论文

FINE MICROSTRUCTURE AND TOUGHNESS OF LOW CARBON COPPER CONTAINING ULTRA HIGH STRENGTH NV-F690 HEAVY STEEL PLATE

  • LIU Dong-Sheng ,
  • CHENG Bing-Gui ,
  • CHEN Yuan-Yuan
Expand
  • Institute of Research of Iron and Steel, Shasteel, Zhangjiagang 215625

Received date: 2011-08-19

  Revised date: 2011-11-21

  Online published: 2012-03-11

Abstract

Advanced NV-F690 heavy steel plates for offshore structure and shipbuilding have been produced via continuous casting of the slab, thermomechanical control rolling of the plate followed by solutionizing (austenitizing), quenching and tempering (QT) steps. The present work is to reveal the microstructure evolution and evaluate the mechanical properties of 80 mm thick plates subjected to the QT process. The microstructures were characterized with SEM, EBSD and TEM. At quarter thickness ($t$/4) where the cooling rate was rapid, the as quenched microstructures consist of mainly lath--like bainite (LB), between the laths exist fine martensite/austenite (M/A) constituents. At center thickness (t/2), the as quenched microstructures consist of granular bainite (GB)+dislocated LB. The fraction of high angle grain boundary (HAGB) at t/4 of the quenched plate is 67.5% while that at t/2 is 63.0%. After tempering at 650 ℃ for 150 min, the average width of the laths is 0.2 μm at t/4 and\linebreak 0.4 μm at t/2. Cell structures with high misorientations exist in the tempered LB at t/4 while these are absent at t/2. The fraction of HAGB is increased to 71.7% at t/4 while that at t/2 is not significantly changed. Profuse Cu precipitation occurs and the M/A constituents decompose into Cr-Mo containing carbides during tempering. Ductile fracture behaviour is observed even at -80 ℃ at both t/2 and t/4 of the 80 mm thick NV-F690 plate treated by the QT process. The impact toughness at t/4 is higher than that at t/2 due to the predominance of finer LB and higher fraction of HAGB. With the increase of the displacement of the ductile crack propagation, the area with dimples and the size of the dimples increase leading to increased Charpy impact absorbed energy of the NV-F690 plate\linebreak at -80 ℃.

Cite this article

LIU Dong-Sheng , CHENG Bing-Gui , CHEN Yuan-Yuan . FINE MICROSTRUCTURE AND TOUGHNESS OF LOW CARBON COPPER CONTAINING ULTRA HIGH STRENGTH NV-F690 HEAVY STEEL PLATE[J]. Acta Metall Sin, 2012 , 48(3) : 334 -342 . DOI: 10.3724/SP.J.1037.2011.00528

References

[1] Weng Y Q, Kang Y L. Iron Steel, 2010; 45(9): 1

(翁宇庆, 康永林. 钢铁, 2010; 45(9): 1)

[2] Hodnik P, F¨urst C, Pennerstorfer P, Lengauer H. Stahl Eisen, 2008; 128(10): 35

[3] Schmidt D, Dehmel R, Horn G. Stahl Eisen, 2008; 128(8): 25

[4] Shikanai N, Mitao S, Endo S. JFE Tech Report, 2008; (1): 1

[5] Sch¨utz W, Schr¨oter F. Mater Sci Technol, 2005; 21: 590

[6] DeArdo A J. ISIJ Int, 1995; 35: 946

[7] Dhua S K, Mukerjee D, Sarma D S. Metall Mater Trans, 2003; 34A: 2493

[8] Shome M, Mohanty O N. Metall Mater Trans, 2006; 37A: 2159

[9] Dhua S K, Mukerjee D, Sarma D S. Metall Mater Trans, 2001; 32A: 2259

[10] Mujahid M, Lis A K, Garcia C I, DeArdo A J. J Mater Eng Perform, 1998; 7: 247

[11] Hwang G C, Lee S, Yoo J Y, Choo W Y. Mater Sci Eng, 1998; A252: 256

[12] Luo X B, Yang C F, Su H, Chai F. Trans Mater Heat Treat, 2011; 32(6): 73

(罗小兵, 杨才福, 苏航, 柴峰. 材料热处理学报, 2011; 32(6): 73)

[13] Liu D S, Cheng B G, Luo M. Trans Mater Heat Treat, 2011; 32(9): 125

(刘东升, 程丙贵, 罗咪. 材料热处理学报, 2011; 32(9): 125)

[14] Yuan G, Han Y, Wang C, Wang Z D, Wang D G. Trans Mater Heat Treat, 2010; 31(12): 148

(袁国, 韩 毅, 王超, 王昭东, 王国栋. 材料热处理学报, 2010; 31(12): 148)

[15] Gao G H, Zhang H, Bai B Z. Acta Metall Sin, 2011; 47: 513

(高古辉, 张寒, 白秉哲. 金属学报, 2011; 47: 513)

[16] Han S Y, Shin S Y, Lee S, Kim N J, Bae J H, Kim K. Metall Mater Trans, 2010; 41A: 329

[17] Miao C L, Shang C J, Wang X M, Zhang L F, Mani S. Acta Metall Sin, 2010; 46: 541

(缪成亮, 尚成嘉, 王学敏, 张龙飞, Mani S. 金属学报, 2010; 46: 541)

[18] Liu D S, Cheng B G, Luo M. Acta Metall Sin, 2011; 47: 1233

(刘东升, 程丙贵, 罗咪. 金属学报, 2011; 47: 1233)

[19] Nie Y, Shang C J, Chen H, Wang X M, He X L. Trans Mater Heat Treat, 2010; 31(2): 51

(聂燚, 尚成嘉, 陈辉, 王学敏, 贺信莱. 材料热处理学报, 2010; 31(2): 51)

[20] Hwang B, Lee C G, Lee T H. Metall Mater Trans, 2010; 41A: 85

[21] Han S Y, Shin S Y, Seo C H, Lee H, Bae J H, Kim K. Metall Mater Trans, 2010; 41A: 1851

[22] Liu D, Cheng B, Luo M. ISIJ Int, 2011; 51: 603

[23] Bhagat A N, Pabi S K, Ranganathan S, Mohanty O N. ISIJ Int, 2004; 44: 115

[24] Wiesner C S. Int J Pres Ves Piping, 1996; (69): 185

[25] Hashemi S H. Int J Pres Ves Piping, 2008; (85): 879

[26] Deng W, Gao X H, Qin X M, Zhao D W, Du L X, Wang G D. Acta Metall Sin, 2010; 46: 533

(邓伟, 高秀华, 秦小梅, 赵德文, 杜林秀, 王国栋. 金属学报, 2010; 46: 533)
Outlines

/

〈 〉