论文

AN ATOM DENSE PACKING MODEL FOR METALLIC GLASS WITH HIGH SOLUTE CONCENTRATION IN (PSEUDO–) TERNARY SYSTEMS

  • LV Bao-Chen ,
  • LIU Hai-Shou ,
  • REN Xin- ,
  • YU Xiao-Liang ,
  • LI Jin-Ling ,
  • LI Gang ,
  • XUN Ti-Jun
Expand
  • Materials Science and Engineering School, Liaoning Science Technology University, Fuxin 123000

Received date: 2011-11-01

  Revised date: 2011-11-01

  Online published: 2012-02-11

Supported by

Supported by PhD Research Start Fund of Liaoning Science Technology Universuty of China (No.09416)

Abstract

A modified Miracle model based on packing different atoms on the first shell of solute–centered cluster is advanced to predict the best glass–former in some high content (pseudo–) ternary systems such as Ti–Ni–Al etc. The calculated results not only for the best ribbon metallic glass–formers in Ti–Ni–Al, Ti–Ni–Sn, but also for the best bulk metallic glass–formers in some other systems correspond to the experimental results very well, indicating the validity of this model.

Cite this article

LV Bao-Chen , LIU Hai-Shou , REN Xin- , YU Xiao-Liang , LI Jin-Ling , LI Gang , XUN Ti-Jun . AN ATOM DENSE PACKING MODEL FOR METALLIC GLASS WITH HIGH SOLUTE CONCENTRATION IN (PSEUDO–) TERNARY SYSTEMS[J]. Acta Metall Sin, 2012 , 48(2) : 240 -244 . DOI: 10.3724/SP.J.1037.2011.00676

References

[1] Inoue A, Nishiyama N, Kimura H. Mater Trans JIM, 1997; 38: 179

[2] Inoue A, Zhang T. Mater Trans JIM, 1996; 37: 185

[3] Ma H, Shi L L, Xu J, Li Y, Ma E. Appl Phys Lett, 2005; 87: 181915

[4] Guo F Q, Wang H J, Poon S J, Shiflet G J. Appl Phys Lett, 2005; 86: 091907

[5] Turnbull D. Contemp Phys, 1969; 10: 473

[6] Inoue A. Acta Mater, 2000; 48: 279

[7] Lu Z P, Liu C T. Acta Mater, 2002; 50: 3501

[8] Lisboa R D S, Bolfarini C, Botta W J F, Kiminami C S. Appl Phys Lett, 2005; 86: 211904

[9] Miracle D B. Nat Mater, 2004; 3: 697

[10] Wang A P, Wang J Q, Ma E. Appl Phys Lett, 2007; 90: 121912

[11] Shi L L, Xu J, Ma E. Acta Mater, 2008; 56: 3613

[12] L¨u B C, Yao J H, Xu J, Li Y. Appl Phys Lett, 2009; 94: 241913

[13] Pelton A D, Degterov S A, Erksson G, Robelin C, Dessureault Y. Metall Mater Trans, 2000; 31B: 651

[14] Guo F Q, Poon S J, Shiflet G J. J Appl Phys, 2004; 97: 013512

[15] Miracle D B. J Non–Cryst Solids, 2004; 342: 89

[16] Miracle D B, Sanders W S, Senkov O N. Philos Mag, 2003; 83: 2409

[17] Senkov O N, Scott J M. Scr Mater, 2004; 50: 449

[18] Miracle D B. Acta Mater, 2006; 54: 4317

[19] L¨u B C, Li Y, Xu J. J Alloys Compd, 2009; 467: 261

[20] L¨u B C, Xu J. J Non–Cryst Solids, 2008; 354: 5425

[21] Jing Q, Zhang Y, Wang D, Li Y. Mater Sci Eng, 2006; A441: 106

[22] Zhang T, Inoue A. Mater Trans, 1998; 39: 1001

[23] Inoue A K, Nishiyama N K, Matsuda T K. Mater Trans, 1996; 37: 181