论文

MODIFICATION OF STRESS DISTRIBUTION ALONG THE THICKNESS OF (Ti, Al)N COATINGS AND PREPARATION OF THE COATINGS WITH LARGE THICKNESS

  • DIAO Sheng-Sheng ,
  • CHENG Yu ,
  • CHANG Zheng-Kai ,
  • YU Tie-Gang ,
  • XUN Tiao
Expand
  • 1) Shenzhen Polytechnic, Shenzhen 518055
    2) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2011-08-08

  Revised date: 2011-11-02

  Online published: 2012-03-11

Supported by

Supported by National Natural Science Foundation of China (No.50471072) and Guangdong Natural Science Foundation (No.S2011040004468})

Abstract

The effects of N2 partial pressure on the depth distribution
of residual stresses and mechanical properties in the (Ti, Al)N coatings
prepared by arc ion plating (AIP), were investigated. The results indicate
that the stress distribution was roughly uniform when the coatings were
deposited under lower NN2 partial pressure. As the partial pressure
increased the stress distribution to exhibited a “bell” shape and the
average stresses of coatings increased remarkably. The mechanism of
stress distribution was analyzed by characterizing the microstructure and
the composition of the coating. The N2 partial pressure also affected the
hardness of coatings and the coating/substrate adhesion obviously. The
higher the N2 partial pressure is, the higher the coating hardness but
the lower the adhesion. The stress distribution can be modified and the
adhesion of the coating/substrate can be improved by optimizing N2 partial
pressure parameter. Finally, the coatings with the thickness over 130 μm
were successfully directly deposited on the substrate through optimizing
the N2 partial pressure.

Cite this article

DIAO Sheng-Sheng , CHENG Yu , CHANG Zheng-Kai , YU Tie-Gang , XUN Tiao . MODIFICATION OF STRESS DISTRIBUTION ALONG THE THICKNESS OF (Ti, Al)N COATINGS AND PREPARATION OF THE COATINGS WITH LARGE THICKNESS[J]. Acta Metall Sin, 2012 , 48(3) : 277 -282 . DOI: 10.3724/SP.J.1037.2011.00504

References

[1] Palmers J, Van Stappen M. Surf Coat Technol, 1995; 76/77: 363

[2] Shew B Y, Huang J L. Surf Coat Technol, 1995; 71: 30

[3] Cheng Y H, Tay B K, Lau S P, Shi X, Chua H C. Thin Solid Films, 2000; 379: 76

[4] Zhao S S, Yang Y, Li J B, Gong J, Sun C. Surf Coat Technol, 2008; 202: 5185

[5] Huang J H, Ma C H, Chen H. Surf Coat Technol, 2006; 201: 3199

[6] Sun X L, Fan Z X, Shao J D. Acta Metall Sin, 2007; 43: 307

(孙喜莲, 范正修, 邵建达. 金属学报, 2007; 43: 307)

[7] Song G H, Zheng J D, Liu Y, Sun C. J Synth Crys, 2004; 33: 422

[8] Stein C, Keunecke, M, Bewilogua K, Chudoba T, Koelker W, van den Berg H. Surf Coat Technol, 2011; 205(spec): 2

[9] Wu P, Zhou C Z, Tang X N. Acta Metall Sin, 1994; 30: 508

(吴萍, 周昌炽, 唐西南. 金属学报, 1994; 30: 508)

[10] PalDey S, Deevi S C. Mater Sci Eng, 2003; A361: 1

[11] Manaila R, Devenyi A, Biro D, David L, Barna P B, Kovacs A. Surf Coat Technol, 2002; 151: 21

[12] Li M S, Wang F H. Surf Coat Technol, 2003; 167: 197

[13] Sanchette F, Czerwiec T. Surf Coat Technol, 1997; 96: 184

[14] Paul H M, Christian M, Lars H, Helmut C. Prog Mater Sci, 2006; 51: 1032

[15] Zhao S S, Du H, Hua W G, Gong J, Li J B, Sun C. J Mater Res, 2007; 22: 2659

[16] Yang H G, Li S, Zhang R L. China Surf Eng, 2009; 22(2): 20

(杨洪刚, 李曙, 张荣禄.中国表面工程, 2009; 22(2): 20)

[17] Wang T G, Zhao S S, Hua W G, Li J B, Gong J, Sun C. Mater Sci Eng, 2010; A527: 454

[18] Zhou Y, Rao G B, Wang J Q, Zhang B, Yu Z M, Ke W, Han E H. Thin Solid Films, 2011; 519: 2207

[19] Wan X S, Zhao S S, Yang Y, Gong J, Sun C. Surf Coat Technol, 2010; 204: 1800

[20] Yang Y, Zhao S S, Gong J, Jiang X, Sun C. J Mater Sci Technol, 2011; 27: 385

[21] Josson B, Hogmark S. Thin Solid Films, 1984; 114: 257

[22] Zheng J D, Zou Y S, Song G H, Gong J, Liu Y, Sun C, Wen L S. Acta Metall Sin, 2004; 40: 745

(郑静地, 邹友生, 宋贵宏, 宫骏, 刘 越, 孙超, 闻立时. 金属学报, 2004; 40: 745)

[23] Thornton J A. Ann Rev Mater Sci, 1977; 7: 239

[24] Tian M B, Liu D L. Film Science and Technology Handbook (1st Vol.). Beijing: China Machine Press, 1980: 7

(田民波, 刘德令. 薄膜科学与技术手册 (上). 北京: 机械工业出版社, 1980: 7)

[25] Carvalho N J M, Zoestbergen E, Kooi B J, Hosson D J T M. Thin Solid Films, 2003; 429: 179
Outlines

/

〈 〉