Yang , YU Tai-Qian , JIANG Su-Meng , MA Jun , LIU Shan-Chuan , GONG Jun , XUN Tiao . HOT CORROSION BEHAVIOR OF A (NiCoCrAlYSiB+AlSiY) COMPOSITE COATING[J]. Acta Metall Sin, 2012 , 48(4) : 461 -468 . DOI: 10.3724/SP.J.1037.2012.00031

References

[1] Liang J J, Wei H, Hou G C, Guan H R, Hu Z Q.  Rare Met Mater Eng,2008; 37: 1134

    (梁静静, 韦华, 侯桂臣, 管恒荣, 胡壮麒. 稀有金属材料与工程, 2008; 37: 1134)

[2] Nicholls J R, Stephenson D J.  Met Mater, 1991; 7: 156

[3] Brandl W, Toma D, Kruger J, Grabke H J, Matthaus G.  Surf Coat Technol, 1997; 94: 21

[4] Czech N, Schmitz F, Stamm W.  Mater Manuf Process, 1995; 10: 1021

[5] Goward G W.  Surf Coat Technol, 1998; 108: 73

[6] Wang Q M, Wu Y N, Ke P L, Cao H T, Gong J, Sun C, Wen L S. Surf Coat Technol, 2004; 186: 389

[7] Xu C Z, Jiang S M, Ma J, Gong J, Sun C.  Acta Metall Sin,2009; 45: 964

    (徐朝政, 姜肃猛, 马军, 宫骏, 孙超. 金属学报, 2009; 45: 964)

[8] Guo M H, Wang Q M, Gong J, Sun C, Huang R F, Wen L S. Corros Sci, 2006; 48: 2750

[9] Wang Q M.  PhD Thesis, Institute of Metal Research,Chinese Academy of Sciences, Shenyang, 2006

    (王启民. 博士学位论文. 中国科学院金属研究所, 沈阳, 2006)

[10] Tang F, Ajdelsztajn L, Schoenung J M.  Oxid Met, 2004; 61: 219

[11] Suresh S.  Science, 2001; 292: 2447

[12] Wang W X, Jiang S M, Wei G Z, Ma J, Gong J, Sun C. Acta Metall Sin, 2011; 47: 578

     (王维新, 姜肃猛, 卫广智, 马军, 宫骏, 孙超.金属学报, 2011; 47: 578)

[13] Li M S.  High Temperature Corrosion of Metal.Beijing: Metallurgical Industry Press, 2001: 417

     (李美栓. 金属的高温腐蚀. 北京: 冶金工业出版社, 2001: 417)

[14] Peng X, Jiang S M, Duan X H, Gong J, Sun C.  Acta Metall Sin,2009; 45: 378

     (彭新, 姜肃猛, 段绪海, 宫骏, 孙超. 金属学报, 2009; 45: 378)

[15] Grunling H W, Bauer R.  Thin Solid Films, 1982; 95: 3

[16] Nicholls J R, Simms N J, Chan W Y, Evans H E.  Surf Coat Technol,2002; 149: 236

[17] Wang Q M, Wu Y N, Ke P L, Ji A L, Sun C, Huang R F, Wen L S. Acta Metall Sin, 2004; 40: 399

     (王启民, 武颖娜, 柯培玲, 纪爱玲, 孙超, 黄荣芳, 闻立时. 金属学报,2004; 40: 399)

[18] Felix P C.  Deposition and Corrosion in Gas Turbines.London: Applied Science Publish, 1973: 331

[19] Li W J, Liu Y, Wang Y, Han C, Tang H P.  Chin J Nonferrous Met,2010; 12: 2327

     (李维杰, 刘咏, 王岩, 韩朝, 汤慧萍. 中国有色金属学报,2010; 12: 2327)

[20] Simms N J, Encinas--Oropesa A, Nicholls J R.  Mater Corros,2008; 59: 476

[21] Eliaz N, Shemesh G, Latanision R M.  Eng Fail Anal, 2002; 9: 31

[22] Li M H, Zhang Z Y, Sun X F, Li J G, Yin F S, Hu W Y, Guan H R,Hu Z Q.  Surf Coat Technol, 2003; 165: 241

[23] Mckee D W, Shores D A, Luthra K L.  J Eectrochem Soc,1978; 125: 411

[24] Tsaur C C, Rock J C, Chang Y Y.  Mater Chem Phys, 2005; 91: 330
Outlines

/

〈 〉