论文

MORPHOLOGICAL INSTABILITY OF γ' PHASE IN NICKEL-BASED POWDER METALLURGY SUPERALLOYS

  • HU Ben-Fu ,
  • LIU Guo-Quan ,
  • WU Kai ,
  • TIAN Gao-Feng
Expand
  • 1) School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
    2) State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083

Received date: 2011-11-25

  Revised date: 2011-12-15

  Online published: 2012-03-11

Supported by

Supported by National Defence Pre-research Funds (No.9140A12070507QT0202) and High Technology Research and Development Program of China (No.2007AA03A223)

Abstract

The morphological evolution and its regularity of γ'  precipitates in the low mismatch alloys powder metallurgy (P/M) FGH98I and FGH96 under different heat treatment conditions were studied systematically. The results show that the morphological instability of γ'  phase can be summarized as the splitting and unstable protrusion. The splitting of γ'  phase is caused by the interaction of anisotropic elastic strain field between γ'  phase and $\gamma$ matrix which is rich in solute atoms. While the irregular morphology of unstabe protrusion is mainly due to the concentration changes of solute atoms in the matrix or in the local places along grain boundaries, leading to the non-equilibrium growth of γ'  phase. The coexist phenomenon of splitting and unstable protrusion, the formation mechanism of fan type structure induced by discontinous precipitation are discussed respectively.

Cite this article

HU Ben-Fu , LIU Guo-Quan , WU Kai , TIAN Gao-Feng . MORPHOLOGICAL INSTABILITY OF γ' PHASE IN NICKEL-BASED POWDER METALLURGY SUPERALLOYS[J]. Acta Metall Sin, 2012 , 48(3) : 257 -263 . DOI: 10.3724/SP.J.1037.2011.00731

References

[1] Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1984; 67: 247

[2] Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1985; 74: 139

[3] Qiu Y Y. J Alloy Compd, 1998; 270: 145

[4] Leo P H, Lowengrub T S. Acta Mater, 2001; 49: 2761

[5] Lee J K. Theor Appl Fract Mech, 2000; 33: 207

[6] Yang A, Xiong Y, Liu L. Sci Technol Adv Mater, 2001; 2: 105

[7] Banerjee D, Banerjee R, Wang Y. Scr Mater, 1999; 41: 1023

[8] Li D Y, Chen L Q. Acta Mater, 1999; 47: 247

[9] Cha P R, Yeon D H. Chung S H. Scr Mater, 2005; 52: 1241

[10] Khachaturyan A G, Semenovskaya S V, Morris Jr J W. Acta Metall, 1988; 36: 1563

[11] Yoo Y S. Scr Mater, 2005; 53: 81

[12] Radis R, Schaffer M. Superalloy 2008, Warrendale, PA: TMS, 2008: 829

[13] Furrer D. Scr Mater, 1999; 40: 1215

[14] Qiu Y Y. Acta Mater, 1996; 44: 4969

[15] Jackson M P, Reed R C. Mater Sci Eng, 1999; A259: 1241

[16] Hazotte A, Grosdidier T, Denis S. Scr Mater, 1996; 34(4): 60

[17] Gerold V, translated by Wang P X et al. Material Science and Technology: Solid Structre. Beijing: Science Press, 1998: 184

(Gerold V著, 王佩璇等译. 材料科学与技术丛书: 固体结构. 北京: 科学出版社, 1998: 184)

[18] Mullins W W, Sekerka R F. J Appl Phys, 1963; 34: 323

[19] Ricks R A, Porter A J, Ecob R C. Acta Metall, 1983; 31: 43

[20] Mitchell R J, Preuss M, Tin S, Hardy M C. Mater Sci Eng, 2008; A473: 158

[21] Staron P, Kampmann R. Acta Mater, 2000; 48: 701

[22] Staron P, Kampmann R. Acta Mater, 2000; 48: 713

[23] Assadi H, Schroers J. Acta Mater, 2002; 50: 89
Outlines

/

〈 〉