论文

LOCALIZED ELECTROCHEMICAL CHARACTERIZATION OF HIGH STRENGTH ALUMINIUM ALLOY AT THE CRACK TIP IN 3.5NaCl SOLUTION

  • SHENG Hai ,
  • DONG Tiao-Fang ,
  • XIAO Kui ,
  • LI Xiao-Gang
Expand
  • Key Laboratory of Corrosion and Protection, Ministry of Education, Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083

Received date: 2011-11-07

  Revised date: 2012-03-10

  Online published: 2012-04-11

Supported by

National Natural Science Foundation of China

Abstract

The electrochemical microcapillary technique and scanning Kelvin probe (SKP) were applied to study the localized electrochemical characterization and corrosion behavior at the crack tip of 2024-T351 aluminium alloy in 3.5NaCl. To investigate the effect of stress on the localized corrosion process at the crack tip, numerical simulation of the stress distribution on a pre-cracked wedge-open loading (WOL) specimen was conducted using a commercial software package ABAQUS 6.10. Polarization curves revealed that corrosion potential at the crack tip was more negative than that within the region away from the crack tip. Localized electrochemical impedance spectroscope (EIS) showed that the passive film was thinner at the crack tip than within the region away from the crack tip. The results indicate that the crack tip is more electrochemically active than the region away from the crack tip. Furthermore, passive film at the crack tip was less stable than that on other region of the specimen surface. SKP measurements demonstrated that there was a non-uniform distribution of Volta potential on the pre-cracked WOL specimen surface, with a more positive Volta potential occurring at the crack tip after 24 h immersion into 3.5NaCl solution. This might be explained by the preferential anodic dissolution and the accumulation of the corrosion product at the crack tip. Numerical simulation results showed that a very high local stress concentration was developed at the crack tip, which could enhance the electrochemical activity around the crack tip and promote the dissolution process therein. Moreover, a galvanic couple could also occur between the crack tip acting as the anode and the distant region as the cathode, which results from the differences of the corrosion potentials and the electrochemical activities between them. As a result, the anodic dissolution of 2024-T351 aluminium alloy at the crack tip is enhanced.

Cite this article

SHENG Hai , DONG Tiao-Fang , XIAO Kui , LI Xiao-Gang . LOCALIZED ELECTROCHEMICAL CHARACTERIZATION OF HIGH STRENGTH ALUMINIUM ALLOY AT THE CRACK TIP IN 3.5NaCl SOLUTION[J]. Acta Metall Sin, 2012 , 48(4) : 414 -419 . DOI: 10.3724/SP.J.1037.2011.00692

References

[1] Starke E A, Staley J T.  Prog Aerosp Sci, 1996; 32: 131

[2] Immarigeon J P, Holt R T, Koul A K, Zhao L, Wallace W, Beddoes J C.  Mater Charact, 1995; 35: 41

[3] Szklarska-Smialowska Z.  Corros Sci, 1999; 41: 1743

[4] Gupta R K, Sukiman N L, Cavanaugh M K, Hinton B R W,Hutchinson C R, Birbilis N.  Electrochim Acta, 2012; 66: 245

[5] Ruan S, Wolfe D A, Frankel G S.  J Stat Plann Inference,2004; 126: 553

[6] Knight S P, Salagaras M, Trueman A R.  Corros Sci,2011; 53: 727

[7] Speidel M.  Metall Mater Trans, 1975; 6A: 631

[8] Lee H, Kim Y, Jeong Y, Kim S.  Corros Sci, 2012; 55: 10

[9] Vogt H, Speidel M O.  Corros Sci, 1998; 40: 251

[10] Liu X D, Frankel G S, Zoofan B, Rokhlin S I. Corros Sci, 2007; 49: 139

[11] Liu X D, Frankel G S, Zoofan B, Rokhlin S I. Corros Sci, 2004; 46: 405

[12] Cooper K R, Kelly R G.  Corros Sci, 2007; 49: 2636

[13] Moon S M, Pyun S I.  Electrochim Acta, 1999; 44: 2445

[14] Zhang B, Li Y, Wang F H.  Corros Sci, 2007; 49: 2071

[15] Huang V M W, Wu S L, Orazem M E, Pebere N, Tribollet B,Vivier V.  Electrochim Acta, 2011; 56: 8048

[16] Rohwerder M, Turcu F, Lamaka S V, Zheludkevich M L, Yasakau K A,Montemor M F, Ferreira M G S.  Electrochim Acta, 2007; 53: 290

[17] Rossi S, Fedel M, Deflorian F, del Carmen Vadillo M. C R Chim, 2008; 11: 984

[18] Nazarov A, Thierry D.  Electrochim Acta, 2007; 52: 7689

[19] Bohni H, Suter T, Schreyer A.  Electrochim Acta, 1995; 40: 1361

[20] Lohrengel M M, Moehring A, Pilaski M.  Electrochim Acta,2001; 47: 137

[21] Klemm S O, Kollender J P, Hassel A W.  Corros Sci, 2011; 53: 1

[22] Breimesser M, Ritter S, Seifert H P, Virtanen S, Suter T. Corros Sci, 2012; 55: 126

[23] Jorcin J B, Krawiec H, Pebere N, Vignal V.  Electrochim Acta,2009; 54: 5775

[24] Krawiec H, Vignal V, Akid R.  Electrochim Acta, 2008; 53: 5252

[25] Burleigh T D, Smith A T.  J Electrochem Soc, 1991; 138: L34

[26] Schmutz P, Frankel G S.  J Electrochem Soc, 1998; 145: 2285

[27] Zhang G A, Cheng Y F.  Corros Sci, 2010; 52: 960

[28] Dong C F, Sheng H, An Y H, Li X G, Xiao K, Cheng Y F.Prog Org Coat, 2010; 67: 269
Outlines

/

〈 〉