论文

INFLUENCE OF AGING ON THE HARDENABILITY OF 7055 ALUMINUM ALLOY THICK PLATE

  • LIU Qing-Tan ,
  • LI Zhang-Bei ,
  • DENG Yun-Lai ,
  • ZHANG Xin-Meng
Expand
  • Key Laboratory of Nonferrous Metals, Ministry of Education, School of Materials Science and Engineering, Central South University, Changsha 410083

Received date: 2011-08-10

  Revised date: 2011-10-31

  Online published: 2012-03-11

Supported by

Supported by National Basic Research Program of China (No.2012CB619501) and the Freedom Explore Program of Central South University (No.201012200238)

Abstract

The influence of aging on the hardenability of 7055 aluminum alloy thick plate was investigated by means of end-quench test, optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and differential scanning calorimetry (DSC). The results show that the hardenability can be improved by long time natural aging before artificial aging. The hardened depth is about 78 mm after natural aging and only about 45 mm after artificial aging, but increased to be about 100 mm after natural and artificial aging. During slow quenching, the coarse η equilibrium phase forms, and the solute concentration and vacancy concentration are decreased, which lead to larger and fewer η' hardening precipitates, thus lower hardness after aging. The long time natural aging before artificial aging is favorable for formation of stable GP zones at slowly-cooled locations, and consequently more amount of dispersed and fine η'  hardening precipitates, which give rise to higher hardness and simultaneously better hardenability.

Cite this article

LIU Qing-Tan , LI Zhang-Bei , DENG Yun-Lai , ZHANG Xin-Meng . INFLUENCE OF AGING ON THE HARDENABILITY OF 7055 ALUMINUM ALLOY THICK PLATE[J]. Acta Metall Sin, 2012 , 48(3) : 343 -350 . DOI: 10.3724/SP.J.1037.2011.00517

References

[1] Liu S D, Liu W J, Zhang Y, Zhang X M, Deng Y L. J Alloys Compd, 2010; 507: 53

[2] Robinson J S, Cudd R L, Tanner D A. J Mater Process Technol, 2001; 119: 261

[3] Lim S T, Yun S J, Nam S W. Mater Sci Eng, 2004; A371: 82

[4] Liu S D, Zhong Q M, Zhang Y, Zhang X M. Mater Des, 2010; 31: 3116

[5] Zhang X M, Deng Y L, Zhang Y. Chin Pat, 200710034410.8, 2007

(张新明, 邓运来, 张 勇. 中国专利, 200710034410.8, 2007)

[6] Robson J D, Prangnell P B. Mater Sci Technol, 2002; 18: 607

[7] Liu S D, Zhang X M, You J H, Huang Z B, Zhang C, Zhang X Y. Trans Nonferrous Met Soc China, 2006; 16: 2034

刘胜胆, 张新明, 游江海, 黄振宝, 张翀, 张小艳. 中国有色金属学报, 2006; 16: 2034)

[8] Liu S D, Zhang X M, Chen M A. Trans Nonferrous Met Soc China, 2007; 17: 787

[9] Viana F, Pinto A M P, Santos H M C, Lopes A B. J Mater Process Technol, 1999; 92–93: 54

[10] Park J K, Ardell A J. Mater Sci Eng, 1989; A114: 197

[11] Chen J Z. PhD Thesis, Harbin Institute of Technology, 2008

(陈军洲. 哈尔滨工业大学博士学位论文, 2008)

[12] Hansen V, Stiller K, Waterloo G. Mater Sci Forum, 2002; 396–402: 815

[13] Chinh N O, Lendvi J, Ping D H. J Alloys Compd, 2004; 378: 52

[14] Porter D A, Easterling K E. Phase Transformation in Metals and Alloys. Oxford: Alden Press, 1981: 265

[15] Liu S D, Zhang X M, Chen M A. Mater Charact, 2008; 59: 53
Outlines

/