论文

PREPARATION, STRUCTURE AND MAGNETIC PROPERTIES OF SmCo5 NANOPARTICLES AND NANOFLAKES

  • LIU Rong-Meng ,
  • YUE Meng ,
  • ZHANG Dong-Shou ,
  • LIU Wei-Jiang ,
  • ZHANG Jiu-Xin
Expand
  • 1. Key Laboratory of Advanced Functional Materials, Ministry of Education, Beijing University of Technology, Beijing 100124
    2. State Key Laboratory of Magnetism, Institute of Physics, Chinese Academy of Sciences, Beijing 100190

Received date: 2011-10-17

  Revised date: 2012-03-27

  Online published: 2012-04-11

Supported by

National Natural Science Foundation of China

Abstract

Surfactant-assisted high energy ball milling technique is a new method of producing magnetic nanoparticles. In this study, permanent magnetic SmCo5 nanoparticles and nanoflakes with high room-temperature coercivity values and narrow particle size distributions were produced by this technology and a subsequent size-selection process. The SmCo5 nanoparticles with average particle sizes of 9.8 and 47.5 nm, exhibited room-temperature coercivity values of 6.8×104 and 7.3×105 A/m, respectively, while the SmCo5 nanoflakes, with the mean particle size of about 1.4 μm and average thickness of 75 nm, showed excellent permanent magnetic properties with an obvious c-axis crystal texture, a strong magnetic anisotropy and high coercivity values of 5.5×105 and 1.6×106 A/m in their easy-axis and hard-axis directions, respectively. The coercivity values of SmCo5 nanoparticles and nanoflakes exhibited a significant particle size dependance effect.

Cite this article

LIU Rong-Meng , YUE Meng , ZHANG Dong-Shou , LIU Wei-Jiang , ZHANG Jiu-Xin . PREPARATION, STRUCTURE AND MAGNETIC PROPERTIES OF SmCo5 NANOPARTICLES AND NANOFLAKES[J]. Acta Metall Sin, 2012 , 48(4) : 475 -479 . DOI: 10.3724/SP.J.1037.2011.00643

References

[1] Chakka V M, Altuncevahir B, Jin Z Q, Li Y, Liu J P. J Appl Phys, 2006; 99: 08E912

[2] Wang Y P, Li Y, Rong C B, Liu J P.  Nanotechnology, 2007; 18: 465701

[3] Yue M, Wang Y P, Poudyal N, Rong C B.  J Appl Phys,2009; 105: 07A708

[4] Shen Y, Huang M Q, Higgins A K, Liu S, Horwath J C, Chen C H. J Appl Phys, 2010; 107: 09A722

[5] Akdogan N G, Hadjipanayis G C, Sellmyer D J.  IEEE Trans Magn,2009; 45: 4417

[6] Akdogan N G, Hadjipanayis G C, Sellmyer D J.  J Appl Phys,2009; 105: 07A710

[7] Cha H G, Kim Y H, Kim C W, Kwon H W, Kang Y S.  J Phys Chem,2007; C111: 1219

[8] Gabay A M, Akdogan N G, Marinescu M, Hadjipanayis G C. J Phys: Condens Matter, 2010; 22: 164213

[9] Cui B Z, Gabay A M, Li W F, Marinescu M, Liu J F, Hadjipanayis G C. J Appl Phys, 2010; 107: 09A721

[10] Zheng L Y, Cui B Z, Akdogan N G, Marinescu M, Hadjipanayis G C. J Alloy Compd, 2010; 504: 391

[11] Cui B Z, Li W F, Hadjipanayis G C.  Acta Mater,2011;59: 563

[12] Akdogan N G, Hadjipanayis G C, Sellmyer D J.  Nanotechnology,2010; 21: 295705

[13] Jones N.  Nature, 2011; 472: 22

[14] Li S X, Zhang J C, Shen Y, Ni B, Zhang J G.  J Mater Sci Technol, 2006; 22: 659

[15] Jian Z G, Liu W Q, Cao A L, Zhang D T, Yue M, Zhang J X. Chin J Rare Met, 2009; 33: 821

     (菅志刚, 刘卫强, 曹爱利, 张东涛, 岳明, 张久兴. 稀有金属, 2009; 33: 821)

[16] Liu S L,Yu Y Y, Teng R H, Xu J R.  Acta Metall Sin, 1998; 34: 1223

     (刘思林, 于英仪, 滕荣厚, 徐教仁. 金属学报, 1998; 34: 1223)

[17] Cao W M, Chen H, Shi X H, Zhu L J, Ji X B, Zhang L, Yin R H. Acta Metall Sin, 2008; 44: 445

     (曹为民, 陈浩, 石新红, 朱律均, 姬学彬, 张磊, 印仁和.金属学报, 2008; 44: 445)

[18] Liu X M, Fu S Y, Xiao H M, Li Y Q.  Acta Metall Sin, 2006; 42: 497

 (刘献明, 付绍云, 肖红梅, 李元庆. 金属学报, 2006; 42: 497)

[19] http://zjyqyb.cnpowder.com.cn/news/19378.html

[20] Liu R M, Yue M, Liu W Q, Zhang D T, Zhang J X.  Appl Phys Lett,2011; 99: 162510

[21] Liu R M, Yue M, Liu W Q, Zhang D T, Zhang J X, Guo Z H, Li W. IEEE Trans Nanotechnol, doi: 10.1109/TNANO.2012.2184299

[22] Coey J M D.  J Magn Magn Mater, 1995; 140-144: 1041

[23] Ding J, Mc Cormick P G, Street R.  J Alloy Compd, 1993; 191: 197

[24] Strnat K J. In: Wehfarth E P, Buschow K H eds.,  Ferromagnetic Materials. Elsevier: Amsterdam, 1988; 4: 131

[25] Hadjipanayis G C.  J Magn Magn Mater, 1999; 200: 373
Outlines

/

〈 〉