论文

TYPE IV CREEP RUPTURE CHARACTERISTICS OF P92 STEEL WELDMENT

  • YU Hua ,
  • PAN Qian-Gang ,
  • DAO Yong-Shun ,
  • ZHANG Ying-Lin ,
  • ZENG Hui-Jiang ,
  • LIU Hong
Expand
  • 1. School of Power and Mechanics, Wuhan University, Wuhan 430072
    2. Dongfang Electric Corporation, Dongfang Boiler Group Co Ltd.,  Zigong 643001

Received date: 2011-10-17

  Revised date: 2012-01-03

  Online published: 2012-04-11

Supported by

National Natural Science Foundation of China

Abstract

Creep tests at 600~650℃ with applied stresses in the range 100~240MPa and microstructural observations by means of OM, SEM, TEM were conducted on weld joints of P92 steel prepared by SAW process to investigated its characteristics of Type Ⅳ creep rupture. The results showed that Type Ⅳ failure took place at higher temperature and lower stress and tend to have a critical condition expressed by Larson-Miller parameter(L.M.P.)or stress level which values are 35.5 and 120MPa respectively. Type Ⅳ failure showed a lack of ductility and located in the fine grained HAZ(heated to just above AC3)close to intercritical HAZ, where microstructural changes are obviously different from those in the base metal, including formation of equiaxed sub-grain structure, mass precipitation and rapid growth of Laves phases on the grain boundaries during creep exposure, which lead to the Type Ⅳ failure. The size of M23C6 carbide in the AC3 FGHAZ was almost the same as that in the base metal, which has little effect on the failure. Type Ⅳ rupture is a brittle intergranular fracture due to cavity coalescence, which were nucleated at coarse precipitates of Laves phase. The void area ratio of f or AA is employed to quantify grain boundary damage and evaluate Type Ⅳ failure of P92 steel weld joints, and when their values were above 1~1.2% or 0.5%, Type Ⅳ failure would occur.

Cite this article

YU Hua , PAN Qian-Gang , DAO Yong-Shun , ZHANG Ying-Lin , ZENG Hui-Jiang , LIU Hong . TYPE IV CREEP RUPTURE CHARACTERISTICS OF P92 STEEL WELDMENT[J]. Acta Metall Sin, 2012 , 48(4) : 427 -434 . DOI: 10.3724/SP.J.1037.2011.00646

References

[1] Jorgen B, Sven K, Rudolph B.  Energy, 2006; 31: 1437

[2] Richardot D, Vaillant J C, Arbab A, Bendick W.  The T92/P92 steel book. 2nd Ed. Boulogne: Vallourec & Mabbesmann tubes, 2002

[3] Shen Q, Liu H G.  Electr Power Constrc, 2010; 31: 71

    (沈琦, 刘鸿国. 电力建设, 2010, 31: 71)

[4] Tu S D, Xuan F Z, Wang W Z.  Acta Metall Sin, 2009; 45: 781

 (涂善东, 轩福贞, 王卫泽. 金属学报, 2009, 45: 781)

[5] Scheller H J, Haigh L, Woitscheck A.  Der Mascginenschaden,1974; 47: 1

[6] Laha K, Chandravathi K S, Rao K B S, Mannan S L, Sastry D H. Metall MaterTrans, 2001; 32A: 115

[7] Tabuchi M, Watanabe T, Kubo K, Matsui M, Kinugawa J, Abe F. J Pressure Vessel Pip, 2001; 78: 779

[8] Kojima T, Hayashi K, Kajita Y.  ISIJ Int, 1995; 35: 1284

[9] Matsui M, Tabuchi M, Watanabe T, Kubo K.  ISIJ Int, 2001; 41: S126

[10] Li D J, Shinozaki K, Kuroki H.  Sci Technol Weld Join, 2003; 8: 296

[11] Abd El--Azim M E, Nasreldin A M, Zies G, Klenk A. Mater Sci Technol, 2005; 21: 779

[12] Watanabe T, Tabuchi M, Yamazaki M, Hongo H, Tanabe T.  J Pressure Vessel Pip, 2006; 83: 63

[13] Albert S K, Matsui M, Watanabe T, Hongo H, Kubo K.  J Pressure Vessel Pip, 2003; 80: 405

[14] Korcakova L, Hald J.  Mater Charact, 2001; 47: 111

[15] Qin G Y.  Quality Metallography. Chendu: Sichuan Publishing House of Science and Technology, 1987: 1

     (秦国友. 定量金相. 成都: 四川科学技术出版社, 1987: 1)

[16] Chen B L.  Imperfection Analysis and Countmeasures for Welding Engineering. Beijing: China Machine Press, 2006: 301

     (陈伯蠡. 焊接工程缺欠分析与对策. 北京: 机械工业出版社, 2006: 301)

[17] Zhang J S.  High Temperature Deformation and Fracture of Materials. Beijing: Science Press, 2007: 378

     (张俊善. 材料的高温变形与断裂. 北京: 科学出版社, 2007: 378)

[18] Robertson D G, Holdsworth S R.  ECCC Data Sheets 2005. UK: ETD Ltd., 2005: 47

[19] Maruyama K, Sawada K, Koike J.  ISIJ Int, 2001; 41: 641

[20] Komai N, Masuyama F.  ISIJ Int, 2002 ; 42: 1364

[21] Gaffard V, Gourgues-Lorenzon A F, Besson J.  Nucl Eng Des,2005; 235: 2547

[22] Hald J, Korcakova L.  ISIJ Int, 2003; 43: 420

[23] Dimmler G, Weinert P, Kozeschnik E, Cerjak H.  Mater Charact,2003; 51: 341

[24] Hattestrand M, Andren H.  Micron, 2001; 32: 789

[25] Lee J S, Armaki H G, Maruyama K, Muraki T, Asahi H.  Mater Sci Eng, 2006; A428: 270

[26] Peng Z F, Cai L S, Peng F F, Hu Y P, Chen F Y.  Acta Metall Sin,2010; 46: 429

     (彭志方, 蔡黎胜, 彭芳芳, 胡永平, 陈方玉. 金属学报, 2010, 46: 429)

[27] Li D J, Shinozaki K.  Sci Technol Weld Join, 2005; 10: 544

[28] Smith D J, Walker N S, Kimmins S T.  J Pressure Vessel Pip,2003; 80: 617
Outlines

/

〈 〉